Abstract
dc:description.abstractObjective: This study compared the flexural strength and flexural modulus of interim resin bars fabricated with a 3D printable resin (C&B resin, Formlabs), a CAD PMMA disk (Telio CAD, Ivoclar Vivadent), a conventional PMMA resin (Telio Lab, Ivoclar Vivadent), and a Bis-acryl resin (TempSmart, GC America).Null Hypothesis: 1. There is no difference in mean Flexural strength between the printed C&B resin and the conventional interim materials.2. There is no difference in mean Flexural modulus between the printed C&B resin and the conventional interim materials. Materials and Methods: Four groups (n=10) included specimens (2 mm thick x 45 mm long x 12.7 mm wide) of 3D-printed composite-resin: [Temporary CB Resin/Formlabs, (CB)]; and three conventional materials: bis-acrylic resin [TempSmart/GC, (GC)], PMMA [Telio Lab C&B Material/Ivoclar Vivadent, (T)], milled PMMA (Telio CAD/Ivoclar Vivadent, (TC)). The 3D-printed group was designed using CAD software (Autodesk Inventor) and imported to 3D printer software (Preform); and printed at 90° orientation, 50-µm Z-axis layer height, using a 3D printer (Form 3; Formlabs). Post-print processing included immersion in 99% isopropanol (Form Wash; Formlabs), air-dry, and post-print curing for 30 minutes (Form Cure; Formlabs). Conventional materials were fabricated in a custom mold as a bulk block and then cut to a rough size with a precision saw (Isomet 1000; Buehler). All specimens were hand-ground and wet polished to the finished size with 360, 600, and 1200 grit SiC paper. Specimens were then thermocycled for 1,000 cycles (5 and 55°C) prior to three-point bend testing to determine the flexural strength and flexural modulus (2 mm/min crosshead speed). Data were statistically analyzed using one-way ANOVA, Games-Howell for flexural strength and Tukey post-hoc for flexural modulus (α=0.05)Results A one-way ANOVA with Tukey post-hoc test for flexural strength and flexural modulus was employed to analyze the data and evaluate the null hypotheses. It was found that auto-polymerizing PMMA (Telio Lab) had the lowest flexural strength (99.13 MPa) compared with a Bis-acryl resin GC (119.39 MPa), 3D printed CB resin (120.91 MPa), and PMMA Telio CAD (128.96 MPa). For Flexural Modulus, auto-polymerizing PMMA Telio Lab (2.58 GPa) showed the lowest value, followed by CAD/CAM PMMA (Telio CAD) (2,71 GPa). 3D printed CB resin, and Bis-acryl resin GC showed the highest values (3.96 and 3,93 GPa, respectively). Conclusion This study indicates a statistically significantly lower flexural strength for Telio Lab than all other groups (p<.005); no other significantly different means (p>.05) were detected for flexural strength. There was a higher mean flexural modulus for the Formlabs C&B resin and GC compared to either Telio Lab or Telio CAD (p < .005). There was no statistically significant difference in mean flexural modulus between the CB and GC group (p=.993) and between Telio Lab and Telio CAD (p=.682).
Degree
thesis:*- Grantor dc:publisher
- State University of New York at Buffalo
- Year dc:date.issued
- 2021
Author and committee
dc:creator, dc:contributor.*- Author dc:creator
-
- Van, Minh; 0000-0002-1165-9359
- Contributors dc:contributor
-
- Kim, Hyeongil
- Oral Sciences
Subjects
dc:subject × 2Rights
dc:rights- Statement dc:rights
-
- Users of works found in University at Buffalo Institutional Repository (UBIR) are responsible for identifying and contacting the copyright owner for permission to reuse. University at Buffalo Libraries do not manage rights for copyright-protected works and cannot assist with permissions.
- Copyright retained by author.
- Language dc:language
- eng
Identifiers
dc:identifier.*- Handle dc:identifier
- https://hdl.handle.net/10477/87896