Back to search

Aristotle University Of Thessaloniki (AUTH)

Συμβολή στη μελέτη της αντοχής στη διάτμηση του δεσμού μεταξύ εργαστηριακής σύνθετης ρητίνης επικάλυψης και πολυμερών ενισχυμένων με ίνες

Abstract

dc:description

Nowadays, the demand of more aesthetic prosthetic restorations increases constantly. This fact leads to the investigation to develop new materials with improved aesthetic characteristics. Such composite materials are the Fiber-Reinforced Composites (FRCs). They have been introduced for a variety of dental restorative applications. In Fixed Prosthodontics, FRCs are suggested to be used as substructures to provide increased strength and rigidity beneath the newer hybrid particulate filler composite veneering materials (laboratory composites or ceramic optimized polymer-ceromer). According to several studies, FRC substrates have high strength, almost equal to metals. However, in their clinical use it is reported that the veneering composite to the FRC frame bonding, might be inferior. The aim of this study was to compare the shear bond strength of a veneering composite (Adoro) to differently treated FRC (Vectris) substrates (flat surface, fiber net, rods). The use of a silane agent was also estimated. They were fabricated 117 specimens equally divided in nine groups. The veneering composite (SR Adoro dentin) was bonded to substrates of rectangular shape (10x10x1 mm) through a translucent celluloid tube with inner diameter of 5 mm and 3 mm height. In control group the substrates were made of a base metal alloy (4all). The rest groups included FRC substrates. In group 1, the FRC-substructures were flat and made of unidirectional glass fibers and a silane agent was applied. In group 2, the FRC-substructures were also flat with unidirectional glass fibers but without silane agent. In group 3, the FRC substructures were flat made of a glass fiber net where a silane agent was applied. In group 4, the FRC substructures were flat made of a glass fiber net but without a silane agent. In group 5, the FRC substructures had retentive rods on their surface and they were made of unidirectional glass fibers and a silane agent was applied. In group 6, the FRC substructures had retentive rods, unidirectional glass fibers but no silane agent. In group 7 the FRC substructures had retentive rods and made of a glass fiber net and a silane agent was applied and in group 8 the FRC substructures had retentive rods, fiber net but no silane agent. All specimens were thermocycled for 5.000 cycles in 5 oC and 55 oC for 30 s respectively and shear strength testing was performed at a constant crosshead speed of 0.5 mm/min according to ISO 10477. In order to characterize the fracture mode, the fractured specimens were examined under an optical microscope and selected specimens were examined in a Scanning Electron Microscope. Statistical analysis was performed applying ANOVA (one-way and factorial 3-way) and the Mann-Whitney, Kruskall- Wallis and Chi-square tests. Post-hoc tests were applied where necessary. According to the results, the values of the control group were statistically significant higher than the groups with flat surface and unidirectional fibers. Rods seem to increase the shear bond strength significantly when the FRC substructure is made of unidirectional glass fibers. Silane agent applied on the FRC substructure does not seem to increase the bond strength significantly. Mainly, the fracture mode is cohesive. When the fracture appears mostly inside the FRC substructure, the lower values are presented. Retentive rods seem to increase the percentage of the fracture inside the veneering composite. In conclusion, the resin-metal bond does not differ significantly to the FRC specimens with fiber net or rods. The cohesive mode of fracture presents a good FRC-resin bond. The lower values of the shear bond strength are found when the fracture appears mostly inside the FRC substructure and the higher when the fracture appears mostly inside the veneering composite. Retentive rods seem to increase the FRC-resin shear bond strength and to improve the mode of fracture. Silane agent does not seem nether to increase the shear bond strength neither to influence the mode of fracture.

Degree

thesis:*
Grantor dc:publisher
Aristotle University Of Thessaloniki (AUTH)
Year dc:date
2009

Author and committee

dc:creator, dc:contributor.*
Authors dc:creator
  • Antonopoulou, Athina
  • Αντωνοπούλου, Αθηνά

Subjects

dc:subject × 12

Rights

Language dc:language
gre

Identifiers

dc:identifier.*
Identifier
10.12681/eadd/25981

Chain of custody

source
Harvested from
Greek National Archive of PhD Theses
Base URL
phdtheses.ekt.gr/eadd_oai/request
Last updated
2026-11-18
Source record
OAI-PMH GetRecord
citation

Antonopoulou, Athina; Αντωνοπούλου, Αθηνά. Συμβολή στη μελέτη της αντοχής στη διάτμηση του δεσμού μεταξύ εργαστηριακής σύνθετης ρητίνης επικάλυψης και πολυμερών ενισχυμένων με ίνες. Aristotle University Of Thessaloniki (AUTH), 2009. http://hdl.handle.net/10442/hedi/25981