Effects of polymerization on mechanical properties and wear of printed materials

Abstract

dc:description.abstract

OBJECTIVE:This study aimed to evaluate the effects of different post-polymerization methods on the mechanical properties, surface hardness, degree of conversion (DC), and wear resistance of various 3D-printed (3DP) dental materials. The goal was to determine optimal polymerization protocols that enhance performance and longevity of 3DP restorations. MATERIALS AND METHODS: Five commercially available 3DP resins, both filled and unfilled, including 1) Sprintray Ceramic Crown, 2) Rodin Sculpture 2.0, 3) Rodin Titan, 4) Rodin Denture base 2.0, and 5) Sprintray High impact Denture Base were tested following five post-polymerization methods: 1)Sprintray Nanocure, 2) Otoflash with nitrogen, 3) Otoflash without nitrogen, 4) Oven, and 5)Sprintray Procure 2. Standardized bar-shaped, discs and pins specimens were fabricated using Sprintray Pro S and Asiga printers. Flexural strength was measured using a three-point bending test on an Instron 5566A machine; Vickers hardness values were recorded using a Buehler Wilson VH1202 Microhardness tester; DC was analyzed using Fourier-transform infrared spectroscopy (FTIR). Wear resistance was assessed by measuring height and weight loss after one million wear cycles on a pin on plate linear wear tester under simulated loading conditions. RESULTS: Post-polymerization method significantly influenced mechanical properties and wear performance. For filled resins, Otoflash with Nitrogen and Oven yielded the highest flexural strength and surface hardness. In unfilled resins, Otoflash with nitrogen and Nanocure methods showed comparatively better results. Degree of conversion was positively correlated with hardness and strength. Post-polymerization method significantly influenced mechanical properties and wear performance. For filled resins, Otoflash with nitrogen and Oven demonstrated the best wear resistance. In unfilled resins, the Oven and Otoflash with nitrogen methods exhibited the lowest wear loss, whereas Procure showed the highest wear. CONCLUSION: Post-polymerization protocols play a critical role in defining the final properties of 3D-printed dental resins. Selection of polymerization conditions tailored to material type can significantly improve structural integrity and wear behavior, thereby enhancing the clinical reliability of 3DP dental restorations.

Degree

thesis:*
Name thesis:degree_name
Master of Science in Design
Level thesis:degree_level
masters
Discipline thesis:degree_discipline
Restorative Sciences & Biomaterials
Grantor
Boston University
Year dc:date.issued
2027

Author and committee

dc:creator, dc:contributor.*
Author dc:creator
  • Gupta, Navika
Advisor dc:contributor.advisor
  • Giordano, Russell, ll
ORCID dc:identifier.orcid

Subjects

dc:subject × 7

Rights

Language dc:language.iso
en_US

Identifiers

dc:identifier.*
Handle dc:identifier.uri
https://hdl.handle.net/2144/52868

Chain of custody

source
Harvested from
Boston University
Base URL
open.bu.edu/oai/request
Last updated
2026-11-18
Source record
OAI-PMH GetRecord
citation

Gupta, Navika. Effects of polymerization on mechanical properties and wear of printed materials. masters thesis, Boston University, 2027. https://hdl.handle.net/2144/52868