Back to search

Aristotle University Of Thessaloniki (AUTH)

Μελέτη της προστασίας των υλικών κατασκευής αγωγών αποχετευτικών δικτύων από τη διάβρωση με την εφαρμογή καινοτόμων υλικών επίστρωσης ενώσεων μαγνησίου.

Abstract

dc:description

The proper functionality of sewage pipeline infrastructures is vital for urban community, as these systems are major contributors to maintain appropriate hygienic conditions, by transferring the urban sewage away from residential areas to wastewater treatment plants. However, a corrosive environment prevails in most sewer pipes, and this can lead to severe degradation and collapse of the pipe system, creating multiple safety, health, and financial problems (pipes’ repair or replacement). Microbiologically Induced Corrosion, which is a kind of corrosion created due to biological processes taking place in a sewer pipe, plays an important role to the pipes’ degradation, and it is responsible specifically for concrete deterioration, which is the main construction material especially of the larger diameter sewer pipes. Different corrosion mitigation methods can be used depending on the system characteristics and the experience of each wastewater management company. The use of protective coatings applied on the concrete pipe’s inner surface is a relatively inexpensive corrosion control method.The aim of this doctoral thesis is the study of magnesium oxide and hydroxide, as protective coatings applied onto concrete surfaces, against sulfuric acid corrosion, as well as the determination of the materials’ characteristics that enhance the anticorrosion properties of the coatings. The protective mechanism of these coatings is based on their increased alkalinity which blocks the development of microorganisms and their ability to react/neutralize the sulfuric acid, so that it cannot react with concrete.Firstly, preliminary studies were conducted to select the appropriate methodology, regarding the coatings’ adhesion improvement, the coatings’ application onto the substrate, the proper corrosion test and finally, the evaluation of the coatings’ anticorrosion performance. Based on the preliminary test results magnesium oxide and methylcellulose were chosen as adhesion promoters, as it was proved that they can enhance the adhesion of the magnesium hydroxide coatings. Moving on, the use of spatula was selected for the coatings’ application onto wet concrete surface. The use of spatula can help to the application of specific amount of coating, without any material losses, as those were observed in the case of a brush. As far as the corrosion test is concerned, sulfuric acid spraying tests were chosen, due to better simulation with the conditions existing in a sewer pipe and the proper conditions were defined. More precisely, two accelerated spraying tests were selected, a) a sulfuric acid spraying test with a handheld spraying machine, using a sulfuric acid solution of relatively high concentration (4 M) and b) a sulfuric acid spraying test in a spraying chamber, with a lower concentration sulfuric acid solution (0.2 M). Moreover, the evaluation of the coatings’ anticorrosion performance proceeded according to the materials’ characteristics and the bibliography. For instance, these materials tend to “soften” when they meet water, so the capillary absorption could not be evaluated. The parameters that were examined, were the pH surface values, the mass change, the thickness change, the concrete’s surface hardness and roughness, and the X-ray diffraction which was used to determine the formation of gypsum (corrosion product of concrete) before and after the corrosion tests.The first series of coatings was synthesized by combining magnesium oxide and magnesium hydroxide, using the oxide both as an adhesion additive, as well as an alkaline coating component, due to its ability to react with sulfuric acid. Four coatings were synthesized with different proportions of magnesium oxide and magnesium hydroxide (100:0, 80:20, 60:40 και 40:60, respectively) and applied onto appropriate concrete specimens. Uncoated concrete specimens were also used for comparison reasons. According to the results, the increase of magnesium hydroxide proportion led to lower adhesion ability of the coatings onto the concrete surface. However, the magnesium hydroxide proportion did not affect the anticorrosive behavior of each coating, since no differences were observed regarding the gypsum formation between the coated (with different coatings) specimens. All coatings preserved alkaline surface pH values during the spraying tests, hence blocking the microorganisms’ development. Based on the results, these coatings seemed to efficiently protect the concrete substrate, with only drawbacks their fast solidification and the reduced adhesion ability, compared to the following examined coatings.The second series of coatings consisted of magnesium hydroxide coatings with different starting properties, regarding their purity, surface area and particle size distribution, with the addition of methylcellulose, as adhesion promoter. The aim was to come up with conclusions about the properties that lead to the optimal desirable anticorrosion performance. During the acid spraying chamber test, two series of specimens were tested: a) dry condition coatings (dried for 3 days under laboratory conditions) and b) wet condition coatings (dried for 1 hour under laboratory conditions), so that the influence of coatings’ humidity to the coatings’ properties can be examined. Based on the results, the optimal protective performance depends on the combination of magnesium hydroxide powders’ properties. The higher purity and activity of the raw materials, from which the magnesium hydroxide powders were synthesized, seemed to enhance the purity of magnesium hydroxide powder and as a result its protective performance. Coatings with high purity raw materials preserved higher alkaline surface pH values during the spraying tests. Moreover, the larger particles did not favor the coatings’ activity, hence the protection of the coating. This fact was also obvious from the smaller formation of magnesium sulfate (hexahydrite), MgSO4 (product of the coatings’ reaction with sulfuric acid) and the lower pH surface values. The specific surface area did not seem to affect the coatings’ anticorrosion properties, but it affected the tensile bond strength values. All coated specimens presented zero gypsum formation during the spraying tests, a fact that confirms that the magnesium hydroxide coatings can protect the concrete substrate.Based on the previous-mentioned results, a magnesium hydroxide powder (M2m) was selected, which gathers the desirable properties, so that to be examined for its protection performance. The resulting coating was evaluated with the same methodology that all coatings were evaluated. However, a long duration spraying test (4 months/128 days) was also used in the case of this coating, with a smaller concentration sulfuric acid solution (0.1 M). The results showed that this coating presented satisfying performance, except the low hexahydrite formation, despite the relatively small particle size. Nevertheless, the coating preserved high pH surface values, and no gypsum formation was observed during the chamber spraying tests. The long duration spraying test showed that this coating can protect the concrete substrate for a long duration time (88 days of the 128 test days), by maintaining alkaline pH surface value. The gypsum formation was observed after the 68.7% of the theoretical time (128 days). Finally, an estimation of the coating’s real service life was made, based on the bibliography and the experimental results, and the result showed that the coating can efficiently protect the concrete surface for a period of 9-28 months, depending on the existing sewer pipe conditions (less or more adverse conditions, respectively).The experimental results of the magnesium hydroxide coatings, as well as of the magnesium oxide coating (100% magnesium oxide) were used for the multiple decision criteria analysis, performed with PROMETHEE method, to rank the coatings, regarding their protection ability. Three scenarios were examined, a) spraying with a handheld device, b) spraying dry coated specimens in a spraying chamber and c) spraying wet coated specimens in a spraying chamber. Moreover, the total ranking of the coatings was presented regarding all the scenarios. The comparison criteria were the tensile bond strength, the percentage of cohesive failure within the layer of the coating, the surface pH, the mass change, the surface hardness and roughness of concrete, the gypsum formation, and the coatings’ thickness. According to the total results, the selected coating (M2m) was amongst the four optimal coatings. However, other coatings presented better ranking, showing that the combination of high purity raw material and medium sized particles led to better anticorrosive characteristics, in contrast to the smaller particle size of M2m coating.Finally, a small part of this doctoral thesis concerns the study of selected coatings (all magnesium hydroxide coatings and one magnesium oxide coating) onto metallic substrates, as some sewer pipes, mainly those of smaller diameter, are made of metals. During this study, stainless steel 316, and hot-rolled mild steel specimens, both coated and uncoated, were used and subjected to sulfuric acid spraying tests. The coatings’ anticorrosion ability was evaluated by mass change and electrochemical impedance spectroscopy measurements. The results showed that these coatings can protect the metallic substrates existing into a sewer pipe. However, further research needs to be done.

Degree

thesis:*
Grantor dc:publisher
Aristotle University Of Thessaloniki (AUTH)
Year dc:date
2022

Author and committee

dc:creator, dc:contributor.*
Authors dc:creator
  • Merachtsaki, Domna
  • Μεραχτσάκη, Δόμνα

Subjects

dc:subject × 14

Rights

Language dc:language
gre

Identifiers

dc:identifier.*
Identifier
10.12681/eadd/52021

Chain of custody

source
Harvested from
Greek National Archive of PhD Theses
Base URL
phdtheses.ekt.gr/eadd_oai/request
Last updated
2026-11-18
Source record
OAI-PMH GetRecord
citation

Merachtsaki, Domna; Μεραχτσάκη, Δόμνα. Μελέτη της προστασίας των υλικών κατασκευής αγωγών αποχετευτικών δικτύων από τη διάβρωση με την εφαρμογή καινοτόμων υλικών επίστρωσης ενώσεων μαγνησίου.. Aristotle University Of Thessaloniki (AUTH), 2022. http://hdl.handle.net/10442/hedi/52021