Abstract

dc:description.abstract

This thesis presents an analytical and literature-based comparison of the fatigue behavior of bending-loaded and tensile-loaded thin-walled welded joints. The main focus is the difference in through-thickness stress distribution between axial tensile loading and bending loading, and how this difference affects the interpretation of fatigue resistance in welded details. Under axial tensile loading, the nominal stress is approximately uniform through the plate thickness, while under bending loading the maximum stress occurs at the surface and decreases toward the neutral axis. This distinction is important for weld-toe fatigue, since a crack initiated under bending may propagate into a region of lower stress range, whereas a crack under axial tension remains exposed to a more uniform stress range. The thesis reviews fatigue mechanisms, welded-joint fatigue assessment approaches, and relevant design concepts from EN 1993-1-9, IIW recommendations, ISO 14347, BS 7608, and published studies. Particular attention is given to the BS 7608 / Maddox thickness and bending correction concept, which is used to perform a parametric analytical comparison of plate thickness and degree of bending. The analysis shows that bending-loaded fatigue data may include a beneficial stress-gradient effect and should not be directly treated as equivalent to tensile-loaded fatigue data without considering the loading mode, plate thickness, welded detail, and crack path. Weld-toe geometry and relative stress gradient are also discussed as additional factors affecting local fatigue behavior. In the final part of the thesis, a symmetrical non-load-carrying cruciform welded specimen made from S355J2 steel is proposed for future axial tensile fatigue testing. The proposed methodology defines specimen geometry, welding documentation, strain gauge placement, secondary bending control, fatigue loading regime, failure criteria, run-out treatment, and S–N curve construction. The thesis provides a practical basis for future experimental work aimed at generating tensile fatigue data for thin-walled welded joints.

Degree

thesis:*
Level thesis:degree_level
Inženýrský
Discipline thesis:degree_discipline
bez specializace
Grantor dc:publisher
Vysoké učení technické v Brně. Fakulta strojního inženýrství

Author and committee

dc:creator, dc:contributor.*
Author dc:creator
  • Sleiman, Adham
Advisor dc:contributor.advisor
  • Jebáček, Ivo
Committee members dc:contributor.committeemember
  • Augustin, Petr
  • doc. Ing. Jaroslav Juračka, Ph.D. (předseda) doc. Ing. Ivo Jebáček, Ph.D. (místopředseda) doc. Ing. Jiří Hlinka, Ph.D. (člen) doc. Ing. Pavel Zikmund, Ph.D. (člen) Ing. Miroslav Šplíchal, Ph.D. (člen)

Subjects

dc:subject × 11

Rights

dc:rights
Statement dc:rights
  • Standardní licenční smlouva - přístup k plnému textu bez omezení
Language dc:language.iso
en, angličtina (English)

Identifiers

dc:identifier.*
Dc Identifier Citation
SLEIMAN, A. Únavová životnost tenkostěnných svarových spojů [online]. Brno: Vysoké učení technické v Brně. Fakulta strojního inženýrství. 2026.
Dc Identifier Other
174134

Chain of custody

source
Harvested from
Brno University of Technology
Base URL
dspace.vut.cz/oai/request
Last updated
2026-11-19
Source record
OAI-PMH GetRecord
citation

Sleiman, Adham. Únavová životnost tenkostěnných svarových spojů. Inženýrský thesis, Vysoké učení technické v Brně. Fakulta strojního inženýrství, http://hdl.handle.net/11012/257782