dc:description.abstractAims: To evaluate the difference in surface wear between various composite materials when utilised as clear aligner attachments. Materials and Method: A custom-made experimental apparatus was utilised, in combination with an MTS Criterion Model 42 machine (Model 42, MTS Criterion® Series 40 Electromechanical universal test systems, MTS systems corporation, Minnesota, USA), to replicate the clinical technique of aligner removal. Rectangular composite attachments were placed onto a first permanent molar within a typodont. Four commercially available nanohybrid composite resins were evaluated. These included two conventional composites, Venus Pearl (Heraeus-Kulzer, GmbH) and Tetric EvoCeram (Ivoclar Vivadent, Liechtenstein), one flowable composite Wave (SDI Limited, Bayswater, Victoria, Australia) and BracePaste an orthodontic adhesive (American Orthodontics, Sheboygan, CA, USA). A baseline 3D surface scan was taken and a second scan re-taken after a 250 and 500 aligner insertion and removal cycle. Following scan superimposition the median surface wear was assessed for each composite. Results: Using the current model, wear occurs only on the gingival aspect of composite attachments, with the greatest wear being found on the distal corner of the gingival aspect. The median value of wear in the distal corner of the gingival aspect after 500 cycles was 0.06mm for Tetric EvoCeram (ranging from 0.05mm-0.06mm), 0.04mm for Venus Pearl (ranging from 0.03-0.05mm), 0.08mm for Wave (ranging from 0.05-0.08mm) and 0.06mm for BracePaste (ranging from 0.05-0.06mm). The amount of wear found was progressive from 250 to 500 cycles. There was a statistically significant difference in wear at the distal corner of the gingival aspect of the attachments, across the four composite resins tested (p-value = 0.013 and p = 0.024 for 250 and 500 cycles respectively). PostIII hoc pairwise comparisons of the four composite resins showed that there was statistically significantly more wear of Wave composite compared to Venus Pearl (p-value = 0.006 and p = 0.016 for 250 and 500 cycles respectively after Bonferroni correction). Conclusion: Based on the current in vitro model of aligner insertion and removal the distal gingival surface of the attachments showed the greatest wear. The wear of Wave was statistically significantly (p < 0.05) greater than Venus Pearl. Clinically, the amount of wear would probably not be significant.
Degree
thesis:*- Name dc:type.qualificationname
- m_sc
- Level dc:type.qualificationlevel
- m_sc
- Grantor dc:publisher.institution
- University of Birmingham
- Year dc:date.issued
- 2025
Author and committee
dc:creator, dc:contributor.*- Author dc:creator
-
- Litt, Rebecca Jane
Subjects
dc:subject × 1Rights
- Language dc:language.dcterms_iso639_2
- eng