Abstract

dc:description

Strong earthquakes of the last forty years have caused excessive damages and collapses of a large number of reinforced concrete (R/C) structures worldwide. The experience of earthquakes led to improved design methods of modern codes, which limit the damage of recent structures to acceptable levels. One of the most critical factors related to the safety of R/C structures is the premature failure of the lap-spliced column longitudinal reinforcement. This brittle failure significantly affects the hysteretic response of the columns, which are structural members of the vertical bearing system, resulting in rapid degradation of lateral strength, ductility, stiffness and energy dissipation capacity and possible loss of axial load carrying capacity, due to bond failure and excessive slipping of the bars. Consequently the inadequacy of lap splices may result in loss of the structural integrity and collapse.The last thirty years experimental and analytical investigation on the deficiency of lap splices in R/C columns was conducted and valuable knowledge has resulted. Thus, modern codes (EC2 and EC8, ACI-318) introduce the design of lap splices as tensile, rather than compressive splices. However, in existing structures of the 1960s–’70s and the older ones, the inadequacy of lap splices is also combined with poor (or even lack of) confinement and the use of plain steel bars and low strength concrete. Hence, these structures are extremely vulnerable to future strong earthquake excitations, since the seismic performance of the columns is significantly affected by the aforementioned deficiencies. Short length of lap splices (especially when unconfined) results in premature bond failure and slipping of the spliced column reinforcement prior to the development of the nominal moment flexural capacity. Moreover, when the columns of existing R/C structures are retrofitted, the flexural capacity of the strengthened columns may be overestimated if the spliced reinforcement is not effectively confined. The inadequacy of the lap splice length is also critical when the length of starter bars of columns found in existing R/C structures is short (or sometimes extremely short). Due to the severe deterioration of the overall seismic performance, caused by the inadequate lap splice length of the column reinforcement, special efforts is imperative to be made to prevent bar slipping and ensure load transfer between the bars and yielding of reinforcement. Therefore, the earthquake-resistant rehabilitation strategies aim to prevent lap splice failures mainly by implementing adequate confinement to the lap splice region. The restriction of bar slipping may also be achieved by welding the starter bars with the column reinforcement, although this requires more attention to the artful details of the welding. The last decades various strengthening techniques and retrofit schemes have been developed and applied by researchers, to prevent the early failure of lap splices in columns of existing structures. Nevertheless, due to the great importance of improving the load transfer mechanism between the spliced column reinforcement and the need for a reliable prediction of the lateral behaviour of columns with lap splices, further investigation is required in order to achieve a seismic response of existing pre-1960s-‘70s structures similar to that of modern ones. The present experimental and analytical investigation aimed to study: a.The effectiveness of thin steel jackets in improving the hysteretic response and ductility of columns with inadequate lap splices and in preventing the premature failure of the splices.b.The suitability of mechanical anchorages and efficiency of welded spliced reinforcing bars in restoring the load transfer mechanism between the starter bars and the column longitudinal reinforcement, when a column of an existing structure is extended.c.The influence of confinement in the overall seismic performance of columns with deficient lap splices when strengthened by R/C jacketing. The main objective of the analytical part of the present dissertation was to propose a model for predicting the lateral behaviour of lap splices of columns found in either existing or modern structures and also for determining the required amount of confinement during the retrofit process. The experimental part of the research (funded by the Greek Ministry of Infrastructures, Transportation and Networks and the Earthquake Planning and Protection Organization) included three series of almost full-scale column sub-assemblages (Series I, II and III). The first series included eleven (11) specimens and the main parameters examined were the lap splice length (equal to either twenty or twenty-four times the bar diameter, ds) and the steel jacket width (two values). The seismic behaviour of the pre-earthquake retrofitted column specimens was compared with the hysteresis of two original sub-assemblages with inadequate lap splices and a similar control specimen with continuous longitudinal reinforcement. The steel jacket width was calculated according to a proposed equation (Eq. 6.14a) in the Greek Code for Interventions and also according to a simplified form of this equation, which was not included in the Greek Code for Interventions. Both equations were subsequently evaluated.Series II included four (4) column sub-assemblages, in three of which the starter bars and the reinforcement of the new column were welded. In the forth specimen the continuity of reinforcement was achieved via mechanical anchorages. The effectiveness of the welding and mechanical anchorage of reinforcement was evaluated by comparing the hysteresis of the specimens with the seismic behaviour of a control specimen with continuous longitudinal reinforcement. In the third series ten (10) column sub-assemblages (five original and five pre-earthquake retrofitted) were constructed. One specimen, representative of poorly detailed columns found in pre-1960s structures with continuous longitudinal reinforcement, was strengthened by R/C jacketing and used as the control specimen. The other four original columns had deficient lap splices of length equal to either twenty (two sub-assemblages) or twenty four (two sub-assemblages) times the bar diameter. All columns were strengthened with R/C jackets according to the provisions of EC2 and 8. In one of the specimens with lap splices of 20ds length and in one of these with 24ds length the spliced reinforcing bars were welded prior to the construction of the jacket. In the case of the other two columns, additional transverse reinforcement in the form of ties (which was not part of the transverse reinforcement of the R/C jacket) was used to further confine the splice region of the existing structural member. This reinforcement was calculated according to an equation (Eq.8.3) proposed by the Greek Code for Interventions for improving the lap splice behaviour under seismic excitations to achieve yielding of reinforcement. Hysteresis of the sub-assemblages was evaluated with respect to the lateral performance of the control specimen, while Eq.8.3 was also evaluated. The proposed analytical model for predicting the lateral performance of column lap splices is an extended form of the analytical model proposed by the professor of Aristotle University of Thessaloniki A.-D. Tsonos, for preventing the collapse of R/C buildings subjected to seismic loading. Thus, the Tsonos model was slightly transformed to be applied in the lap splice region. With the proposed analytical model the following can be achieved:1.Adequacy control of the lap-splice length in columns of existing structures.2.Adequacy control of the lap-splice length in columns of modern structures.3.Adequacy control of the confinement provided by the jacket (from R/C, steel or from composite materials) during the retrofit process. Moreover, the implementation of the proposed model ensures the yielding of the spliced reinforcement and prevention of premature bond failure by accurately determining the required confinement that has to be applied to the splice region from the strengthening material. The accuracy of the analytical method was checked against experimental results from both the literature and the experimental work included in the present research.

Degree

thesis:*
Grantor dc:publisher
Aristotle University Of Thessaloniki (AUTH)
Year dc:date
2017

Author and committee

dc:creator, dc:contributor.*
Authors dc:creator
  • Kalogeropoulos, Georgios
  • Καλογερόπουλος, Γεώργιος

Subjects

dc:subject × 21

Rights

Language dc:language
gre

Identifiers

dc:identifier.*
Identifier
10.12681/eadd/42265

Chain of custody

source
Harvested from
Greek National Archive of PhD Theses
Base URL
phdtheses.ekt.gr/eadd_oai/request
Last updated
2026-11-18
Source record
OAI-PMH GetRecord
citation

Kalogeropoulos, Georgios; Καλογερόπουλος, Γεώργιος. Θεραπεία ανεπάρκειας μήκους παράθεσης του διαμήκους οπλισμού υποστηλωμάτων παλαιών κατασκευών οπλισμένου σκυροδέματος. Aristotle University Of Thessaloniki (AUTH), 2017. http://hdl.handle.net/10442/hedi/42265