Back to search

National Technical University of Athens (NTUA)

Αξιοποίηση ελληνικών καολινών στην τεχνολογία των γεωπολυμερών

Abstract

dc:description

The subject of this thesis is the exploitation of poor kaolins in geopolymer technology. The geopolymer technology has important applications both in the field of materials development and waste treatment. Geopolymer synthesis comprises a chemical reaction between an aluminosilicate material and an activation solution, under high alkaline conditions. The geopolymerisation of metakaolins coming from kaolins with varying chemical and mineral composition was studied. Initially, the alkaline dissolution of metakaolins and especially the effect of kaolins’ calcination temperature and the type of alkali ion were investigated. Then, the Taguchi model was applied in order to optimize the synthesis on the basis of higher compressive strength. The final products were examined by means of XRD, FTIR and SEM. Finally, the durability of geopolymer pastes and mortars at high temperature was investigated.All metakaolins exhibit high dissolution in alkaline solutions. The extent of dissolution depends on composition of the kaolin, the crystallinity of the kaolinite, the calcination temperature of the kaolin and the type of the alkali ion. Higher degree of dissolution is achieved in NaOH solution and calcination temperature of 650°C.Geopolymerisation is a complicated process affected, both, by the composition of the raw material and the activation solution. The Μ/Al, Na/(Na+K), [Si]/Μ2O (Μ: Na or/and K) ratios affect the properties of final products. In all cases, the factor, having the highest impact on the development of strength, is [Si]/M2O ratio, followed by M/Al ratio, while the kind of alkali ion has a marginal effect. For constant values of the above parameters, increase of solid/water ratio causes significant increase of compressive strength.The geopolymers exhibit strength up to 170 MPa and the presence of quartz and/or cristobalite in the raw material improves the strength. Thus, metakaolins derived from poor kaolins are preferable, against commercial metakaolins. The addition of crashed calcareous sand reduces the strength of mortars. The reduction is proportional to the percentage of sand. Mortars with sand/metakaolin ratio of 3.0 maintain 30-55% of the strength of the respective pastes. Geopolymers have satisfactory durability at high temperatures. At 600°C, pastes maintain up to 55% of their initial strength exhibit an 8% shrinkage while mortars maintain up to 40% of their initial strength with only 1% shrinkage.

Degree

thesis:*
Grantor dc:publisher
National Technical University of Athens (NTUA)
Year dc:date
2013

Author and committee

dc:creator, dc:contributor.*
Authors dc:creator
  • Tsitouras, Alexandros
  • Τσιτούρας, Αλέξανδρος

Subjects

dc:subject × 22

Rights

Language dc:language
gre

Identifiers

dc:identifier.*
Identifier
10.12681/eadd/39727

Chain of custody

source
Harvested from
Greek National Archive of PhD Theses
Base URL
phdtheses.ekt.gr/eadd_oai/request
Last updated
2026-11-18
Source record
OAI-PMH GetRecord
citation

Tsitouras, Alexandros; Τσιτούρας, Αλέξανδρος. Αξιοποίηση ελληνικών καολινών στην τεχνολογία των γεωπολυμερών. National Technical University of Athens (NTUA), 2013. http://hdl.handle.net/10442/hedi/39727