Back to search

Centre for Materials Engineering

Degradation of the beta-alumina electrolyte in a zebra cell

Abstract

dc:description.abstract

Beta-alumina solid electrolytes studied were subjected to charge and discharge cycles in a secondary, high energy density Na/beta-al~mina/NaA1Cl 4/FeC1 2 cell (known as the Zebra cell) at 250 c. These electrolytes were studied by means of optical microscopy, as well as SEM and EDS analyses to establish possible failure modes. After cycling little discolouration, or impurity pickup was found to have occurred in the electrolyte. The forms of degradation of the beta-alumina electrolyte identified appeared to be a result of inherent flaws in the betaalumina electrolyte tube, problems due to protracted storage of the tubes, or an apparent interfacial film on the cathode/electrolyte interface. A lead wetting agent was used in the cells to enhance the wetting of the beta-alumina electrolyte by the liquid Na. A study of the this coating after cycling of the cell showed that the coating was adherent irrespective of the number of cycles completed. The coating did not appear to influence cracking of the electrolyte during cycling. Cracking of the beta-alumina electrolyte was found to have initiated from the Na/electrolyte interface. No evidence of crack initiation nor internal damage was found on the cathode/electrolyte interfac~. The cracks through the beta-alumina electrolyte wall were found to have sealed by the formation of a plug consisting largely of Na and Cl. on the basis of EDS analyses of the fracture surface of the sealed crack possible sealing mechanisms are proposed.

Degree

thesis:*
Grantor
Centre for Materials Engineering
Year dc:date.issued
1988

Author and committee

dc:creator, dc:contributor.*
Author dc:creator
  • Van Heerden, D P
Advisors dc:contributor.advisor
  • Hutchings, Ron
  • Ball, Anthony

Subjects

dc:subject × 1

Rights

Language dc:language.rfc3066
eng

Identifiers

dc:identifier.*
Dc Identifier Apacitation
Van Heerden, D. P. (1988). <i>Degradation of the beta-alumina electrolyte in a zebra cell</i>. (). ,Faculty of Engineering and the Built Environment ,Centre for Materials Engineering. Retrieved from http://hdl.handle.net/11427/40084
Dc Identifier Chicagocitation
Van Heerden, D P. <i>"Degradation of the beta-alumina electrolyte in a zebra cell."</i> ., ,Faculty of Engineering and the Built Environment ,Centre for Materials Engineering, 1988. http://hdl.handle.net/11427/40084
Dc Identifier Citation
Van Heerden, D.P. 1988. Degradation of the beta-alumina electrolyte in a zebra cell. . ,Faculty of Engineering and the Built Environment ,Centre for Materials Engineering. http://hdl.handle.net/11427/40084
Dc Identifier Ris
TY - Thesis / Dissertation AU - Van Heerden, D P AB - Beta-alumina solid electrolytes studied were subjected to charge and discharge cycles in a secondary, high energy density Na/beta-al~mina/NaA1Cl 4/FeC1 2 cell (known as the Zebra cell) at 250 c. These electrolytes were studied by means of optical microscopy, as well as SEM and EDS analyses to establish possible failure modes. After cycling little discolouration, or impurity pickup was found to have occurred in the electrolyte. The forms of degradation of the beta-alumina electrolyte identified appeared to be a result of inherent flaws in the betaalumina electrolyte tube, problems due to protracted storage of the tubes, or an apparent interfacial film on the cathode/electrolyte interface. A lead wetting agent was used in the cells to enhance the wetting of the beta-alumina electrolyte by the liquid Na. A study of the this coating after cycling of the cell showed that the coating was adherent irrespective of the number of cycles completed. The coating did not appear to influence cracking of the electrolyte during cycling. Cracking of the beta-alumina electrolyte was found to have initiated from the Na/electrolyte interface. No evidence of crack initiation nor internal damage was found on the cathode/electrolyte interfac~. The cracks through the beta-alumina electrolyte wall were found to have sealed by the formation of a plug consisting largely of Na and Cl. on the basis of EDS analyses of the fracture surface of the sealed crack possible sealing mechanisms are proposed. DA - 1988 DB - OpenUCT DP - University of Cape Town KW - Material Engineering LK - https://open.uct.ac.za PY - 1988 T1 - Degradation of the beta-alumina electrolyte in a zebra cell TI - Degradation of the beta-alumina electrolyte in a zebra cell UR - http://hdl.handle.net/11427/40084 ER -
Dc Identifier Vancouvercitation
Van Heerden DP. Degradation of the beta-alumina electrolyte in a zebra cell. []. ,Faculty of Engineering and the Built Environment ,Centre for Materials Engineering, 1988 [cited yyyy month dd]. Available from: http://hdl.handle.net/11427/40084

Chain of custody

source
Harvested from
University of Cape Town
Base URL
open.uct.ac.za/oai/request
Last updated
2026-11-26
Source record
OAI-PMH GetRecord
citation

Van Heerden, D P. Degradation of the beta-alumina electrolyte in a zebra cell. Centre for Materials Engineering, 1988. https://hdl.handle.net/11427/40084