Abstract

dc:description

The comprehensive understanding of the interaction between plasma and plasma-facing materials constitutes a critical issue for the safe operation of fusion devices and the prediction of the life time of the inner wall of fusion machines. The most important mechanisms that are caused by the plasma-material interaction are the surface erosion, the fuel retention and the migration and deposition of impurities on the plasma facing surfaces (PFSs) and the castellation sides of the first wall. Until 2009 the Joint European Torus (JET) tokamak operated with carbon as plasma facing material where high fuel retention was observed. So the period 2009-2011, the JET tokamak was transformed from a carbon to a full metal wall machine with beryllium in the main chamber and tungsten in the divertor (ITER-like wall), in order to investigate the results of the interaction between the plasma and the plasma facing components (PFCs) for the next generation fusion device, ITER. After the new wall installation, three D – D experimental campaigns were carried.In this work, the phenomena of material migration and deposition, fuel retention and surface erosion in samples from a) beryllium limiters and inner wall cladding (IWC) of the main chamber and b) tungsten lamellae from the divertor were investigated. The methodology was based on nuclear reaction analysis (NRA) and particle-induced X-ray emission (PIXE) employing deuteron and 3He ions, using milli- or micro-beams, X-ray fluorescence spectroscopy (XRF), scanning electron microscopy (SEM) with X-ray energy dispersive spectroscopy (EDS) and X-ray diffraction (XRD). Additionally, in order to obtain reliable quantitative results from the NRA measurements, the differential cross sections of the deuteron on beryllium reactions were measured for suitable angles and energies. The experiments were carried out at the Institute of Nuclear & Radiological Sciences and Technology, Energy & Safety (INRASTES), the Institute of Nuclear and Particle Physics (INPP) and the Institute of Nanoscience and Nanotechnology (INN) of NCSR “Demokritos” and at the Laboratory for Ion Beam Interaction (LIBI) of the Ruđer Bošković Institute (RBI) in Croatia. The cross sections of the 9Be(d,p0)10Be, 9Be(d,p1)10Be, 9Be(d,a0)7Li and 9Be(d,a1)7Li in the energy range Elab = 0.75 – 2.2 MeV with the non-constant energy step up to 1 MeV and then with a step of 20 keV were measured. The detection angles were 120o, 140o, 150o, 160o and 170o with respect to the beam direction. The thickness of the target was determined with proton and oxygen beams. The benchmarking using a bulk beryllium sample coated with a thin gold layer shows that the cross sections of the current work simulate the experimental spectra with deviation no more than 10%. The samples from the beryllium limiter marker tiles from the main chamber have a nickel interlayer between the top beryllium layer and the bulk beryllium. The aim of this interlayer is to assess the erosion of the samples. Apart from the erosion, the emphasis of the investigation was put on carbon deposition and fuel (deuterium) retention. Specifically, the carbon and deuterium amounts and spatial distribution and their correlation were investigated both on the PFSs and the castellation sides. For the quantification of the carbon amount and its spatial distribution the NRA technique employing deuteron milli- and micro-beam was used. The reaction for the carbon content determination was 12C(d,p0)13C. On the other hand, for the deuterium retention a 3He micro-beam was used as the most appropriate reaction to detect deuterium is 2H(3He,p0)4He. It was found that the carbon and deuterium amounts on the castellation sides are higher than those on the PFS. Furthermore, both the carbon and the deuterium amounts on the investigated castellation sides either stay constant or reduces with the depth from the edge of the PFS. The carbon amount is, in general, higher than the deuterium one. No systematic correlation between the carbon and the deuterium amounts have been observed. Moreover, the surface morphology, the erosion, the nickel (marker layer or deposition) distribution, the heavier material deposition, and the new compound formation were determined. Areas with melted surface, with intensive deposition, areas suffered enhanced erosion and others with mild or partial erosion were observed. The areas with intensive deposition present the higher carbon amount. On the other hand, the areas with enhanced erosion have the lowest carbon deposition. Nickel is the only element with inhomogeneous spatial distribution originating either from deposition or the marker interlayer. On the castellation sides areas rich in aluminium, chlorine, calcium, molybdenum and tungsten were detected. BeNi is formed on most surfaces.The carbon and oxygen amount as well as their depth profile were determined on the PFS of the inner wall cladding (IWC) and the dump plate (DP) of the main chamber. Additionally, the morphology, the heavier elemental distribution and the new compound formation were investigated. Generally, high carbon content is accompanied with high oxygen. The samples from the IWC have the highest carbon and oxygen content and their surface morphology seems unchanged after the plasma exposure. The samples of the ILWG1-3 3A8 from the DP have suffered melting. On the surfaces of the samples from the ILW3 2B2C from the DP oriented strips have been formed. Samples from W lamellae of tile 5 from the divertor were studied in order to determine the light elemental deposition and the corresponding depth profiles. Two of the investigated lamellae consist of a molybdenum interlayer between top tungsten and bulk tungsten in order to assess the surface erosion. The results were correlated with the strike point time. Additionally, the areas with different phases, the change of the surface morphology and compound formation after the plasma exposure were determined. The amount of the deposited beryllium and carbon increases with the strike point time. Beryllium deposition increases from the first to the second campaign and from the second to the third campaign. Carbon deposition decreases from the first to the second campaign but increases from the second to the third campaign, while there is no pattern for the oxygen amount. Furthermore, the carbon and beryllium concentrations are reduced with depth in a similar way for each sample, either abruptly or smoothly. The as-fabricated W lamellae installed in JET are characterized by a network of micro-cracks on the surface. After plasma exposure the morphology of their surface shows mild or strong plasma surface interaction. The density and the width of the micro-cracks were affected in the lamellae from the stack C and after the second campaign. Plenty of heavy elements were detected, on deposition areas of all the samples. The marker lamellae have been eroded up to 6 μm maximum, which is considered as mild erosion.

Degree

thesis:*
Grantor dc:publisher
National Technical University of Athens (NTUA)
Year dc:date
2023

Author and committee

dc:creator, dc:contributor.*
Authors dc:creator
  • Tsavalas, Pavlos
  • Τσαβαλάς, Παύλος

Subjects

dc:subject × 14

Rights

Language dc:language
eng

Identifiers

dc:identifier.*
Identifier
10.12681/eadd/53405

Chain of custody

source
Harvested from
Greek National Archive of PhD Theses
Base URL
phdtheses.ekt.gr/eadd_oai/request
Last updated
2026-11-18
Source record
OAI-PMH GetRecord
citation

Tsavalas, Pavlos; Τσαβαλάς, Παύλος. Investigation of plasma facing materials at JET Tokamak. National Technical University of Athens (NTUA), 2023. http://hdl.handle.net/10442/hedi/53405