Abstract

dc:description.abstract

OBJECTIVES: To test and compare the effects of static and cyclic loading on fracture toughness (K1C) and microhardness of dental restorative CAD/CAM materials. MATERIAL AND METHODS: Five commercially available CAD/CAM restorative materials were included in this study: Lava™ Ultimate Restorative (3M ESPE), IPS Empress® CAD (Ivoclar Vivadent), Enamic® (VITA), IPS e.max® CAD (Ivoclar Vivadent), and CERASMART™ (GC Dental). Polished rectangular bars 4×2×14 mm (n=30) were prepared from mill blocks for each material. Single notch of 0.5-1 mm in depth was made on the center of one length edge. Ten specimens per group for each material were randomly selected for 1) static mode, 2) after 100k cyclic loads, and 3) after 200k cyclic loads. The survival bars after the fatigue test were then subjected to a three-point flexural test. K1C values were determined on ‘single-edge-pre-crack-beams’ (SEPB) method. In addition, random specimens after the flexural test were selected for Vickers microhardness test from each group. Additionally indentation fracture method (IF) was used to determine surface fracture toughness for e.max CAD and Empress CAD. All the results were analyzed via ANOVA with Tukey’s HSD test or least square regression model using JMP Pro 12.0. RESULTS: The mean fracture toughness (K1C) of the material tested in static mode (3.2 MPa.m1/2 for e.max CAD, 2 MPa.m1/2 for Lava Ult, 1.95 MPa.m1/2 for Empress CAD, 1.92 MPa.m1/2 for Enamic, and 1.65 MPa.m1/2 for Cerasmart). The 100k fatigue group (4.02 MPa.m1/2 for e.max CAD, 3.06 MPa.m1/2 for Cerasmart, 2.55 MPa.m1/2 for Lava Ult, 2.01 MPa.m1/2 for Enamic, 1.94 MPa.m1/2 for Empress CAD) The 200k fatigue group (3.14 MPa.m1/2 for Cerasmart, 2.83 MPa.m1/2 for Lava Ult, 2.68 MPa.m1/2 for e.max CAD, 2.01 MPa.m1/2 for Enamic, 1.72 MPa.m1/2 for Empress CAD). While there was a significant difference in the mean fracture toughness (K1C) and (VHN) after fatigue of material tested (p<0.05). CONCLUSION: The CAD/CAM materials tested exhibited a higher K1C values after cyclic loading, along with lower K1C compared to the static group. In addition, K1C values by IF method exhibit lower K1C values after fatigue that was not a good way to test the fracture toughness value.

Degree

thesis:*
Name thesis:degree_name
Doctor of Science in Dentistry
Level thesis:degree_level
doctoral
Discipline thesis:degree_discipline
Restorative Sciences & Biomaterials
Grantor
Boston University
Year dc:date.issued
2016

Author and committee

dc:creator, dc:contributor.*
Author dc:creator
  • Kensara, Alaa Ahmed

Subjects

dc:subject × 7

Rights

Language dc:language.iso
en_US

Identifiers

dc:identifier.*
Handle dc:identifier.uri
https://hdl.handle.net/2144/18716

Chain of custody

source
Harvested from
Boston University
Base URL
open.bu.edu/oai/request
Last updated
2026-11-19
Source record
OAI-PMH GetRecord
citation

Kensara, Alaa Ahmed. Static and cyclic loading effects on fracture toughness of contemporary CAD/CAM restorative materials. doctoral thesis, Boston University, 2016. https://hdl.handle.net/2144/18716