dc:description.abstractIn this thesis the antiferromagnetism of NixMn100-x thin films in contact with ferromagnetic Ni film(s) in exchange-biased bilayers and trilayers on Cu3Au(001) is investigated by means of magneto-optical Kerr effect (MOKE). NixMn100-x ultrathin films (10≤x≤77) grow in layer-by-layer mode on Cu3Au(001) with face-centered tetragonal structure similar to its bulk form. NixMn100-x can couple to out-of-plane (OoP) as well as in-plane (IP) magnetized Ni films, the latter stabilized by Co under-layer deposition. The antiferromagnetic (AFM) ordering temperature (TAFM) of NixMn100-x films coupled to IP magnetized Ni increases significantly with decreasing x from ~50 to ~20%, whereas only a slight change in TAFM is observed for bilayers with OoP magnetized Ni as a function of x. The blocking temperature (Tb) is always higher for the IP case than for the OoP except for Ni50Mn50, where the reverse is true. The critical thickness of NixMn100-x for the onset of exchange bias (EB) decreases significantly for both coupling directions when decreasing x. These results suggest that for decreasing x, the non-collinear 3Q-like spin structure of NixMn100-x deviates, driven by composition-dependent strain, from a more-OoP to a more-IP configuration with an associated increase in magnetic anisotropic energy to establish EB at smaller NixMn100-x thicknesses. Trilayers of Ni/NixMn100-x/Ni (17≤x≤25) on Cu3Au(001) are studied in detail, while manipulating the easy axis of magnetization of one or both of the FM Ni layers by the deposition of an adjacent Co layer. For the trilayers the exchange bias field Heb is found to be always smaller than in the corresponding bilayers at similar temperatures. This difference of Heb increases as the thickness of the NixMn100-x layer decreases. At reduced thickness (27 ML) of NixMn100-x, along with a significant reduction in Heb, a markedly reduced Tb of ~150 K and ~90 K for trilayers with IP-IP and OoPOoP configurations of the FM layers, respectively, is observed compared to the bilayer. These results are attributed to some pinned magnetic moments located inside the bulk of the AFM layer which are equally shared by both interfaces. For the perpendicular configuration of the two FM layer magnetizations in trilayers, Heb and Tb are similar as in the bilayers. This indicates a 3Q-like AFM spin structure where the IP and the OoP spin components independently couple to the adjacent FM layer. Further two important observations are a training-induced positive EB shift, and a temperaturedependent sign reversal of Heb in trilayers when both FM layers are IP as well as OoP magnetized. The former is attributed to interlayer exchange coupling, and the latter to a competition between interlayer and interfacial coupling. Some signs of perpendicular interlayer coupling are also observed, which can be attributed to thickness fluctuations of the NixMn100-x film.
Degree
thesis:*- Department dc:contributor.department
- Physik
- Year dc:date.issued
- 2012
Author and committee
dc:creator, dc:contributor.*- Author dc:creator
-
- Khan, Muhammad Yaqoob
- Committee members dc:contributor.committeemember
-
- Prof. Dr. Wolfgang Kuch
- Prof. Dr. Robert Bittl
Subjects
dc:subject × 3Rights
dc:rights.accessrights- Statement dc:rights.accessrights
-
- open access
- Licence dc:rights.uri
- Language dc:language
- eng
Identifiers
dc:identifier.*- URN
- urn:nbn:de:kobv:188-fudissthesis000000038446-4
- Identifier URI
- http://dx.doi.org/10.17169/refubium-12295
- Dc Identifier Other
-
FUDISS_thesis_000000038446
FUDISS_derivate_000000011636