Abstract
dc:description.abstractIn the present work charge carrier kinetics at the Si/SiNx interface are investigated. SiNx films deposited on silicon wafers by plasma-enhanced chemical deposition (PECVD) act as antireflecting and surface recombination passivating layers in solar cells. PECVD SiNx films are a low-temperature and cheap promising alternative to the standard silicon passivation method by thermal oxidation involving high temperatures. The aim of this work is to characterize the Si/SiNx interface by (photo)-conductance and impedance methods. Impedance (C-V) measurements have been performed on Si/SiNx Metal- Insulator-Semiconductor structures and (photo)electrochemical cells. A positive fixed surface charge density over 10¬12cm-2 and donor and acceptor- like gaussian distributions over 1011cm-2eV -1 around mid-gap have been found to characterize the Si/SiNx interface. This fixed charge brings the n-Si into strong accumulation regime and the p-Si into strong inversion regime without the need of an applied external voltage. Potential-modulated microwave reflection measurements have been proved to be a compatible and valuable characterization technique at electrochemical cells, confirming and complementing the impedance characterization. Cyclic voltammetry and photoelectrochemical measurements have shown that SiNx is not an inert layer in Si/SiNx devices. It has been proved that leakage currents change the Si/SiNx electronic configuration and that charge carriers can be exchanged between the layers. SiNx has proven to be not appropriate for (photo)catalytic applications in aqueous medias. Time Resolved Microwave Conductivity measurements have been performed on electrochemical cells as a function of the applied potential. It has been found that the SiNx passivation on Si wafers is induced by a field effect. Dark conductivity microwave measurements on p-Si/SiNx samples suggest a strongly reduced mobility of electrons at the interface, probably due to the presence of a high density of interface states. TRMC and Surface Photovoltage (SPV) measurements show a strongly non linear recombination behavior at low injection levels which is quenched with increasing injection level. This decay at low injection levels is not characteristic of p-Si/SiO2 and cannot be easily ascribed to a recombination over the potential barrier of the depletion layer.
Degree
thesis:*- Department dc:contributor.department
- Physik
- Year dc:date.issued
- 2009
Author and committee
dc:creator, dc:contributor.*- Author dc:creator
-
- Martínez Moreno, Elías
- Committee members dc:contributor.committeemember
-
- Profl. William D. Brewer
- Dr. Thomas Dittrich
Subjects
dc:subject × 7Rights
dc:rights.accessrights- Statement dc:rights.accessrights
-
- open access
- Licence dc:rights.uri
- Language dc:language
- eng
Identifiers
dc:identifier.*- URN
- urn:nbn:de:kobv:188-fudissthesis000000015539-1
- Identifier URI
- http://dx.doi.org/10.17169/refubium-14756
- Dc Identifier Other
-
FUDISS_thesis_000000015539
FUDISS_derivate_000000006960