Back to search

University of Patras

Μέθοδος ταχέως προσδιορισμού κύριων συστατικών μεταλλουργικών σκωρίων (FeO, CaO, MgO, SiO2)

Abstract

dc:description

To investigate the ability of LIBS technique considering the rapid qualitative and quantitative analysis of metallurgic slag was the main objective of the particular thesis. Firstly, the LIBS technique applied on pure metals and then on samples containing the same metals in CaO matrix and the time-resolved characteristics of the plasmas produced by nsec and psec pulses were studied. Both the plasma temperature and electron density are decaying similarly and the space-averaged values determined in the nanosecond case are slightly higher than for the picosecond one. Moreover, the calibration curves obtained, show that the inherent sensitivity of the technique remains almost unaltered independently of the pulse duration. The detection limits were found to be few ppm. Then, the potentiality of LIBS method for quantitative on-line, multi-element slag analysis on plant scale was examined. Further, in order to examine more closely the produced slag, slag samples were analysed in the laboratory. The measurements were performed on solidified slag samples in a pelletized form and on as delivered solidified slag samples. The limits of the accuracy of this technique depend mainly on the laser spot/phase size ratio, the level of surface abnormalities and the distribution of each element in the matrix. The non-homogeneity level of the slag product seems to be not important in LIBS analysis, when the above ratio is quite large. It is of great importance whether the element is embedded in the matrix or in a specific crystallized phase. The influence of surface abnormalities is reduced in the case of pressed slag, but primarily for the elements distributed in the matrix, fragmentation of the slag should be avoided. The accuracy of LIBS quantitative slag analysis is strongly dependent on the standard samples that are used Regarding the liquid slag analysis, the calibration curves presented satisfactory linear dependence between the intensity of analytic lines with the corresponding concentrations while the intensity values of liquid slag appeared to be relatively increased with regard to the intensity values of solid slag under the same experimental conditions. Widening phenomena were characterized the lines of certain elements in liquid slag. For concentrations >4-5% an increased slope in calibration curves of liquid slag was observed. Finally, it was observed that each element behaves in a different way from sample in sample but also from phase in phase.

Degree

thesis:*
Grantor dc:publisher
University of Patras
Year dc:date
2008

Author and committee

dc:creator, dc:contributor.*
Authors dc:creator
  • Palagas, Christos
  • Παλάγκας, Χρήστος

Subjects

dc:subject × 16

Rights

Language dc:language
gre

Identifiers

dc:identifier.*
Identifier
10.12681/eadd/17981

Chain of custody

source
Harvested from
Greek National Archive of PhD Theses
Base URL
phdtheses.ekt.gr/eadd_oai/request
Last updated
2026-11-18
Source record
OAI-PMH GetRecord
citation

Palagas, Christos; Παλάγκας, Χρήστος. Μέθοδος ταχέως προσδιορισμού κύριων συστατικών μεταλλουργικών σκωρίων (FeO, CaO, MgO, SiO2). University of Patras, 2008. http://hdl.handle.net/10442/hedi/17981