dc:description.abstract

In a steam reformer furnace the HK-40 catalyst tubes are subjected to severe conditions of high temperature and pressure, and are vulnerable to creep-rupture failures. The resultant lost production and high cost of replacing tubes provide a strong incentive for predicting the service life of catalyst tubes. The crack growth behaviour of the HK-40 alloy under creep conditions was investigated and the results used to ascertain whether current concepts of creep-fracture mechanics were applicable to the HK-40 alloy. It was demonstrated that crack growth rates in different specimen geometries could not be correlated as a whole with either nett-section stress or the elastic stress intensity factor. The metallographic studies provided a valuable insight into the crack growth mechanisms operating in the HK-40 alloy. It was apparent that the cracks followed the continuous interdendritic chromium carbide networks; interdendritic microcracks were always observed ahead of the main cracks in the HK-40 alloy.

Degree

thesis:*
Name dc:type.qualificationname
Ph.D.
Level dc:type.qualificationlevel
doctoral
Grantor dc:publisher.institution
Aston University
Year dc:date.issued
1980

Author and committee

dc:creator, dc:contributor.*
Author dc:creator
  • Bain, Malcolm D.M.

Rights

Language dc:language.dcterms_iso639_2
eng

Identifiers

dc:identifier.*

Chain of custody

source
Harvested from
Aston University
Base URL
publications.aston.ac.uk/cgi/oai2
Last updated
2026-11-19
Source record
OAI-PMH GetRecord
related terms
citation

Bain, Malcolm D.M.. Crack Growth Under Creep Conditions in HK-40 Stainless Steel. doctoral thesis, Aston University, 1980. https://doi.org/10.48780/publications.aston.ac.uk.00014469