Back to search

Boston University

Effect of surface treatment on porcelain bond strength to titanium

Abstract

dc:description.abstract

OBJECTIVES: The aim of this study was to evaluate the bond strength of a low fusing veneering porcelain fired on Titanium grade V with different surface treatments. MATERIALS & METHODS: One hundred and twenty bars of Titanium grade V (25±1x 3±0.5x 0.5±0.05mm) were divided randomly into twelve groups: group 1 no surface treatment, group 2 Gold sputter coating, group 3 TiN sputter coating, group 4 Sandblasting Al2O3 125μm, group 5 Sandblasting Al2O3 180μm, group 6 Sandblasting Al2O3 250μm, group 7 Sandblasting Al2O3 125μm then gold sputter coating, group 8 Sandblasting Al2O3 180μm then gold sputter coating, group 9 Sandblasting Al2O3 250μm then gold sputter coating, group 10 Sandblasting Al2O3 125μm then TiN sputter coating, group 11 Sandblasting Al2O3 180μm then TiN sputter coating, group 12 Sandblasting Al2O3 250μm then TiN sputter coating. Vita Titankeramik porcelain was applied for all groups and built up manually with dimensions limited to 8x3x1mm and fired on Ti bars following the manufacturer’s instructions and ISO 9693 recommendations, and tested for bond strength by Schwickerath crack initiation test (ISO 9693) using an Instron universal testing machine (Model: 5566A). The mode of failure and bond interface were evaluated by SEM / EDS. RESULTS: The mean bond strength values of groups 1, 2, 3, 4, 5, 6, 7, 8, 9, 10, 11, and 12 were 2.31MPa (±0.2), 24.3MPa (±0.78), 46.94MPa (±1.29), 6.18MPa (±0.98), 9.46MPa (±1.08), 15.14MPa (±0.74), 24.84MPa (±1.73), 36.24MPa (±1.43), 41.49MPa (±2.13), 49.45MPa (±0.96), 69.36MPa (±0.96), 94.45MPa (±1.51), respectively. Two-way ANOVA with Tukey multiple comparisons test was performed to determine the groups that are statistically different. All tested groups (1-12) showed statistically significant difference except groups 2, and 7, P< 0.05. CONCLUSIONS: Within the limitations of this study, the following conclusions can be drawn: 1- Surface finish significantly affects the bond strength of low fusing porcelain to Ti grade V. 2- Larger Al2O3 particle size corresponded to higher bond strengths. 3- Sandblasting in combination with Au or TiN coatings produced the highest bond strength values. 4- Groups 1, 4, 5, & 6 showed Adhesive failure at the ceramic – metal interface; for groups 3, 10, 11, & 12 were found to be Cohesive failure within the porcelain layers; and for groups 2, 7, 8, & 9 were found to be mixed Adhesive / Cohesive failure.

Degree

thesis:*
Name thesis:degree_name
Doctor of Science (D.Sc.)
Level thesis:degree_level
doctoral
Discipline thesis:degree_discipline
Prosthodontics
Grantor
Boston University
Year dc:date.issued
2016

Author and committee

dc:creator, dc:contributor.*
Author dc:creator
  • Naas, Haitem MM

Subjects

dc:subject × 3

Rights

Language dc:language.iso
en_US

Identifiers

dc:identifier.*
Handle dc:identifier.uri
https://hdl.handle.net/2144/18698

Chain of custody

source
Harvested from
Boston University
Base URL
open.bu.edu/oai/request
Last updated
2026-11-19
Source record
OAI-PMH GetRecord
citation

Naas, Haitem MM. Effect of surface treatment on porcelain bond strength to titanium. doctoral thesis, Boston University, 2016. https://hdl.handle.net/2144/18698