National Technical University of Athens (NTUA)
Εφαρμογή γεωπολυμερισμού για την αξιοποίηση της ιπτάμενης τέφρας στην τεχνολογία σκυροδέματος
Abstract
dc:descriptionThe subject of the doctoral thesis is the application of geopolymers for the utilization of fly ash in concrete technology. Fly ash (FA) is a by-product of coal combustion in power generation plants, accounting for approximately 37% of the global energy mix over the past 50 years. The annual global production of FA is around 600 million tons, and it is projected to exceed 1.04 billion tons by 2030, of which only 6.5% is currently utilized. The domestic production of FA from 2019 to 2022 is approximately 3.5 million tons per year, with only 3% being used. The application of geopolymer technology to a wide range of solid industrial waste and byproducts of aluminosilicate composition for the production of structural materials presents a particular interest.In the initial phase, geopolymer pastes (GFA) were prepared using fly ash (FA) with fixed molar ratios of silicon to alumina (Si/Al=2.40) and alkalis to alumina (R/Al=0.85), but at different solid-to-liquid (S/L) ratios. The selected S/L ratios were 2.8, 2.9, 3.0, 3.1, and 3.2, as the literature suggests that the most commonly chosen ratio for fly ash geopolymerisation is 3.0. The variation in the S/L ratio was solely due to the addition or removal of a certain amount of water. Subsequently, for selected S/L ratios (3.0 and 3.2), four chemical additives of cementitious materials with different properties were used at various addition percentages. The produced GFAs of all the mentioned compositions were measured for setting time, workability, drying shrinkage, sorptivity and uniaxial compression strength. Depending on the case, the GFAs were either kept in the laboratory environment during their curing or underwent an initial stage of curing at 70°C for 2 days. The obtained results were compared with the requirements and conformity criteria specified in the corresponding cement standard, ELOT EN 197-1, as well as relevant related research.In the second phase, three geopolymer concretes (GC) were prepared with different content of FA by volume, 15%, 22.5%, and 30%. The selection of the content was based on literature references regarding the maximum cement content in concrete. For all GC compositions, the S/L ratio was fixed at 3.20, Si/Al ratio at 2.90, and R/Al ratio at 1.00. Additionally, for comparative purposes, three conventional concretes (CC) of suitable composition and mechanical properties were prepared for direct comparison with GC. The CC specimens were cured according to the requirements of the national Concrete Technology Regulation (KTS-2016), while the GC specimens underwent an initial stage of curing at 70°C for 2 days and were subsequently maintained in the laboratory environment until they were tested. The produced GC and CC specimens of all compositions were measured for their workability, air content, density, compressive strength, modulus of elasticity, Poisson’s ratio, tensile strength via cylinder splitting and beam bending, ultrasonic pulse velocity (UPV), sorptivity and porosity, durability to freeze – thaw and wet – dry cycles, chloride ion penetration, resistance to corrosive environments containing sulfur ions at two different temperatures (5°C and 20°C), as well as resistance to acids, acetic and sulfuric. The obtained results were compared with the requirements of the prevailing regulations for concrete, KTS-2016 and Greek Reinforced Concrete Regulation (EKOS 2000), as well as relevant related research.Taking the above into consideration, it is evident that the S/L ratio in geopolymer paste does not significantly affect the uniaxial compressive strength and setting time but does have a significant contribution to the workability of the geopolymer. Additionally, it appears that the studied chemical additives do not all perform in the same manner as in conventional concrete. The GC demonstrated competitive strength in compression comparable to CC, tensile strength within the limits specified by EKOS 2000 for CC, and an elastic modulus approximately 50% lower than that of CC. The content of geopolymer paste seems to have a significant impact on the properties of GC. In the presence of sulfur ions at both temperatures, GC exhibits complete resistance. When exposed to acids, GC experiences a mass loss of 60% in a sulfuric acid environment and 20% in acetic acid. GC with the maximum content of fly ash (750 kg/m3) appears to be the best choice considering the mechanical properties, durability, and environmental impacts. In conclusion, fly ashes can be utilized as a raw material for the production of structural materials, particularly geopolymer concrete and mortar.
Degree
thesis:*- Grantor dc:publisher
- National Technical University of Athens (NTUA)
- Year dc:date
- 2023
Author and committee
dc:creator, dc:contributor.*- Authors dc:creator
-
- Nikoloutsopoulos, Nikolaos
- Νικολουτσόπουλος, Νικόλαος
Subjects
dc:subject × 21- Γεωπολυμερές
- Σκυρόδεμα
- Ιπτάμενη τέφρα
- Μηχανικές ιδιότητες
- Φυσικές ιδιότητες
- Ανθεκτικότητα
- Geopolymer
- Concrete
- Fly ash
- Mechanical properties
- Physical properties
- Durability
- Επιστήμη Χημικού Μηχανικού
- Επιστήμες Μηχανικού και Τεχνολογία
- Χημική μηχανική
- Επιστήμη Πολιτικού Μηχανικού
- Κατασκευή και Οικοδομική τεχνολογία
- Chemical Engineering
- Engineering and Technology
- Civil Engineering
- Construction and Building technology
Rights
- Language dc:language
- gre
Identifiers
dc:identifier.*- Identifier
- 10.12681/eadd/54642