Μηχανισμοί διάβρωσης γυαλιού και τρόποι αποκατάστασής τους
Abstract
dc:descriptionThe aim of current PhD research is to investigate non-destructively glass corrosion and specifically metal-leaf glass tesserae from the wall mosaics of the Byzantine Monastery of Daphni (11th century). Metal-leaf (gold/ silver) glass tesserae were used in abundance for the byzantine wall mosaics, particularly when gold was established for the background. Metal-leaf is a unique type of glass tessera due to its sophisticated manufacture technique - a metal leaf is enclosed between two layers of normally transparent glass, the support glass and a second thin layer the top glass.The research comprise of a systematic macroscopic and microscopic examination of tesserae (detached and in situ) followed by analysis of selected tesserae-samples, as received, using scanning electron microscopy energy dispersive x-ray spectroscopy (SEM/EDX) and supplementary ion beam analyses, proton induced X-ray and γ-ray emission micro-spectrometry ( through the European programme CHARISMA Fixlab). After the completion of non-destructive evaluation, analysis of represented samples in cross-section was carried out, via SEM/EDX analysis.The study of the mosaics of Daphni Monastery revealed the use of metal-leaf tesserae of different glass colour (yellowish, aqua and roughly purple). The basic composition of the tesserae is a soda-lime-silicate glass of mixed type, a mixture of natron and plant ash glass. A low percentage of manganese and iron in the glass give the colour variations. Moreover, the discovery of a large number of gold tesserae deriving from the border of the glass slab, referred to as edges, facilitated the investigation of manufacturing technique.The condition of the metal-leaf glass tesserae is the combined effect of the alteration of the glass at the external surface and at the interface due to the presence of the metal leaf. Furthermore, non-destructive investigation facilitated the surface study of the altered glass areas, demonstrating that the altered glass exhibits a similar morphology independently the location: the external surface or the interface with the metal leaf (botryoidal and inverted botryoidal texture of the layers). Advanced corrosion on all the tesserae areas and particularly at the interface with the metal leaf, is associated with the creation of manganese-rich areas. Manganese rich areas were classified based on their morphology in spots, laminas and layers. The gold/silver tesserae constitute a category of artifacts with distinctive manufacture technique and characteristic way of alteration, mainly attributed to internal factors; appear to be less durable compare to the other types of glass tesserae. The decay of the examined tesserae is attributed to the combined effect of glass deterioration and corrosion of water, through the mortar.
Degree
thesis:*- Grantor dc:publisher
- National Technical University of Athens (NTUA)
- Year dc:date
- 2014
Author and committee
dc:creator, dc:contributor.*- Authors dc:creator
-
- Loukopoulou, Polytimi
- Λουκοπούλου, Πολυτίμη
Subjects
dc:subject × 27- Γυαλί
- Χρυσή/αργυρή γυάλινη ψηφίδα
- Διάβρωση γυαλιού
- Φαινόμενα διάβρωσης γυαλιού
- Μικροδομή διαβρωμένων περιοχών
- Θέσεις πλούσιες σε μαγγάνιο
- Ηλεκτρονική μικροσκοπία
- Φασματοσκοπία ακτίνων Χ
- Ιοντικές τεχνικές ανάλυσης
- Μικρο-φασματοσκοπία ακτίνων Χ και γ επαγομένων από πρωτόνια
- Glass
- Gold/silver leaf glass tesserae
- Glass corrosion
- Glass corrosion phenomena
- Microstructure of corroded areas
- Manganese rich areas
- Scanning electron microscopy
- Energy dispersive X-ray spectroscopy
- ion beam analyses; proton induced X-ray and γ-ray emission micro spectrometry
- Επιστήμες Μηχανικού και Τεχνολογία
- Επιστήμη Χημικού Μηχανικού
- Ανθρωπιστικές Επιστήμες και Τέχνες
- Ιστορία και Αρχαιολογία
- Engineering and Technology
- Chemical Engineering
- Humanities and the Arts
- History and Archaeology
Rights
- Language dc:language
- gre
Identifiers
dc:identifier.*- Identifier
- 10.12681/eadd/41607