Back to search

Schulich School of Engineering

Effect of Metallurgical Structure on Hydrogen Diffusion and Distribution in Steel

Abstract

dc:description.abstract

Hydrogen has been regarded as an ideal alternative to fossil fuels to achieve the 2050 net-zero goal while meeting the rapidly increasing energy demand. Transporting large amounts of hydrogen via pipelines is the most effective and economical methods. However, hydrogen embrittlement (HE) may occur to endanger the structural integrity and operational safety of the pipeline. Hydrogen induced pipeline degradation is strongly dependent on the trapping behavior of the steel lattice structure. Various microstructures often found in pipeline steel consist of features which serve as potential traps for hydrogen. These trap sites include dislocations, grain boundaries, alloying elements, defects and interfaces. Thus, it is important to study the effect of metallurgical structure on hydrogen diffusion and distribution in steel. In this work, we first used scanning Kelvin probe force microscopy (SKPFM) measurements and finite element modelling to study the diffusion and distribution of hydrogen atoms at metallurgical microphases contained in X52 pipeline steel. Results show that the pearlite contained in the steel is more stable than the ferrite during electropolishing, as indicated by the measured topographic profiles and contact potential differences (CPD). The hydrogen charging enhances the electrochemical activity of both pearlite and ferrite, as shown by increased contact potential differences and thus the decreased work function. As the hydrogen charging time increases, the contact potential differences of both phases further increase, implying that their activities increase with the H-charging time. The pearlite has a greater contact potential difference and thus a lower work function than the ferrite. This is associated with more H atoms accumulating at the pearlite than at the ferrite. The H atom diffusion and accumulation are affected by H diffusivity at phase boundaries, H-trap binding energy and the number of traps in the steel. Then, considering that some macroscopic defects such as dents, corrosion pits, and notches are found on X52 pipeline steel during its long-term service, causing local stress concentration, we investigated the distribution of hydrogen atoms at a notch on an X52 pipeline steel under various applied loads or displacements by using a scanning Kelvin probe and finite element modeling. Results show that when the stress concentration at the notch is elastic, the hydrogen atom diffusion and distribution are driven by stress, rather than strain, in the steel. However, when displacements are applied to the steel specimen, the strain dominates the H atom distribution. As the local stress or strain increases, the H atom concentration increases, as indicated by negative shifts of the contact potential difference. For newly constructed hydrogen transportation pipelines, it has been reported that using higher grade steels for large-scale, long-distance hydrogen transportation can effectively reduce overall costs. Thus, we analyzed the effect of metallurgical microphases on H-atom accumulation in the X80 steel. Results show that hydrogen charging elevates the electrochemical dissolution activity of both ferrite and bainite contained in X80 steel, as indicated by the increased contact potential difference and thus the decreased work function. The H atoms tend to accumulate at ferrite, making the local hydrogen atom concentration much greater than the concentration at bainite. This phenomenon may partially result from the mechanical polishing process applied during sample preparation. Given that ferrite is softer than bainite, it is more susceptible to the generation of a high density of dislocations during polishing. These dislocations can act as potential hydrogen trapping sites, promoting the accumulation of hydrogen in ferrite. This possible effect of polishing has now been noted to avoid any misunderstanding regarding the hydrogen distribution in X80 steel. The results imply that, compared with bainite, ferrite is the location to accumulate more hydrogen atoms initiating hydrogen-induced cracks once the local hydrogen atom concentration reaches a threshold value, particularly under external loading conditions during service. Furthermore, considering the new pipelines may be constructed in different environmental conditions, we used nanoindentation tests, combined with hydrogen permeation test to study the effect of solution pH and current density on H permeating parameters and nanomechanical properties of X80 pipeline steel. Results show that the steady-state hydrogen permeating current density, hydrogen permeating flux, and the hydrogen subsurface concentration obtained in 0.5 M H2SO4 solution are apparently greater than the parameters obtained in near-neutral pH NS4 and 0.1 M NaOH solutions. The changes in nanoindentation of the steel subjected to electrochemical hydrogen charging depend on the charging solution used. In the 0.5 M H2SO4 solution, as the electrochemical H-charging time increases, the nanoindentation of the steel continues to decrease. However, in NS4 and 0.1 M NaOH solutions, the steel nanoindentation increases with time. This phenomenon is attributed to the formation of corrosion product films on the steel surface. The softening and hardening transition phenomenon occurs on the steel subjected to electrochemical hydrogen charging. Although measurement errors may cause variations in the nanoindentation results, the evolution of nanoindentation upon electrochemical H-charging exhibits a discernible tendency. H atoms could affect the elastic modulus of steel. When electrochemical H-charging promotes a uniform distribution of H atoms within the steel, achieved through either extended charging time or application of a cathodic current density, the elastic modulus of the steel tends to increase.

Degree

thesis:*
Name thesis:degree_name
Doctor of Philosophy (PhD)
Discipline thesis:degree_discipline
Engineering – Mechanical & Manufacturing
Grantor
Schulich School of Engineering
Year dc:date.issued
2025

Author and committee

dc:creator, dc:contributor.*
Author dc:creator
  • Hu, Qing
Advisor dc:contributor.advisor
  • Cheng, Yufeng (Frank)
Committee members dc:contributor.committeemember
  • Egberts, Philip
  • Tiamiyu, Ahmed Alade
  • Lu, Qingye Gemma
  • Li, Huazhou Andy

Subjects

dc:subject × 1

Rights

dc:rights
Statement dc:rights
  • Unless otherwise indicated, this material is protected by copyright and has been made available with authorization from the copyright owner. You may use this material in any way that is permitted by the Copyright Act or through licensing that has been assigned to the document. For uses that are not allowable under copyright legislation or licensing, you are required to seek permission.
Language dc:language.iso
en

Identifiers

dc:identifier.*
Dc Identifier Citation
Hu, Q. (2025). Effect of metallurgical structure on hydrogen diffusion and distribution in steel (Doctoral thesis, University of Calgary, Calgary, Canada). Retrieved from https://prism.ucalgary.ca.

Chain of custody

source
Harvested from
University of Calgary
Base URL
ucalgary.scholaris.ca/server/oai/request
Last updated
2026-11-19
Source record
OAI-PMH GetRecord
citation

Hu, Qing. Effect of Metallurgical Structure on Hydrogen Diffusion and Distribution in Steel. Schulich School of Engineering, 2025. https://hdl.handle.net/1880/122437