The impact of different low-pressure plasma types on the physical, chemical and biological surface properties of PEEK

Abstract

dc:description.abstract

Due to its outstanding material properties, polyether ether ketone (PEEK) is increasingly used as a medical device material. But its surface energy is too low e.g. to achieve sufficient osseointegration, resulting in a biologically inert surface. Plasma treatment can modify the surface properties of PEEK by improving the surface energy and biological activity of PEEK and thus its osseointegration behavior. Plasma treatment can also improve the bonding strength between PEEK denture frameworks and veneering composites. The changes of PEEK surface characteristics after low-pressure plasma treatment (LPPT) may be based on both, physical and chemical changes. A better understanding of the effects induced by plasma treatment seems to be useful since low-pressure plasma processses show a high reproducibility. By now, there is no specific research reporting on the effects of LPPT on various surface characteristics of PEEK. Therefore, the purpose of this study was to assess the roughness, hydrophilicity, microhardness, crystallinity and biological activity of PEEK surfaces after the exposure to different LPPTs. For this, 218 PEEK samples in the shape of round discs were prepared and divided into 4 groups, according to the different LPPTs: 1. Untreated PEEK (n=32, without LPPT) 2. H-PEEK (n=62, hydrogen LPPT) 3. O-PEEK (n=62, oxygen LPPT) 4. H/O-PEEK (n=62, hydrogen/oxygen LPPT, mixing ratio 2:1) Compared to untreated PEEK, the hydrophilicity, surface crystallinity and micro-hardness of PEEK after LPPT were significantly increased, whereas the O-PEEK and the H/O-PEEK groups showed the highest hydrophilicity with a contact angle close to 0 degrees. This property occurred ten times faster under hydrogen/oxygen LPPT than under oxygen LPPT. Using a test force of 0.02 N, all groups showed significantly different micro-hardnesses. Cell culture tests with human osteoblasts (HOB) revealed significantly higher cell densities on plasma-treated PEEK surfaces compared to untreated PEEK, which might be due to better cell adhesion. The changes may have been caused by both the size and the chemical properties of the specific atoms used in the plasma chamber. In the future, further tests should be conducted to assess the duration of LPPT that causes the highest crystallinity. The effects on osseointegration should also be evaluated in vivo.

Degree

thesis:*
Department dc:contributor.department
Charité - Universitätsmedizin Berlin
Year dc:date.issued
2023

Author and committee

dc:creator, dc:contributor.*
Author dc:creator
  • Fu, Qian
Committee member dc:contributor.committeemember
  • N.N.

Subjects

dc:subject × 5

Rights

dc:rights.accessrights
Statement dc:rights.accessrights
  • open access
Language dc:language
eng

Identifiers

dc:identifier.*
URN
urn:nbn:de:kobv:188-refubium-37237-6

Chain of custody

source
Harvested from
Freie Universität Berlin
Base URL
refubium.fu-berlin.de/oai/request
Last updated
2026-11-19
Source record
OAI-PMH GetRecord
citation

Fu, Qian. The impact of different low-pressure plasma types on the physical, chemical and biological surface properties of PEEK. 2023. https://refubium.fu-berlin.de/handle/fub188/37237