Back to search

State University of New York at Buffalo

Evaluation of Flexural Strength and Microhardness in Interim Restoration Materials: Comparing Subtractive and Additive Manufacturing Methods

Abstract

dc:description.abstract

Introduction: There are a variety of materials currently available for use in prosthodontics to fabricate prostheses that help restore function, either in the short term as temporary materials or in the long term as definitive ones (1). There are many methods of fabrication, including milling, printing, and casting (2, 3). The material of interest is urethane dimethacrylate (UDMA)-based dental resin, it can be either milled or printed and can be used as an interim prosthesis in either fixed or removable prosthetics (4, 5). The company Graphy has developed a type of 3D printable urethane dimethacrylate resin for the fabrication of crown and bridge work. Graphy claims that their product has superior mechanical properties, higher flexural toughness and microhardness, compared to other printed materials on the market (6, 7). Objective: The aim of this study is to compare the flexural strength and microhardness of urethane dimethacrylate-based dental resin material (TC-80DP, Graphy), printed resin (C&B resin, Formlabs), and milled PMMA discs (Telio CAD, Ivoclar Vivadent), both with and without thermocycling.Materials and MethodsFlexural strengthA total number of six groups each one is made up from (n=10) specimens that either went Thermocycling or not (2.3 mm thick x 45 mm long x 12.7 mm wide) were tested (8). With 10 specimens per group for a total of 60 samples. For the thermocycling group, specimens were exposed to 5,000 cycles (5 and 55°C) prior to three-point bend testing to determine the flexural strength and flexural modulus (2 mm/min crosshead speed). Samples were tested within 24 hours after thermocycling. Data was statistically analyzed using one-way ANOVA, using a significance level of (α=0.05) (8-10).Micro Indentation HardnessFor micro indentation hardness, a total of six groups were tested. The three main groups of interest, with number of (n=10) for each group, were made. Micro indentation hardness testing was performed on specimens before and after thermocycling for thermocycling group, specimens were exposed to 5,000 cycles (5 and 55°C). Post-thermocycling micro indentation hardness was tested again on different areas of the same samples...

Degree

thesis:*
Grantor dc:publisher
State University of New York at Buffalo
Year dc:date.issued
2025

Author and committee

dc:creator, dc:contributor.*
Author dc:creator
  • AlBaghli, Abdullah; 0000-0002-2445-1434
Contributors dc:contributor
  • Kim, Hyeongil
  • Oral Biology

Subjects

dc:subject × 1

Rights

dc:rights
Statement dc:rights
  • Copyright retained by author. Users of works found in University at Buffalo Institutional Repository (UBIR) are responsible for identifying and contacting the copyright owner for permission to reuse. University at Buffalo Libraries do not manage rights for copyright-protected works and cannot assist with permissions.
Language dc:language
eng

Identifiers

dc:identifier.*
Handle dc:identifier
http://hdl.handle.net/10477/90282

Chain of custody

source
Harvested from
Buffalo
Base URL
ubir.buffalo.edu/oai/request
Last updated
2026-11-19
Source record
OAI-PMH GetRecord
related terms
citation

AlBaghli, Abdullah; 0000-0002-2445-1434. Evaluation of Flexural Strength and Microhardness in Interim Restoration Materials: Comparing Subtractive and Additive Manufacturing Methods. State University of New York at Buffalo, 2025. http://hdl.handle.net/10477/90282