Ghent University. Faculty of Engineering and Architecture
Innovative superabsorbent polymers for crack mitigation of concrete structures : from laboratory to construction site
Abstract
dc:descriptionThere is no doubt that concrete is one of the most used and diverse building materials ever created by mankind. Concrete is everywhere in our daily life and for some structures we have the feeling that they will remain there for a lifetime. That might not really be true. Despite its considerable strength and technological development, the durability of concrete is frequently endangered by cracks that may not even be visible to the human eye (at least, initially). As old as the material itself, cracks are almost inevitable and can develop in a concrete structure at a very early age. They are intrinsic to the material, as a consequence of the shrinkage that follows cement hydration and their growth can be enhanced by environmental factors. Through cracks, a preferential pathway is built for the ingress of a vast number of aggressive substances that in time become responsible for the most common problems affecting concrete structures: carbonation, sulfate-attack, acid-attack and ingress of chlorides, being the key factors leading to concrete degradation, corrosion of reinforcement, spalling of concrete layers and consequently the reduction of the service life of a structure. Until recently, cracks were only dealt with by means of repairs and maintenance after their appearance, always resulting in addition costs. But is it possible to avoid cracks from forming in the first place? The answers is YES! Most of the mechanisms behind the formation of shrinkage cracks in concrete can be related to water movement in the hydrating cement paste e.g. the loss of water in the capillary pores or at the structure’s surface by means of drying (leading to drying and plastic shrinkage, respectively), and the consumption of water during hydration and development of tension in the capillary pores following self-desiccation (autogenous shrinkage). With advances in the field of concrete technology, shrinkage reducing admixtures have been developed and later on the concept of internal curing by adding water reservoirs in the mixture was introduced and explored (a clear example of that is the use of saturated light-weight aggregates). These solutions work to a certain extent, but other important questions might be raised. What if cracks occur nevertheless at a later age? Is it possible to make concrete mixtures, not only subjected to lower risk of early-age cracking, but also able to deal with future cracks by themselves? That question represents a very complex and dynamic context and the solution to that should be equally dynamic and versatile. One of the answers was found with the use of superabsorbent polymers. Superabsorbent polymers, or SAPS, are present in our daily life since a very early-age. One of the most common uses for SAPs is the production of hygiene products such as diapers, but they can also be found in a diverse range of applications from the food industry to agriculture. SAPs are composed of a 3D network of polymeric chains connected by means of crosslinkers and possess an incredible ability to absorb and retain water (sometimes even up to 1500 times their own weight). Such polymers can be produced and adapted to be stable in diverse media, allowing them to keep absorbing and releasing water for infinite times, as long as water is available. With such features, this material figures as a very promising answer to the question above. Given its absorption and retaining ability, SAPs can be used to promote internal curing in cementitious systems, reducing significantly the incidence of early-age cracks. Additionally, should cracks occur at a later age, SAP particles present at the cracked surface can re-swell and provide instant sealing and potentially promote healing, given that certain conditions are met. In that context, SAPs have been intensively studied as a chemical admixture for cementitious materials for the past 20 years and promising results have been found. In this thesis, ten different SAPs were studied with the main intent to reduce shrinkage cracking by means of internal curing and to provide concrete structures with the features of self-sealing and self-healing of cracks. Two commercially available SAPs based on acrylic acid, four “inhouse” developed SAPs based on sulfonates and four also “in-house” developed SAPs based on alginates were used. The water kinetics of SAPs and their effects on cement paste and concrete were investigated and two SAPs, being one commercial and one “in-house” developed, were selected based on performance criteria and used for the construction of crack-free large scale walls built with reinforced concrete and monitored under realistic conditions for a period of eight months. When tested in cement pastes the acrylic acid-based SAPs were found to have an absorption capacity of around 20 g of water per g of SAPs, with a controlled release taking place around the time when a solid skeleton is formed in the cement paste and autogenous shrinkage takes place. This controlled water release kept the internal relative humidity in the paste at higher levels for more than seven days and promoted a complete mitigation of autogenous shrinkage with limited reduction of compressive strength (below 20%) in comparison to a reference paste produced without SAPs. In contrast, the sulfonate-based SAPs presented an initially higher absorption capacity in cement paste, above 50 g/g and up to 180 g/g, and strong incontinent behavior that resulted initially in a partial reduction of autogenous shrinkage. Full mitigation demanded an increased amount of SAPs and water that resulted in a significant reduction of strength, up to 74% at the age of 28 days. An additional and innovative sulfonate-based SAP was developed with two types of crosslinkers, one of which being alkali-unstable. This double crosslinker feature enabled this new SAP to absorb a limited amount of water at the first stage (up to 13 g/g in cement paste) but with the potential for a considerable increase in absorption capacity upon hydrolysis of the alkaliunstable crosslinker when immersed in the alkaline environment of the cement paste. With this SAP, a full mitigation of shrinkage was achieved with a reduction of compressive strength below 30% at the age of 28 days. The alginate-based SAPs were used as promising alternative to reduce the negative effects of SAPs on the compressive strength. They presented a limited absorption capacity in cement paste (as low as 7 g/g). Amongst all tested SAPs the alginate SAPs promoted the lowest reduction of strength (between 10-18%) at 28 days. However, given their early release of water, only a partial mitigation of shrinkage was found, which gave no improvement over the addition of the same amount of water to a mixture without SAPs. During the investigation of the effects of SAPs on cement pastes, a detailed study about the determination of the time-zero as starting point for the measurement of autogenous shrinkage was conducted. The socalled “knee-point” of the autogenous strain curve was then selected as the most appropriate moment to start the measurements of autogenous shrinkage. This point represents the moment of transition of the cement paste from a fluid to solid state and can be directly derived from the autogenous shrinkage test (in this thesis performed with the use of corrugated tubes). The inclusion of SAPs in concrete mixtures showed evidence that the absorption capacity of SAPs in cement pastes could be used as a very good approximation for their absorption in concrete mixtures. The kinetics of water release observed for the pastes and their effects on the promotion of internal curing, and reduction of autogenous shrinkage, as well as the effects on the compressive strength were also found to be valid for concrete mixtures. The commercial SAPs promoted a complete mitigation of autogenous shrinkage in the concrete mixtures with a reduction of compressive strength at 28 days limited to less than 20%. The reduction of strength was found to be more intense at early ages but not so prominent at later ages (as of 28 and 56 days). In addition to the mitigation of autogenous shrinkage, the compressive strength of the mixtures with commercial SAPs was found to be at the same level or higher than for a concrete mixture where additional water was added to the same amount as in the SAP mixtures. The amount of additional water used for mitigation of autogenous shrinkage in the mixtures with the commercial SAPs was in line with the amount of water theoretically needed to compensate for the chemical shrinkage of the cement type used as binder in the production of the concrete mixtures. The use of SAPs with limited addition of water and a controlled water release also increased the salt-scaling resistance of concrete subjected to freeze-thaw cycles substantially. That was found to be mostly related to the reduction of the distance between the capillary pores and the macro-pores left by SAPs after water release. The double crosslinker feature of the innovative sulfonate-based SAPs showed its most promising application for the promotion of immediate sealing of cracked concrete specimens. A reduction of 72% in the water permeability of cracked specimens was found for the mixture with the sulfonate-based SAP, against 45% with the commercial SAPs (both in comparison to a reference mixture with no SAPs). In terms of compressive strength, a very similar result was found for both SAP mixtures: 16% reduction for the commercial SAP and 18% reduction for the “in-house” developed SAP. The inclusion of SAPs in the large-scale production of concrete mixtures in a concrete plant was possible without considerable changes to the existing mixing protocol. SAPs were easily transported together with other dry materials on a transporting belt normally used at concrete plants. To avoid moisture uptake during transportation and swelling prior to the mixing, SAPs were inserted in water-soluble bags that were completely destroyed during the mixing procedure and dissolved afterwards, enabling a homogenous distribution of SAPs over the concrete mass with very limited to almost no agglomeration. With one commercial and one sulfonate-based SAP and their combination, three walls with dimensions 14 m x 2.75 m x 0.8 m were built with reinforced concrete and were found to remain crack-free over the complete monitoring period of more than eight months. In contrast, two reference walls without SAPs and different water content (respectively same total and same effective water-to-cement ratio as the SAP mixtures) presented cracks already five days after casting. The use of optical fiber sensors and multi-reference electrodes embedded in the concrete (attached to the steel reinforcement) enabled the continuous and automated monitoring of both shrinkage deformation and corrosion potential in the walls. The total shrinkage strain measured by the optical fiber sensors was 63% lower in the wall with a combination of both SAPs than in the reference wall, at the age of 7 days. Furthermore, the strain level measured in the reference wall at the moment the first cracks were noticed (five days), was only recorded in the combined SAPs wall after 14 days. The multireference electrodes indicated a possible corrosion initiation near a cracked area of the reference wall around six months after casting. In contrast, no corrosion potential was measured in the SAP wall. To conclude, the use of SAPs for the production of large-scale elements under realistic conditions was proven to be successful from different perspectives: 1) SAPs could be easily introduced in the mixing routine of concrete plants without the need of significant changes in the mixing protocols; 2) SAPs promoted a considerable reduction in the total shrinkage strain of the concrete, especially during the first seven days, enough to avoid the formation and development of cracks; 3) the addition of SAPs enabled the reduction of (minimally) 10% in the amount of shrinkage reinforcement, in comparison to one reference wall without SAPs; 4) the effect of SAPs on the compressive strength of the structures was limited to a 17% decrease in strength; 5) the addition of SAPs would enable the concrete to self-seal and heal future cracks that might occur at later ages.
Degree
thesis:*- Grantor dc:publisher
- Ghent University. Faculty of Engineering and Architecture
- Year dc:date
- 2021
Author and committee
dc:creator, dc:contributor.*- Author dc:creator
-
- Tenório Filho, José Roberto
- Contributors dc:contributor
-
- De Belie, Nele
- Snoeck, Didier
Subjects
dc:subject × 1Rights
dc:rights- Statement dc:rights
-
- info:eu-repo/semantics/openAccess
- Language dc:language
- eng
Identifiers
dc:identifier.*- Identifier
-
https://biblio.ugent.be/publication/8715640
urn:isbn:9789463555050
https://biblio.ugent.be/publication/8715640/file/8715642