Ανάπτυξη τραχύτητας κατά την εγχάραξη πυριτίου με πλάσμα για μικρορευστομηχανικές διατάξεις
Abstract
dc:descriptionThe purpose of this thesis is the characterization and explanation of roughness formation on silicon during plasma etching, the design, construction and sealing of silicon microfluidics and application of this microfluidics in affinity chromatography of phosphopeptides. In the first part of this thesis, an extensive study of the roughness formation on silicon surface during plasma etching is done, in order to know the maximum roughness expected during the fabrication processes of microfluidic devices, and its possible impact on their flow and other properties. SF6 gas is used for silicon etching in an ICP plasma reactor. Silicon surface etching leads to a dual scale morphology, which consists of underlying nano-roughness and superimposed much higher nano-mounds. For the dual-scale surface characterization a methodology is proposed, which is based on five roughness metrics: a) the root mean square of the surface heights rms, b) the correlation length ξ, c) the roughness component α, d) the mean width of the nano-mounds, and e) the mean distance of the nano-mounds. A mechanism which explains the dual scale roughness formation is proposed, according to which, inhibitors were deposited in the surface during etching and decrease the etching rate locally. There are two kinds of inhibitors: 1) the “hard” AlXFY that come from the alumina Al2O3 reactor dome and/or the anodised Al from the clamping ring, and are removed from the surface with ion sputtering, and 2) the “soft” inhibitors which can be large molecules or radicals and may be coming from the plasma e.g. SFx ή CFx or even products from the chemical reaction of the etching process In the second part of this thesis, we designed and fabricated two microfluidic devices, on Silicon one for liquid chromatography and another for gas flow. For the anisotropic etching of the silicon, the Bosch process was preferred method rather than the cryogenic method due to the higher etching rate and the smaller induced roughness. Regarding the sealing of the microfluidic devices, we preferred a bonding method with an intermediate layer. A lamination film with chemically inert and uniform glue was used for sealing the microfluidic devices for liquid flow. A bonding method with an intermediate layer provides a cheap, quick and easy solution, without the use of special equipment. In the third part of the thesis, the microfluidic devices for liquid chromatography were used for the separation of phosphopeptides with affinity chromatography and TiO2 as ligand. The deposition of TiO2 films in microfluidics devices may be made by bombardment of targets (rf sputtering) or by means of wet deposition by precipitation from “fluorotitanate” solution. In this thesis we used a solution of a mixture H2TiF6-H2ZrF6. The liquid deposition method creates TiO2-ZrO2 crystalline films. Affinity chromatography with TiO2 is a very good method for separating phosphopeptides.
Degree
thesis:*- Grantor dc:publisher
- National Technical University of Athens (NTUA)
- Year dc:date
- 2009
Author and committee
dc:creator, dc:contributor.*- Authors dc:creator
-
- Boulousis, Georgios
- Μπουλούσης, Γεώργιος
Subjects
dc:subject × 14Rights
- Language dc:language
- gre
Identifiers
dc:identifier.*- Identifier
- 10.12681/eadd/25565