Aristotle University Of Thessaloniki (AUTH)
Μελέτη κυτταρικής αντίδρασης στην τροποποιούμενη - με βιοπολυμερή ικριώματα - επιφάνεια οδοντιατρικών κεραμικών υλικών
Abstract
dc:descriptionTissue engineering is a quite promising science at the area of tissue regeneration. Scaffolds are commonly used in tissue engineering in order to provide a friendly micro-environment for 3D cell development. They have been used in soft and hard tissue development, commonly in medical practice. In dentistry, scaffolds have been used at periodontal regeneration and implantology. Moreover, in tissue engineering bioactivity and biocompatibility of materials is of great importance. Dental ceramic although is considered biocompatible, is incapable of interacting with the surrounding tissues. Bioactive modification of dental ceramic discs is already investigated. Coatings of bioactive glass – ceramic (1:1 wt), ceramic (50%), HAp (35%) and bioactive glass s (15%) (in system SiO2 45%, Na2O 24,5%, CaO 24,5%, P2O5 6%) and ceramic (50%), Al2O3 (7,5%) and bioactive glass (42,5%) were made. Furthermore, bioactivity of bioactive glass and hydroxyapatite (HAp) is well established, while in HAp is reported to be more chemically stable compared to bioactive glass. Moreover, materials like Al2O3 may reinforce dental porcelain and improve mechanical properties. Cell proliferation and morphology were investigated with scanning electron microscopy. Ceramic discs with coating of ceramic and bioglass (1:1) seem to benefit compared to all others. On these specimens, an HCAp film is developed at day 15th. Besides, Ca–P aggregates were observed at the surface. Overall, it could be concluded that the presence of Ca–P aggregates on the cells’ surface, enhances the hypothesis that PDLC interactions with modified ceramics might trigger the growth of such aggregates, while a network consisting of cells and Ca-P aggregates is continuously developing. Biopolymer scaffolds attached on bioactive glass modified dental ceramics could act as vehicles, in order to guide periodontal ligament cell (PDLC) proliferation and finally tissue development. This could have a beneficial effect on long term prognosis of fixed restorations. The aim of this study was to investigate the optimum proliferation pattern of human PDLC on composite scaffolds (chitin/chitosan/chitosan-gelatin), attached on bioactive glass modified dental ceramics. Three types of scaffolds were used: made of chitin, chitosan and chitosan – gelatin, with pore size 120- 250μm. They were fabricated thhrough Particulate leaching, supercritical CO2 foaming and Critical Point Drying, on the surface of ceramic disks, being coated with a mixture of bioactive glass – ceramic (1:1 wt) and thermally treated. The mostly used method, was Particulate leaching, in all cases. Composite scaffolds were incubated at 370C up to 15 days on well plates, either with culture medium (DMEM supplemented with 10% FCS) or with culture medium in the presence of 105 cells PDLC. To evaluate cell proliferation the MTS technique (Aqueous Non – Radioactive Cell proliferation assay, Promega) was used. Cell proliferation was evaluated at 1, 3, 7, 10 and 15 days. Finally, optical density (OD) was measured at a test wavelength of 490 nm and a reference wavelength of 630 nm. MTS assay. OD values of day 1 confirmed the presence of cells at all scaffolds. In cases of CHN and CHS, the number of attached cells was progressively decreasing, while the rate of cell death was significantly higher for CHN. On the contrary, proliferation rate on CH-G presented a peak after 7 days, a slowdown until day 12 and then attained a constant rate until the end of the experiment. In conclusion, all 3 types of examined composites ceramic-scaffolds were successfully loaded with PDL cells. However, only in CH-G composites ceramic-scaffolds the human PDL cells proliferated, then decreased and finally remained stable, while in case of CHN and CHS the number of cells was progressively decreasing. The successful cellular response could support the development of a protocol for tissue engineering on the materials used.
Degree
thesis:*- Grantor dc:publisher
- Aristotle University Of Thessaloniki (AUTH)
- Year dc:date
- 2009
Author and committee
dc:creator, dc:contributor.*- Authors dc:creator
-
- Θεοχαρίδου, Άννα
- Theocharidou, Anna
Subjects
dc:subject × 22- Ιστομηχανική
- Ικριώματα
- Βιοενεργότητα
- Ανάπλαση περιοδοντικού ιστού
- Κυτταρικός πολλαπλασιασμός
- Ανθρώπινα κύτταρα περιοδοντικού ιστού
- Χιτίνη
- Χιτοζάνη
- Ζελατίνη
- Tissue engineering
- Scaffolds
- Bioactivity
- Periodontal ligament regeneration
- Cell proliferation
- Human periodontal ligament cells
- Chitin
- Chitozan
- Zalatin
- Ιατρική και Επιστήμες Υγείας
- Κλινική Ιατρική
- Medical and Health Sciences
- Clinical Medicine
Rights
- Language dc:language
- gre
Identifiers
dc:identifier.*- Identifier
- 10.12681/eadd/20438