Ανάπτυξη και εφαρμογή τροποποιημένων και σύνθετων νάνο-φωτοκαταλυτών SrTiO3 για την αποδόμηση οργανικών ρύπων σε υδατικά υποστρώματα

Abstract

dc:description

Nowadays environmental pollution is a global menace and the magnitude of it is increasing day-by-day due to urbanization, heavy industrialization and the changing lifestyles of people. Over the past several decades, a broad series of chemical contaminants (persistent organic pollutants, heavymetal, polychlorinated biphenyl) have been released to the environment by various industries, agriculture and traffic activities, personal care products as well as from poorly treated effluents from wastewater treatment plants. High production volume of such pollutants are continuously being released into waterbodies, and these have the potential to impact negatively on humans and ultimately upset the entire ecosystem. Over the last few years, environmental technologies have been devoted to improve conventional water and wastewater treatment methods and develop new and effective purification methods for wastewater treatment. Advanced Oxidation Processes (AOPs) are based in the generation of highly reactive radical species, mostly ●OH. AOPs are rapidly developing technologies against the conventional water and wastewater treatment methods. Among them, heterogeneous photocatalysis with semiconductors appears as a very emerging destructive technology. Photocatalysis with semiconductors has received great interest due to several advantages, such as the use of ambient conditions of temperature and pressure, the use of solar light, the absence of fouling, lack of mass transfer limitation, and the mineralization of organic pollutants into carbon dioxide, water and inorganic ions. In the present study titanate perovskites ATiO3 (A = Ca, Sr, Ba, etc.) were used. They are semiconductors with a wide band gap and interesting electronic, optical, magnetic and photocatalytic properties. They are considered promising materials for photocatalytic processes because of their strong resistance to photo corrosion, suitable oxidation potential and their high physicochemical stability. Among them, SrTiO3 is the most promising material for photocatalytic applications. It is a cubic perovskite (Pm3m, a = 3.9 Å) with an indirect band gap of 3.1–3.7 eV depending on the crystal structure and morphology obtained by the synthesis method. Therefore, SrTiO3 is an excellent photocatalyst only under UV light, which include about 5.0% of sunlight energy. Modification of SrTiO3 in order to increase absorptivity into the visible light spectrum has been made by N- and N,S- doping with the use of amino acids as dopant sources and by the formation of g-C3N4/ SrTiO3 composites with a mixing method. Amino acids are selected as doping agents because of their ability to form stable complexes with alkaline earth and transition metals. The selected amino acids were glycine, L-histidine and L-cysteine. The prepared materials had the following molar ratios and code names in parenthesis: (a) glycine dopant source: N:Sr:Ti 1:1:1 (G-N-STO1), 2:1:1 (G-N-STO2), 3:1:1 (G-N-STO3); (b) L-histidine dopant source: N:Sr:Ti 1:1:1 (H-N-STO); (c) L-cysteine dopant source: N:S:Sr:Ti 1:1:1:1 (C-NS-STO). A cleaning process was made for the as prepared materials. The materials G-N-STO1 and H-N-STO were washed with 50 mL of nitric acid 1M heated at 700C and the materials G-N-STO2 and G-N-STO3 with 100 mL of nitric acid 2M heated at 700C. In both cases after the cleaning procedure the samples were washed with distilled water. The C-NS-STO sample was washed with 100 mL 2M of both HNO3 and KOH which were both heated at 700C and then washed with distilled water. On the other hand, graphitic carbon nitride (g-C3N4) is a polymeric semiconductor with a mild band gap (2.7 eV) and a good response to visible light (up to 460 nm). The medium band gap, along with low cost, simple preparation method, high chemical stability, and non-toxicity, makes g-C3N4 appropriate for photocatalytic applications. Despite its remarkable electronic and optical properties though, g-C3N4 photocatalytic activity faces some limitations, such as high recombination of charge carriers, low conductivity, low valence band (VB) potential and small specific surface area (<10 m2/g). g-C3N4 has been widely used in formation of heterojunctions with perovskites, like SrTiO3, in order to improve their photocatalytic performance. The as-prepared samples contained different g-C3N4 to SrTiO3 amounts and had the following %wt content and code names (in brackets): i) 10% (% wt g-C3N4/SrTiO3) (10CNSTO) ii) 20% (% wt g-C3N4/SrTiO3) (20CNSTO) iii) 30% (% wt g-C3N4/SrTiO3) (30CNSTO) iv) 40% (% wt g-C3N4/SrTiO3) (40CNSTO) v) 50% (% wt g-C3N4/SrTiO3) (50CNSTO). Pure SrTiO3(STO) was used for comparison to the doped photocatalysts and for the comparison to the heterojunction oxides, g-C3N4 which had been sonicated for 1 h (CN) was used. All samples were characterized by X-ray diffraction (XRD), scanning electron microscopy (SEM), N2 porosimetry, UV-Vis diffuse reflectance (DRS), dynamic light scattering (DLS), point of zero charge (PZC) and fluorescence spectroscopy. The XRD patterns for the prepared N-doped and N,S-co-doped SrTiO3 photocatalysts were assigned to SrTiO3 perovskite phase with cubic symmetry. The sharp peaks indicate that the obtained powders are highly crystalline and free from impurities. The crystal size values of the N-doped with glycine photocatalysts are decreased while doping is increased. The crystal size of the N- and N,S- doped SrTiO3 ranged from 14.2 nm for the G-N-STO3 sample to 35.7 nm for the G-N-STO1 sample. SEM images for G-N-STO1, G-N-STO2 and G-N-STO3 show a porous structure with shapeless and irregular particles with internal cavities. The images revealed that all particles exhibited nearly identical morphologies, regardless the doping degree. On the contrary, the surface roughness increased with the nitrogen-doping degree. The images of H-N-STO present a similar but less stony structure. Finally, SEM images of C-NS-STO sample present a macroporous network with an interconnected structure into a single block of stone like a monolith. For G-N-STO1, G-N-STO2, G-N-STO3, H-N-STO and CN catalysts IV(a)—type isotherms with an H2(b) hysteresis loop were observed indicating mesoporous materials according to IUPAC classification. For G-N-STO1, G-N-STO2, G-N-STO3 and CN photocatalysts the existence of hysteresis loop is characteristic for the presence of mesopores while the peak at about 18 Ǻ in the PSD curves is due to the presence of finer pores (micropores). C-NS-STO material was non-porous and its isotherm belong to type II isotherms. Hydrodynamic particle size (median diameter) measurements were also performed by the dynamic light scattering (DLS) and the values ranged from 0.263 μm for G-N-STO1 to 0.337 μm for the C-NS-STO material. The G-N-STO1, G-N-STO2 and G-N-STO3 have PZC 6.95, 6.41 and 5.52 respectively. It is observed that while the N-doping increases in all three samples, PZC decreases. Also, the PZC of C-NS-STO and H-N-STO is 6.55 and 6.38 respectively. The Eg values of the N, NS doped photocatalysts had the following trend: H-N-STO> C-NS-STO, G-N-STO1> G-N-STO2> G-N-STO3. Among them G-N-STO3 presented the greater shift to the visible light region. The ability of the N, NS doped photocatalysts to generate ●OH followed the trend: G-NSTO3> G-N-STO2> G-N-STO1> C-NS-STO> H-N-STO. G-N-STO3 presented greater ●OH formation ability compared to all other prepared composites. The photocatalytic activity of the N-, N,S-co-doped SrTiO3 materials was tested against the degradation of methylene blue (MB) dye under UV-Vis and visible light irradiation following first order kinetics. The photocatalytic activity followed the same trend for both UV-Vis and Visible light irradiation: G-NSTO3> G-N-STO2> G-N-STO1> H-N-STO> C-NS-STO> STO. G-N-STO3 sample presented the higher photocatalytic activity. This result comes in agreement with the results of the characterization of the materials. G-N-STO3’s stability was investigated for three consecutive photocatalytic cycles. The intermediates of MB that were identified were the following: azure B (λmax: 648–655 nm), azure A (λmax: 620–634 nm), azure C (λmax: 608–612 nm) and thionine or phenothiazine (λmax: 602 nm). The photocatalytic activity of G-N-STO3 was also tested against the degradation of tris(2–butoxyethyl) phosphate (TBEP). The degradation followed first order kinetics. Ten transformation products (TP1 to TP10) were detected during the photocatalytic degradation of TBEP by the catalyst. The XRD patterns for the prepared g-C3N4/SrTiO3 heterojunctions were assigned to SrTiO3 perovskite phase with cubic symmetry. The sharp peaks indicate that the obtained powders are highly crystalline and free from impurities. The weak peak at 13.1o and the strong one at 27.4o represent the g-C3N4 surfaces. For the heterojunctions it can be observed that the crystal size values of the materials present a small variation, increasing along with the % content of CN until 30CNSTO, and then they decrease. The crystal size of the heterojunctions ranged from 17.1 nm for the 10CNSTO sample to 29.0 nm for the 30CNSTO sample. SEM images of the heterojunctions showed that after mixing with g-C3N4, the spherical particles of SrTiO3 were deposited in the CN sheet-stacks. 10CNSTO, 20CNSTO, 30CNSTO, 40CNSTO and 50CNSTO materials were non porous and their isotherm belong to type II- isotherms. Hydrodynamic particle size (median diameter) measurements were also performed by the dynamic light scattering (DLS) and the values ranged from 1.324 μm for the 10CNSTO material to 0.344 μm for the 30CNSTO material. The PZC of CN was determined to be 4.63. 10CNSTO, 20CNSTO, 30CNSTO, 40CNSTO and 50CNSTO presented PZC values 8.02, 7.90, 7.87, 7.79 and 7.65 respectively. It is observed that the increment of CN decreases the PZC of the composite materials. For the heterojunctions, Kubelka-Munk plots for each photocatalyst contain both the bands of CN and STO. Also it can be observed that with the increment of CN in the composites, the band of STO decreases. The Eg values for 20CNSTO for both bands were EgSTO= 3.28 eV, EgCN= 2.80 eV. The ability of the heterojunctions for the generation of ●OH followed the trend: 20CNSTO > 50CNSTO > 30CNSTO > 10CNSTO > 40CNSTO. 20CNSTO showed greater ●OH formation ability compared to all other prepared composites. The photocatalytic activity of the g-C3N4/SrTiO3 heterojunctions was tested against the degradation MB dye under UV-Vis and visible light irradiation following first order kinetics. The photocatalytic activity followed the same trend for both UV-Vis and Visible light irradiation: 20CNSTO > 30CNSTO > 40CNSTO > 50CNSTO ≈10CNSTO. 20CNSTO sample presented the higher photocatalytic activity. The result comes in agreement with the results of the characterization of the heterojunctions. 20CNSTO’s stability was investigated for three consecutive photocatalytic cycles. The Z -scheme mechanism is proposed for the photocatalytic activity of the heterojunctions. In the Z-scheme mechanism the photogenerated electrons in the CB of STO will combine with the photogenerated holes in the VB of CN while the accumulated holes with high oxidation potential in the VB of STO and electrons with high reductive potential in the CB of CN could produce easily •OH and O2•- which participate in the oxidative degradation of MB.Finally, the photocatalytic activity of TiO2, CN, 20CNSTO and G-N-STO3 was tested against pharmaceutical active compounds (PhACs) that were detected in real wastewater samples collected from the University hospital WWTP effluent of Ioannina city (N.W. Greece). These compounds were the antidepressant venlafaxine (VNX) and its metabolite O-desmethyl venlafaxine (ODV), the antipsychotic amisulpride (AMS), the antibiotic sulfamethoxazole (SMX) and the antiepileptic carbamazepine (CBZ). Their degradation followed pseudo-first order kinetics. The photocatalytic activity of all samples against the degradation of AMS and CBZ is described by the trend CN>TiO2>20CNSTO>G-N-STO3 while for SMX by the trend TiO2> CN>G-N-STO3. Against the degradation of VNX and ODV the photocatalytic activity of the materials followed the trend CN>TiO2>G-N-STO3>20CNSTO. For all PhACs 11 TPs were detected. TPs evolution as a function of irradiation time under TiO2 and CN photocatalytic treatment was also determined by UHPLC-Orbitrap MS. All TPs were irradiated for 180 min and they were completely or nearly degraded within this time.

Degree

thesis:*
Grantor dc:publisher
University of Ioannina
Year dc:date
2020

Author and committee

dc:creator, dc:contributor.*
Authors dc:creator
  • Konstas, Panagiotis-Spyridon
  • Κώνστας, Παναγιώτης-Σπυρίδων

Subjects

dc:subject × 14

Rights

dc:rights
Statement dc:rights
  • BY
Language dc:language
gre

Identifiers

dc:identifier.*
Identifier
10.12681/eadd/47658

Chain of custody

source
Harvested from
Greek National Archive of PhD Theses
Base URL
phdtheses.ekt.gr/eadd_oai/request
Last updated
2026-11-18
Source record
OAI-PMH GetRecord
citation

Konstas, Panagiotis-Spyridon; Κώνστας, Παναγιώτης-Σπυρίδων. Ανάπτυξη και εφαρμογή τροποποιημένων και σύνθετων νάνο-φωτοκαταλυτών SrTiO3 για την αποδόμηση οργανικών ρύπων σε υδατικά υποστρώματα. University of Ioannina, 2020. http://hdl.handle.net/10442/hedi/47658