THE LIFECYCLE OF ADVANCED FIBERS: (I) A NEW METHOD FOR THE FABRICATION OF FIEBRS, (II) THE FUNCTIONALIZATION OF ELECTROSPUN PLA/PLA-B-PEG FIBERS, AND (III) THE DEGRADATION OF CELLULOSE FIBERS BY OXYGEN PLASMA

Abstract

dc:description.abstract

This dissertation covers a broad spectra of fiber research that includes (i) fabrication, (ii) functionalization, and (ii) physical/chemical degradation. In the first stage of this dissertation, a new method for fiber fabrication that combines electro- and wet- spinning, Immersion Electrospinning, was developed to direct fiber deposition by the selective application of voltage. Next, electrospun PLA/PLA-b-PEG (Poly(lactic acid)/Poly(lactic acid)-b-Poly(ethylene glycol) fibers were studied for stability over time (i.e. aged). Fiber properties were studied under humid conditions and water wicking properties of PLA/PLA-b-PEG fibers came to an equilibrium fairly quickly. While the ability to wick water was lessened with aging, PLA/PLA-b-PEG fibers could still wick more than PLA fibers. In the next study, biotin was then added to PLA/PLA-b-PEG fibers (where Dimethylformamide, DMF, was the solvent). PLA/PLA-b-PEG/biotin fibers resulted in a greater amount of biotin reaching the surface of fibers compared to PLA/biotin fibers. Water stability tests, however, showed a weight loss of the samples over 1 and 7 days, correlating with biotin and copolymer loss. To reduce this loss, two solvents were investigated, 1,1,1,3,3,3-Hexafluoro-2-propanol (HFIP) and DMF. In addition, the PLA-b-PEG block lengths were tailored. Biotin was attached directly to PLA-b-PEG. HFIP spun samples resulted in less copolymer loss than DMF spun samples, but there was no biotin present at the surface of fibers. By changing the block lengths of PLA-b-PEG, the amount of copolymer and biotin leaching was reduced using DMF as the solvent, and there was still theoretically, enough biotin present at the surface of fibers for use in detection. Lastly, plasma was used to decrease the stability of (i.e. degrade) cellulosic yarns. With the application of oxygen plasma, severe degradation of of high molecular weight cotton yarns was achieved.

Degree

thesis:*
Name thesis:degree_name
Ph. D., Fiber Science and Apparel Design
Level thesis:degree_level
Doctor of Philosophy
Discipline thesis:degree_discipline
Fiber Science and Apparel Design
Grantor
Cornell University
Year dc:date.issued
2017

Author and committee

dc:creator, dc:contributor.*
Author dc:creator
  • Buttaro, Larissa M,
Chair dc:contributor.chair
  • Frey, Margaret W
Committee members dc:contributor.committeemember
  • Ober, Christopher
  • DeLisa, Matthew
  • Netravali, Anil

Subjects

dc:subject × 1

Rights

Language dc:language.iso
en_US

Identifiers

dc:identifier.*
Dc Identifier Bibid
9948767
Dc Identifier Other
ProQuest Submission ID: 10270
ProQuest Publication ID: 10277808

Chain of custody

source
Harvested from
Cornell University
Base URL
ecommons.cornell.edu/server/oai/request
Last updated
2026-11-19
Source record
OAI-PMH GetRecord
citation

Buttaro, Larissa M,. THE LIFECYCLE OF ADVANCED FIBERS: (I) A NEW METHOD FOR THE FABRICATION OF FIEBRS, (II) THE FUNCTIONALIZATION OF ELECTROSPUN PLA/PLA-B-PEG FIBERS, AND (III) THE DEGRADATION OF CELLULOSE FIBERS BY OXYGEN PLASMA. Doctor of Philosophy thesis, Cornell University, 2017. https://hdl.handle.net/1813/51544