Back to search

Aristotle University Of Thessaloniki (AUTH)

Φυσικοχημικές και μηχανικές ιδιότητες θερμικά τροποποιημένου ξύλου

Abstract

dc:description

In the frame of the present thesis dissertation, thermal modification of black pine wood (Pinus nigra) and poplar (Populus sp.) wood was conducted at a temperature of 180oC and 200oC, for 3, 5 and 7 hours in the presence of air and some of the most essential physical, chemical and mechanical properties of these materials were examined. It was observed that, as the intensity of heat treatment increases, the mass loss percentage of pine and poplar boards is increased due to the treatment, which is attributed to moisture loss of specimens and the degradation and loss of chemical wood components. After the treatment, the recovery rate of the initial weight of pine and poplar boards decreases, due to the reduced recovery of wood moisture content, while the equilibrium moisture content percentage, as well as the density of thermally modified samples of both species tends to decrease. Thermal modification considerably enhances the hygroscopic behavior of pine and poplar wood (adsorption, tangential-radial-longitudinal swelling percentages) and reduces in greater extent the swelling in tangential direction, compared to the radial one, contributing to the reduction of the anisotropy of wood. Increasing the treatment intensity, wood darkens and the index of L* decreases, referring to tangential, radial and cross-sectional surface of the specimens. The treatments increased the biological resistance of pine specimens against fungal attack of Coniofora puteana by 24.47% to 93.13%, compared to the control specimens, while against the action of the fungus Poria placenta the mass loss decreased by 28.75% - 68.46%. The mass loss percentage of poplar wood, because of the attack of Coriolus versicolor fungus decreased after treatment by 13.25% - 46.08% relatively to the control, and 31.98% - 64.72% against the action of Poria placenta fungus. Thermal modification did not effectively protect pine and poplar wood from mold growth, but contributed to a slowdown of its development. In the first stages of thermal treatments, the extractives presented a decrease, whereas as the duration and temperature of treatment increases, new extractives are formed. The lignin percentage recorded an increase to 180oC temperature treatments and even more at the treatments of 200oC. The percentage of holocellulose in all treatments was found to be lower in relation to the respective percentage of control, probably due to the intense decomposition of hemicelluloses. In the case of poplar wood, the holocellulose percentage marked slight reduction in the milder treatment, while increasing the duration and temperature, the percentage of holocellulose increased. The treatments of 180oC resulted in the improvement of pine bending strength, while treatments of 200oC temperature showed a decrease of 1.52% -16.97% in strength. The modulus of elasticity of pine specimens increased due to thermal treatment, regardless of the duration or temperature of treatment. In the case of poplar specimens, the resistance to bending forces decreased by 2.05% - 44.65% compared to control, due to the treatments. The elasticity of poplar samples decreased in all the cases of treatment (5.66% - 24.86%). The treatments of 180oC temperature increased the tangential hardness of pine wood by 6.58% - 15.13%, while in the treatments of 200oC this hardness improvement was limited to an increase of 4.20% and a reduction of 2.79% -13, 53% of hardness in subsequent treatments. The radial hardness was increased by 2.45% only in the milder treatment, while increasing the treatment intensity it decreased by a percentage between 1.36% and 30%. The tangential hardness of poplar modified at temperature of 180oC for 3 and 5 hours, decreased by 10.24% and 14.59%, respectively, while in the duration of 7 hours it grew by 2.35%, while at the treatments of 200oC it decreased again by 17.04 -26.05%. The radial hardness decreased by 2.81% - 11.06% at the treatments of 180oC (3 and 5 hours) and when the duration reached the 7 hours, it increased by 9.28%, while at the treatments of 200oC radial hardness levels of the specimens decreased by 2.68% - 18.86%. Treatments of 180oC (3, 5 and 7 hours) appeared to improve the impact bending strength of pine specimens by 41.81%, 27.59% and 7.33% respectively, compared to the control specimens, while the treatments of 200oC demonstrated a decrease of impact bending strength. All the treatments reduced the impact bending strength of poplar specimens, recording a decrease of 24.27% - 62.02%. Additionally, all the treatments raised the resistance levels to compressive forces of pine and poplar specimens, in relation to the control specimens. Only the milder treatment achieved to decrease the surface roughness of pine and poplar wood, while increasing the duration and temperature, the degree of roughness showed a strong increase compared to the control. After an exposure of 100 days of pine and poplar boards in external conditions, a similar degree of discoloration of control boards was observed in thermally modified boards, also demonstrated by the progress of L*, a* and b* of poplar and pine surfaces, which is probably attributed to leaching of the water soluble extractives. Wood also acquired a wilder look and new cracks appeared in the surface, while fungi infestation signs emerged most intensely in control and specimens of less intense treatments. The roughness of all of the exposed boards was found increased compared to the respective roughness values prior the exposure. The treatments of low intensity protected wood by reducing the roughness compared to the control, while treatments of higher intensity presented higher surface roughness values. Conclusively, the thermal treatment tends to enhance many crucial for the exploitation of these species attributes, greatly mitigates some of their major disadvantages and introduces these materials to an extensive range of applications of their potential future uses.

Degree

thesis:*
Grantor dc:publisher
Aristotle University Of Thessaloniki (AUTH)
Year dc:date
2015

Author and committee

dc:creator, dc:contributor.*
Authors dc:creator
  • Kamperidou, Vasiliki
  • Καμπερίδου, Βασιλική

Subjects

dc:subject × 16

Rights

Language dc:language
gre

Identifiers

dc:identifier.*
Identifier
10.12681/eadd/36186

Chain of custody

source
Harvested from
Greek National Archive of PhD Theses
Base URL
phdtheses.ekt.gr/eadd_oai/request
Last updated
2026-11-18
Source record
OAI-PMH GetRecord
citation

Kamperidou, Vasiliki; Καμπερίδου, Βασιλική. Φυσικοχημικές και μηχανικές ιδιότητες θερμικά τροποποιημένου ξύλου. Aristotle University Of Thessaloniki (AUTH), 2015. http://hdl.handle.net/10442/hedi/36186