State University of New York at Buffalo
Fracture Strength of PEEK Hybrid Abutment Restored with Lithium Disilicate Crown
Abstract
dc:description.abstractThe purpose of this study was to compare the fracture strength of single lithium disilicate implant-supported crowns fabricated on two-piece abutments with various materials PEEK, zirconia, and lithium disilicate. Materials and methods: Thirty-six implants (Conical connection, 4.3 in diameter and 10 mm in length; Nobel Biocare, USA) were embedded in acrylic cylinders in the vertical position. An implant replica was placed at site maxillary left central on a typodont, then, a scan body (Nobel Biocare, USA) was used to scan the position of an implant using an intraoral scanner (TRIOS Design Studio; 3Shape A/S). A hybrid abutment and a crown were designed following a pre-operation scan (Dental System; 3Shape A/S). Then, 36 abutments were manufactured from the design using 3 materials; each 12: A) ZR - zirconia (IPS e.max ZirCAD Prime; Ivoclar Vivadent Inc.); B) LD- lithium disilicate (Ivoclar Vivadent Inc., IPS e.max CAD; Ivoclar Vivadent Inc.); C) PEEK - ceramic-reinforced PEEK (BioHPP, Bredent). Zirconia and lithium disilicate abutments were processed following manufacturers’ instructions. Titanium bases and intaglio surface of the abutments and the crowns were treated following the manufacturers’ instruction. Then, the abutments were luted on the titanium bases using a resin cement (Multilink hybrid abutment; Ivoclar Vivadent Inc.) under a constant pressure. The abutments were screwed on their assigned implants at 35 Ncm twice with interval time of 10 minutes. The designed crown was used to mill and process 36 lithium disilicate crowns. Intaglio surface of crowns were etched using hydrofluoric acid; then, a coupling agent (Monobond Plus, Ivoclar Vivadent Inc.) was applied on the intaglio surface of crowns, and they were luted on the assigned hybrid abutments using a resin cement (Multilink; Ivoclar Vivadent Inc.) under a constant pressure. All the restorations were then stored in 37°C distilled water for 24 hours prior to undergoing thermal-cycling between 5°C and 55°C with interval time of 30 seconds for 5,000 cycles. Then, they were subjected to dynamic loading in a computer‐controlled dual‐axis chewing simulator (Chewing Simulator CS‐4; SD‐Mechatronik, Westerham, Germany) for 1,200,000 loading cycles. Specimens were then assessed for screw loosening and incipient fracture visually and under low power (50×) stereo‐magnification. Specimens were then subjected to static load using a universal testing machine (MTS 858 mini bionix II; MTS Systems Corporation) at an angle of 30° degrees to the implant axis with a crosshead speed of 2 mm/min until failure occurs. All specimens were examined under stereomicroscope (DinoXLite; Dunwell Tech Inc.) (50×) to determine the mode of failure. One-way ANOVA (SPSS for Windows v16.0; SPSS Inc.) followed by a post hoc test was used to assess the effect of abutment material on the fracture strength of single implant-supported restorations at a significant level of .05. The failure modes were reported descriptively.
Degree
thesis:*- Grantor dc:publisher
- State University of New York at Buffalo
- Year dc:date.issued
- 2023
Author and committee
dc:creator, dc:contributor.*- Author dc:creator
-
- Kaenploy, Jekita; 0009-0004-2125-4357
- Contributors dc:contributor
-
- Sadid-Zadeh, Ramtin
- Biomaterials
Subjects
dc:subject × 1Rights
dc:rights- Statement dc:rights
-
- Copyright retained by author. Users of works found in University at Buffalo Institutional Repository (UBIR) are responsible for identifying and contacting the copyright owner for permission to reuse. University at Buffalo Libraries do not manage rights for copyright-protected works and cannot assist with permissions.
- Language dc:language
- eng
Identifiers
dc:identifier.*- Handle dc:identifier
- http://hdl.handle.net/10477/89004