dc:description.abstract

Fatigue crack propagation has been observed for a number of commercial aluminium alloys. Comparable data was obtained for a variety of crack and specimen geometries over a range of crack lengths for a given alloy. Where crack propagation only was of interest the initiation event has been excluded by pre-cracking the specimen using a fin of material adjacent to the crack face. By this method a controlled defect size is introduced in to the specimen. By modification of the D.C. potential drop method it has been shown possible to measure the growth of cracking from 0.12mm by this method. Crack growth from defects greater than 0.6mm have been shown to give conventional crack propagation deduced by principle of similitude. Fatigue fracture surface analysis has been conducted for cracking from both free surfaces and from blunt notches. A `quasi cleavage' feature has been identified and is shown to be prominent when the fatigue stress intensity range is below 10 MNm-3/2.

Degree

thesis:*
Name dc:type.qualificationname
Ph.D.
Level dc:type.qualificationlevel
doctoral
Grantor dc:publisher.institution
Aston University
Year dc:date.issued
1986

Author and committee

dc:creator, dc:contributor.*
Author dc:creator
  • Hunt, Anthony W.

Chain of custody

source
Harvested from
Aston University
Base URL
publications.aston.ac.uk/cgi/oai2
Last updated
2026-11-19
Source record
OAI-PMH GetRecord
related terms
citation

Hunt, Anthony W.. Fatigue of commercial aluminium alloys. doctoral thesis, Aston University, 1986.