National Technical University of Athens (NTUA)
Διάβρωση μεταλλικών βιοϋλικών- εφαρμογές στην προσθετική και γναθοπροσωπική χειρουργική
Abstract
dc:descriptionDental casting alloys as biomaterials are widely used in applications that place them into contact with oral tissues for many years. Ni-Cr and Co-Cr casting alloys are part of the group of the predominantly base metal alloys which now account for the majority of the prosthetic restorations used clinically. Thus, it is of great importance that these alloys have high corrosion resistance. The in vitro corrosion behaviour of Ni-Cr and Co-Cr alloys for metal-ceramic restorations was investigated. For this purpose both electrochemical (linear and cyclic polarization) and non-electrochemical (ICP-AES, SEM/EDS) methods have been applied. The results show that the mean corrosion rates (μg/d.cm2) of 0,28±0,22, 0,193±0,18, 0,104±0,32 and 1,009±0,34 for WCER, W99, WBC and UNI alloy were estimated by ICP-AES measurements, respectively, after 64 days, whereas mean corrosion rates of 0,563±0,38 μg/d.cm2 for W99 alloy, 24±0.298 for WCER alloy, 0.347±0.57 μg/d.cm2 for WBC alloy and 3.215±0,53 μg/d.cm2 for UNI alloy were estimated by linear polarization measurements, respectively. The in vitro corrosion resistance of the four alloys according to immersion test and linear polarization are in the following order: WBC>W99>WCER>UNI. Therefore, UNI (Co-Cr alloy) has the lowest corrosion resistance and WBC (Co-Cr alloy) the highest. The corrosion properties of Ni-Cr and Co-Cr alloys are dependent on their chemical composition. The addition of Cr, W and Mo enhances their corrosion behavior. The results of SEM/EDS analyses reveal that Mo and W might be acting in the pits (active centers) reducing alloy corrosion and originating the heterogeneous surface. The in vitro corrosion of Ni-Cr and Co-Cr alloys leads to the release of very small amounts of metallic elements (Ni,Co,Cr,Mo). The clinical significance of our findings is unknown. Therefore, more biocompatibility testing in cell cultures and animal model is needed. Magnesium and its alloys are very promising metallic biomaterials due to their favorable mechanical and biological properties. In the field of interventional cardiology (stents), orthopaedic and maxillofacial surgery (bone regeneration), there is adequate evidence supporting the viability of magnesium as a biocorrodible/bioabsorbable biomaterial. The in vitro corrosion behavior of magnesium alloys designated as AZ31, Mg-pure, Mg-12Li, Mg-Ca was investigated. For the immersion test mean corrosion rates (CRWL) of 142,8± 1,09 mg/day.cm2 for Mg-pure, 0.4 ± 0,11 mg/day.cm2 for Mg12Li, 0,82± 0,14 mg/day.cm2 for Mg1Ca, 0.24 ± 0.06 mg/day.cm2 for Mg1Zn and 12,5± 0.94 mg/day.cm2 for AZ31, were estimated by weight loss, respectively. For the electrochemical corrosion tests the mean corrosion rates (CRLP) were estimated by linear polarization and were found to be; 1214,5±2,83 mg/day.cm2 for Mg-pure, 2,02±0,09 mg/day.cm2 for Mg12Li, 2.75±0,07 mg/day.cm2 for Mg1Ca, 1,016±0,09 mg/day.cm2 for Mg1Zn and 102,8 ±2,9 mg/day.cm2 for AZ31 alloys. Thus, the in vitro corrosion resistance of the four alloys according to immersion test and linear polarization are in the following order: Μg-pure >>AZ31>> MgCa > MgLi > MgZn. Mg and Mg(OH)2 was clearly detected in the XRD and EDS microanalysis results confirming the corrosion mechanism of magnesium, which includes the formation of a Mg(OH)2 surface layer. Peaks of CaO Mg and Mg(OH)2 were detected in the XRD analysis of the corroded MgCa alloy. Two areas having different compositions could be distinguished by EDS semi quantitative microanalysis. The smaller sized, brighter ones probably represent precipitates of chloride salts of Ca, Mg and Na, while the wide darker ones are richer in Mg(OH)2. SEM observation of the corroded Mg12Li shows regions with a relatively continuous corrosion layer and distinct regions covered with punctiform, needle-like corrosion products. The EDS analysis of the punctiform, needlelike corrosion products demonstrates a tendency to the enrichment in Mg which may be attributed to the selective dissolution of Li. Peaks of lithium were detected in the XRD analysis of the corroded Mg12Li alloy. The surface of the corroded MgZn alloy shows heterogeneous morphology with distinct shallow pits. Two regions having different compositions could be distinguished by EDS semi quantitative microanalysis. In the brighter ones Zn is detected while the wide darker ones are richer in Mg(OH)2. In general, it is believed that the dissolution process comes initially from a number of active centers. Zn might be acting in these centers reducing Mg corrosion and originating the heterogeneous surface verified through SEM analyses. Peaks of ZnO and Zn were detected in the XRD analysis of the corroded MgZn alloy. The biocorrodibility of the magnesium alloys should be further investigated both in osteoblast cultures and animal model. In addition it is recommended that magnesium alloys for bone regeneration should be porous.
Degree
thesis:*- Grantor dc:publisher
- National Technical University of Athens (NTUA)
- Year dc:date
- 2007
Author and committee
dc:creator, dc:contributor.*- Authors dc:creator
-
- Yfantis, Constantinos
- Υφαντής, Κωνσταντίνος
Subjects
dc:subject × 14Rights
- Language dc:language
- gre
Identifiers
dc:identifier.*- Identifier
- 10.12681/eadd/20730