Back to search

Aristotle University Of Thessaloniki (AUTH)

Ανατομικά χαρακτηριστικά και τεχνικές ιδιότητες ξύλου πρεμνοφυούς καστανιάς (Castanea sativa Mill.) σε σχέση με την αξιοποίησή της

Abstract

dc:description

Anatomical characteristics, chemical, physical and mechanical properties were studied in wood from chestnut coppice forests. The average proportion of bark was 3,95%, of heartwood 91,60% and of sapwood 4,45%. The mean fibre length ranged from 0,95 mm-1,13 mm and was found to be reducing with the increase of ring width and increasing with the increase of age. The hot water soluble extractives content was of bark 26,33%, of heartwood 19,22% and of sapwood 7,08% and the dichloromethane soluble extractives content was of bark 2,43%, of heartwood 0,58% and of sapwood 1,09%. Between the bark, heartwood and sapwood were found differences in electrical conductivity (840 μS/cm, 349 μS/cm και 387 μS/cm respectively), acidity (pH) (4,60, 4,05 και 4,83 respectively), buffering capacity (acid equivalent) (0,0146 ml/ml, 0,014 ml/ml και 0,043 ml/ml respectively). The quantitative analysis of inorganic contents (ash) showed that the content was higher in bark (6,46%) and lower in sapwood (0,487%) and heartwood (0,118%). Differences were found as well at the qualitative analysis of ash for the elements Ca, K, Mg, Na, P, Mn, Cu, Zn and Fe. The extraction with hot water in all cases resulted in reducing of electrical conductivity and inorganic contents. Ring width ranged from 1,17mm-7,07mm was found to reduce from pith to bark. The average proportion of earlywood ranged from 7,72%-67,13% of ring width and was found to be reducing with the increase of ring width. The mean dry density of wood was 0,60 g/cm³, (from 0,57 g/cm³-0,63 g/cm³) and was found to be increasing with the increase of ring width and to be reducing with the increase of age. The extraction with hot water resulted in reducing of dry and basic density of wood. The average maximum shrinkage was 3,83% radically and 6,58% tangentially. Removal of hot water soluble extractives resulted in increasing of radial and tangential shrinkage. The mean shrinkage anisotropy was 1,74 and after extraction with hot water increased to 1,86. In extracted samples soaked in water was observed faster swelling at the beginning, in comparison to non extracted samples, but afterwards the difference was found to be reducing. The mean strength properties of chestnut wood in static bending were: modulus of rapture 107,79Ν/mm², stress at proportional limit 46,40Ν/mm2, modulus of elasticity 11,36 Ν/mm². The shear modulus of elasticity in GLT plane was 0,268 ΚΝ/mm² and in GLR plane 0,200 ΚΝ/mm². The mean strength of wood in axial compression was 0,268 ΚΝ/mm², the toughness 5,04 Joule/cm² and the mean lateral hardness (Janka) 41,11 Ν/ mm². In all cases between “immature” and “mature” wood were not found considerable differences in mechanical properties. Exposure of chestnut wood surfaces in atmospherical precipitation without covering or covered with water repellent substances of low effectiveness resulted in discolorations due to leaching of water-soluble extracts.

Degree

thesis:*
Grantor dc:publisher
Aristotle University Of Thessaloniki (AUTH)
Year dc:date
2009

Author and committee

dc:creator, dc:contributor.*
Authors dc:creator
  • Χαβενετίδου, Μαρίνα
  • Chavenetidou, Marina

Subjects

dc:subject × 18

Rights

Language dc:language
gre

Identifiers

dc:identifier.*
Identifier
10.12681/eadd/26205

Chain of custody

source
Harvested from
Greek National Archive of PhD Theses
Base URL
phdtheses.ekt.gr/eadd_oai/request
Last updated
2026-11-18
Source record
OAI-PMH GetRecord
citation

Χαβενετίδου, Μαρίνα; Chavenetidou, Marina. Ανατομικά χαρακτηριστικά και τεχνικές ιδιότητες ξύλου πρεμνοφυούς καστανιάς (Castanea sativa Mill.) σε σχέση με την αξιοποίησή της. Aristotle University Of Thessaloniki (AUTH), 2009. http://hdl.handle.net/10442/hedi/26205