Boston University
Evaluation of mechanical properties and load to failure of peek and 3D printed materials as an implant supported fixed complete denture framework
Abstract
dc:description.abstractObjectives: This study aims to systematically evaluate and compare the Mechanical properties and Load to Failure between two 3D printed materials (Titan, On X Tough2) and comparing them to PEEK as a suitable final framework material for Implant fixed complete dental prothesis. Materials and methods:Three groups of materials-PEEK (milled), On X Tough 2, and Titan (3D printed)-were tested. Standardized bar-shaped specimens were prepared for flexural testing using a three-point bending setup. Mechanical properties assessed included flexural strength, flexural modulus, and Young’s modulus. Fracture toughness was evaluated using notched specimens tested on a universal testing machine (Instron), and fracture energy and fracture work were calculated based on force-displacement data. Load to failure and area under the force-displacement curve were also measured to assess overall strength and toughness. Statistical analysis was performed using one-way ANOVA followed by post-hoc Bonferroni tests to evaluate differences among the materials (significance level set at p < 0.05). Results: PEEK demonstrated significantly superior mechanical properties compared to both 3D printed materials in all tested categories (p < 0.001). It exhibited the highest flexural strength (263.79 MPa), flexural modulus (9.17 GPa), and Young’s modulus (10,085 MPa), confirming its superior stiffness and resistance to deformation. PEEK also showed the highest fracture toughness (4.88), fracture work (1529.59 J/m²), and energy absorption metrics, making it the most resilient to crack propagation and impact forces. In load to failure tests, PEEK withstood the greatest force (1480.17 N), and had the largest area under the force-displacement curve, indicating exceptional toughness. Among the 3D printed materials, On X Tough 2 outperformed Titan in flexural strength (164.60 MPa vs. 147.22 MPa), flexural modulus (5.36 GPa vs. 4.18 GPa), Young’s modulus (5448 MPa vs. 163 MPa), and load to failure (922.08 N vs. 582.20 N). However, both materials exhibited comparable and substantially lower fracture toughness (2.01 for both). Energy absorption (area under the force-displacement curve: On X Tough 2: 195,851, Titan: 76,488) when compared to PEEK. These results highlight PEEK’s unmatched mechanical resilience and structural reliability for demanding clinical applications. Conclusion: This study confirms that PEEK exhibits superior mechanical performance compared to the 3D printed materials On X Tough 2 and Titan across all evaluated parameters, including flexural strength, stiffness, fracture toughness, energy absorption, and load to failure. PEEK’s exceptional resistance to deformation and fracture makes it the most suitable material for applications requiring high strength, durability, and structural integrity, such as implant-supported prosthetic frameworks. While On X Tough 2 demonstrated better performance than Titan in terms of stiffness and load-bearing capacity, both 3D printed materials remain inferior to PEEK and may only be appropriate for less demanding clinical situations. These findings support the continued use of PEEK as the benchmark material for high-performance dental prosthetics and highlight the need for further development of 3D printed resins to approach the mechanical reliability of traditional high-performance polymers.
Degree
thesis:*- Name thesis:degree_name
- Master of Science in Design
- Level thesis:degree_level
- masters
- Discipline thesis:degree_discipline
- Restorative Sciences & Biomaterials
- Grantor
- Boston University
- Year dc:date.issued
- 2028
Author and committee
dc:creator, dc:contributor.*- Author dc:creator
-
- Rabah, Bahaa
- Advisor dc:contributor.advisor
-
- Giordano II, Russell
Subjects
dc:subject × 1Rights
- Language dc:language.iso
- en_US
Identifiers
dc:identifier.*- Handle dc:identifier.uri
- https://hdl.handle.net/2144/53730