The use of glass is as old as humanity and throughout human history it has been extensively used in countless applications. Initially in the form of obsidian (naturally occurring glass), glass has been used, amongst other, for the production of weapons and tools as well as for ornamental purposes. Consequently the capability to produce glass has rendered it the primary material used for packaging purposes as well as for the production of ornamental and tableware pieces. By any account soda-lime glass is presently the prevalent form of glass produced, since it is used for the production of countless widely used items. Indeed, in Europe soda-lime glass accounts for almost 90% of the total glass production. Additionally it should be noted that its particular physicochemical properties make it effectively irreplaceable in respect of numerous important applications, including medicine, architecture, energy, aeronautical engineering, food industry and information technology. Despite the fact that glass is one of the few 100% recyclable materials, the glass industry, which absorbs most of the used glass, is forced to discard large quantities primarily due to a) foreign impurities (metallic, ceramic and paper impurities) and b) the presence of mixed coloured glass cullet, which cannot be utilised for the production of flint glass. Therefore, it is imperative for the discarded quantities of glass cullet to be reused in existing product as well as in innovative applications and materials. Perhaps one of the essential parameters for the reuse of the discarded glass cullet and the more efficient absorption of the glass cullet from the new material is in relation to the determination of the quality of the surface of the cullet, namely the degree of deterioration and corrosion that it has sustained, since it is that surface that will come in contact with or will possibly react with other materials.Purpose of the present doctoral thesis is to map the deterioration that the glass surfaces have sustained and to examine the environmental factors that contribute to their degradation from the moment of their production, during their storage and up to the moment of their collection in recycling sites. The underlying aim, based on the behaviour of glass surfaces in different corrosive environments, is to minimise waste production by promoting their utilisation as resources, thus achieving higher recycling levels as those imposed as part of European’s Union Waste Management Policy. The originality of the present doctoral thesis consists in that:i)It engages in the examination of three different qualities of glass cullet, exhibiting different degrees of prior corrosion (production line, glass industry exterior storage sites, glass recycling facilities) for the four colours of glasses that the industry produces (flint, green, amber, blue), and on one hand analyses their reaction when exposed to environmental factors, thus providing answers on the effect of time and storage conditions by the industry, while on the other hand it records the mechanism of further corrosion during the reuse of glass cullet. ii)It examines the behaviour of and effect on the mechanical properties of mortars, when the building material is exposed in a fire environment. Such an examination is imperative in the field of building materials, which after all represents the second most important area where glass cullet can be used. iii)It utilises the Zeta potential as a “tool” for the determining the colour and quality of the glass cullet.The initial stage of the study focused on determining the chemical composition of the samples as well as their basic physical and mechanical properties.During the first circle of experiments, purpose of which was to assimilate “worst case scenario” conditions, grounded samples (<200μm) that had been chemically attacked with alkaline (Na2CO3, NaΟΗ) and acidic (HNO3, HCl, H2SO4) solutions and water (deionized, ultrapure) under varying temperatures (-20οC, 25οC και 60οC) for one hour, were used. The effect of deterioration was evaluated by determining the metals that were leached from the main silicate network and any chemical alterations that might have occurred by conducting FT-IR analysis, whereas the surface activation of the samples was evaluated by measuring their Zeta potential. The correlation of the qualitative and quantitative characteristics of the variables was conducted by utilising the Correspondence Factor Analysis technique. It was established that the negative redox value production line samples (flint and blue) suffer a higher degree of degradation when compared to the corresponding recycling sites samples, whereas the positive redox value recycling sites samples (green and amber) suffer a higher degree of degradation when compared to the corresponding production line samples. This finding can be attributed to the degree of prior corrosion of the material that forms part of the aggregated mass of the grounded material. Additionally, it must be stated that the Zeta potential is a very promising “tool” for determining the quality of the glass cullet. As a result of the alkaline attack there was a reduction in the absolute value of the Zeta potential value of the samples, whereas as a result of the acidic attack there was an increase in the relevant value, leading to more stable systems. During the second experimental circle the effect of alkaline, acidic and aquatic factors on flint and green glass samples, in the form of glass cullet 2-6cm2, under specific temperatures and time periods, was evaluated. The determination of their effect on the glass surfaces was determined by measuring the pH alterations of the deterioration solutions and by determining the metals that were leached from the main silicate network. Furthermore, the deterioration was also optically observed by conducting SEM analysis. It was established that the deterioration effect on recycling sites samples is greater something also evident during the optical observation of the samples, the surfaces of which were rougher as a result of the existence of craters and cracks. The higher deterioration effect can be attributed to their existence, since it led to porosity that allowed the diffusion of the solutions resulting in the reversal of the expected passivation from prior corrosion.In light of the results produced from the above mentioned experimental circles the study proceeded (third experimental circle) with the examination of the deterioration rate in acidic, alkaline and neutral environments of 60οC in bottles (filling the bottles and observing the effects on the inner surface), by determining the existing silica and calcium concentration levels. Additionally, XRD and FT-IR analyses were conducted in order to determine the nature and chemical composition of the secondary corrosion products generated after the alkaline attack. It was established that there as a was a slower deterioration rate in recycling sites samples, when compared to the production line and exterior storage sites samples, attributable to the robustness of the secondary corrosion products on the inner surface of the samples.Aim of the fourth experimental circle of the study was the evaluation of the deterioration in conjunction with the prevailing weather conditions (temperature, humidity, UV-radiation) in Greece during a full calendar year. This was achieved by emulating the weather conditions in an accelerated aging chamber using 5 individual weather condition programmes and one alternating weather condition programme. The evaluation of the effect that these parameters had on the final quality of the samples was determined by measuring the hardness of the samples, any colour alterations and the chemical durability of the samples. It was established that the individual summer and winter weather condition programmes have a greater effect on the samples, while the effect of the alternating weather condition programme will depend on the starting exposure conditions of the samples. The recycling site samples, when compared to those collected from the production line, are more vulnerable when modest spring and fall weather conditions are applied, but their properties remain relatively unaffected when exposed to summer and winter weather conditions.Finally, in order for the effect of the quality of the glass cullet to be evaluated that is the effect of the degree of deterioration on the mechanical properties of building materials, mortars by substituting aggregates or cement with multi-coloured glass cullet were created and the effect in respect of the granulometry (1-4mm και <90μm) as well as the substitution degree (5, 7,5 και 10%) were examined. The strength of the materials before and after their exposure to high temperatures, any changes in their microstructure by conducting XRD and SEM analysis and their thermal behaviour by conducting TG analysis was also examined. It was established that the sufficiently corroded glass cullet (SiO2 gel formation) can be used as a substitute for sand not exceeding 10%. As far as non-corroded glass cullet is concerned it can be used as a substitute for sand not exceeding 5% and for cement not exceeding 7,5%. Aim of the present doctoral thesis was to demonstrate the different behaviour that glass samples with different degrees of prior corrosion exhibit, establish the use of Zeta potential as a new method for the determination of the quality of glass cullet, examine the effect of climatological conditions on glass stored by the glass industry and finally consider the importance of glass cullet quality (corroded or not) when used for the production of building material that require exposure to high temperatures.Additionally and in light of the effect that climatological conditions can have on glass, glass industries are advised on the issue of during which seasons the production of specific types of coloured glasses should be preferred or avoided in order for their final properties to remain unaffected.

Degree

thesis:*
Grantor dc:publisher
National Technical University of Athens (NTUA)
Year dc:date
2016

Author and committee

dc:creator, dc:contributor.*
Authors dc:creator
  • Drosou, Christina-Amalia
  • Δρόσου, Χριστίνα-Αμαλία

Subjects

dc:subject × 18

Rights

Language dc:language
gre

Identifiers

dc:identifier.*
Identifier
10.12681/eadd/37796

Chain of custody

source
Harvested from
Greek National Archive of PhD Theses
Base URL
phdtheses.ekt.gr/eadd_oai/request
Last updated
2026-11-18
Source record
OAI-PMH GetRecord
citation

Drosou, Christina-Amalia; Δρόσου, Χριστίνα-Αμαλία. Διερεύνηση περιβαλλοντικών παραμέτρων και καθορισμός των μηχανισμών στην κινητοποίηση ιόντων πυριτίου σε υλικά με άμορφη δομή. National Technical University of Athens (NTUA), 2016. http://hdl.handle.net/10442/hedi/37796