Μελέτη και χαρακτηρισμός νέων βιοαποικοδομήσιμων πολυεστέρων
Abstract
dc:descriptionEnvironmental pollution due to synthetic polymers is continuously increasing to dangerous proportions and for this reason there is a growing demand for biodegradable polymers as a solution to solid waste management. In the present work three aliphatic polyesters, namely poly(ethylene adipate) (PEAd) poly(propylene adipate) (PPAd) and poly(butylene adipate) (PBAd) were synthesized and characterized by using the techniques of thermal analysis, nuclear magnetic resonance, FTIR spectroscopy, X-ray diffraction, scanning electron microscopy, gel permeation chromatography. Also, their intrinsic viscosities and mechanical properties were measured. The prepared polyesters were with high molecular weight and their hardness varied with chemical structure, PPAd being the softest, while PBAd had the better thermal stability. The decomposition kinetic parameters of all polyesters were investigated and calculated and the activation energies were estimated using the Ozawa, Flynn and Wall (OFW) and Friedman methods. Thermal degradation of PEAd is found to be satisfactorily described by one mechanism, with activation energy 153.2 kJ/mol, while that of PPAd and PBAd by two mechanisms having different activation energies: the first mechanism corresponding to a small mass loss with activation energies 121 and 185 kJ/mol for PPAd and PBAd respectively, while the second being attributed to the main decomposition mechanism, where substantial mass loss took place, with activation energies 156.7 and 217.2 kJ/mol, respectively. The form of the conversion function was the mechanism of n-order autocatalysis. The polyester PPAd demonstrates the highest biodegradation rates while the PBAd the lowest. The polyester PBAd was chosen as the most appropriate to be modified by the addition of multiwall carbon nanotubes (MWCNT's) and graphene oxide. For each from the above nanoadditives, nanocomposites materials were prepared, in various concentrations, by the solution method and they were characterized. The nanocomposites with MWCNT's exhibited, compared to the reference polyester PBAd, much better mechanical properties, lower rates of biodegradation, while their thermal stability and degree of crystallinity remained almost similar. The nanocomposites with graphene oxide exhibited relatively better mechanical properties, higher rates of biodegradation, a slight reduction of their thermal stability and increase in the degree of crystallinity along with increase of the crystal phase β.
Degree
thesis:*- Grantor dc:publisher
- Aristotle University Of Thessaloniki (AUTH)
- Year dc:date
- 2013
Author and committee
dc:creator, dc:contributor.*- Authors dc:creator
-
- Zorba, Triantafillia
- Ζορμπά, Τριανταφυλλιά
Subjects
dc:subject × 12Rights
- Language dc:language
- gre
Identifiers
dc:identifier.*- Identifier
- 10.12681/eadd/38794