National Technical University of Athens (NTUA)
Επίδραση της φυσικοχημικής συμπεριφοράς νικελιούχων λατεριτών στην ενεργειακή βελτιστοποίηση της πυρομεταλλουργικής τους κατεργασίας
Abstract
dc:descriptionThe objective of the present study is to contribute to the investigation of the physicochemical behaviour of laterite ores during their roasting reduction, in order to optimize the energy requirements of their metallurgical treatment. Roasting reduction constitutes a critical step of the pyrometallurgical treatment of nickeliferous laterites for ferronickel production. The energy requirements for this step are almost 65% of the total energy required to produce a ferronickel alloy of 12-14% in Ni, while at the same time this total energy corresponds to a very significant portion of the treatment cost. Therefore, the optimization of roasting reduction contributes significantly to the economics of the metallurgical process through improving its energy efficiency and reducing the frequency of the operational problems in the following step of smelting reduction. Within the framework of the current study, the reducibility of nickeliferous lateritic ores of domestic and foreign origin with a different mineralogical composition as well as the reducibility of the hematite mineral was investigated, giving special emphasis to the study of the rate controlling mechanisms in the various steps of reduction. The reducibility study included reduction experiments with gaseous (CO-N2) and solid (lignite and coke) reducing agents. The main part of the study was based on the experimental work including standard ASTM reduction tests with a gaseous reducing mixture (CO-N2), similar with the ASTM tests designed for the determination of the reducibility of iron ores. It comes from the experimental results that reducibility of the Greek nickeliferous laterite ore of intermediate type (ore of Kastoria origin) is significantly higher than that of the rest of the laterite ores examined under the same conditions. That is, reduction degree of Kastoria ore after 90 minutes in the temperatures 650 to 9000C, was ranging from 62 to 95%, whereas that of limonitic type of ores from Evia island and Lokrida, as well as an intermediate type of ore from Indonesia, was 26-49%, respectively. This result was verified for the ores in the form of grains (of 6 to 12 mm size), as well as various ore mixtures in the form of pellets. It was also deduced from this study that ore grain size and composition of the gaseous reducing mixture critically affect the results of reduction. Temperature favors the progress of reduction only within the range 650-7500C, whereas its effect is almost negligible within the range 750-9000C. Nevertheless, the effect of temperature is also critical within the range 750-9000C during reduction of laterite ores with a solid reducing agent (lignite). In such a case, it is considered that a temperature increase leads to the higher activation of the solid fuel, i.e. a more intensive reducing atmosphere due to the increased evolution of CO resulting from the gasification of fuel and the decomposition of hydrocarbons contained in its volatile constituents, resulting in an increased rate of reduction.
Degree
thesis:*- Grantor dc:publisher
- National Technical University of Athens (NTUA)
- Year dc:date
- 2010
Author and committee
dc:creator, dc:contributor.*- Authors dc:creator
-
- Zografidis, Charalabos
- Ζωγραφίδης, Χαράλαμπος
Subjects
dc:subject × 14Rights
- Language dc:language
- gre
Identifiers
dc:identifier.*- Identifier
- 10.12681/eadd/21132