Shear Bond Strength of Different Types of Zirconia Bonded with Self-Adhesive Resin Cement with and Without a Primer Application

Abstract

dc:description.abstract

Introduction: Zirconia dental restorations require different surface treatment than what isused for glass ceramics. Primers containing 10-MDP (10-Methacryloyloxydecyl dihydrogen phosphate) and air particle abrasion are frequently used surface treatment techniques on zirconia. Another method utilizes silica coating to link zirconia to resin with air particles coated with silane coupling agents. Several generations of zirconia with different yttria concentrations are now available. However, these generations of zirconia might not behave similarly to the conventional %3 mol yttria-stabilized polycrystalline zirconia. Aim: The first aim of this study was to assess the shear bond strength of self-adhesive resin cement alone and compare it to the shear bond strength of the same self-adhesive resin cement with a universal primer. The study's second aim was to evaluate whether there is a difference in shear bond strength of three generations of yttria-stabilized zirconia. Materials and methods: Three generations of zirconia were used in this study. 3mol% Yttria Tetragonal Zirconia Polycrystals (3Y-TZP, n= 60), 4mol% Yttria Tetragonal Zirconia Polycrystals (4YSZ, n= 60), and 5mol% Yttria Tetragonal Zirconia Polycrystals (5Y-TZP, n=60). All zirconia specimens were sandblasted with a tribochemical surface etch using Rocatec Plus. Zirconia groups were further divided into two subgroups; the first group was bonded with self-adhesive resin cement (SpeedCem Plus). The other group was bonded with the same adhesive cement after Monobond plus (MB+) application. Half of the specimens were tested 24 hours after bonding using a shear bond strength (SBS) test, and the other half were tested after 5,000 cycles of thermocycling. Results: There was no significant difference in SBS of different zirconia generations before and after thermocycling. A significant difference was observed between the two bonding techniques before, and after thermocycling. The group with Monobond Plus application exhibited no change in SBS after thermocycling. There was a significant difference between the two bonding procedures within the zirconia generations (3Y-TZP) and (5-TZP), with higher shear bond strength in the group with Monobond Plus application. Conclusion: Under the conditions used in this study, the use of a universal primer with a self-adhesive resin cement after tribochemical etching improved shear bond strength to zirconia.

Degree

thesis:*
Grantor dc:publisher
State University of New York at Buffalo
Year dc:date.issued
2022

Author and committee

dc:creator, dc:contributor.*
Author dc:creator
  • Abusharifa, Hanadi
Contributors dc:contributor
  • Kim, Hyeongil
  • Biomaterials

Subjects

dc:subject × 1

Rights

dc:rights
Statement dc:rights
  • Copyright retained by author. Users of works found in University at Buffalo Institutional Repository (UBIR) are responsible for identifying and contacting the copyright owner for permission to reuse. University at Buffalo Libraries do not manage rights for copyright-protected works and cannot assist with permissions.
Language dc:language
eng

Identifiers

dc:identifier.*
Handle dc:identifier
https://hdl.handle.net/10477/88399

Chain of custody

source
Harvested from
Buffalo
Base URL
ubir.buffalo.edu/oai/request
Last updated
2026-11-19
Source record
OAI-PMH GetRecord
related terms
citation

Abusharifa, Hanadi. Shear Bond Strength of Different Types of Zirconia Bonded with Self-Adhesive Resin Cement with and Without a Primer Application. State University of New York at Buffalo, 2022. https://hdl.handle.net/10477/88399