Abstract

dc:description

In an effort to reduce the environmental footprint of cement production, there is growing interest in the development and utilization of a wider range of treated clays as supplementary cementitious material (SCM), and alternative processing methods. The aim of this PhD thesis is to investigate the effects of mineral composition and thermal and mechanical processing methods on the use of treated Greek palygorskite clay (GPC) as pozzolanic SCM, in order to develop new treated clays as economic SCM with a variety of impurities, and to optimize thermal and mechanical treatment. The effect of different thermal and mechanical treatment methods on the structure of clay minerals from GPC, was analyzed using a combination of qualitative (XRD) and quantitative - Rietveld (RQXRD) X-ray diffraction analysis (XRD), thermogravimetric analysis (TG-DTG-DTA), Fourier Transform Infrared Spectroscopy (FTIR), Scanning Electron Microscopy (SEM), Energy Dispersion X-ray Spectroscopy (EDX) and laser diffraction. At this stage, the mineralogical composition, crystal chemistry, thermal behavior, grain size distribution, crystallinity, degree of dehydroxylation and amount of amorphous phases were determined qualitatively and quantitatively in relation to the crystal chemistry of the palygorskite and the calcination and grinding treatments. The octahedral structure of the palygorskite was found to influence the degree of dehydroxylation after calcination and grinding. Palygorskite with trioctahedral structure showed a higher degree of dehydroxylation after thermal and mechanical treatments. To achieve the highest palygorskite dehydroxylation degree, calcination at 700 - 750ºC, for 3 h and grinding for 45 min at 800 rpm, were suggested to be the optimum temperature and time, respectively. Both treatments presented similar degree of dehydroxylation: 80% and 83%, for the thermal and mechanical treatment, respectively. These percentages corresponded to 64 wt% and 67 wt% of amorphous phases, respectively, and were lower than metakaolin displaying a content of 88 wt%. The main advantages of mechanical over thermal treatment are: a) the relatively shorter time (e.g. t ≥ 15 min), required for the structure collapse of the clay minerals, such as GPC palygorskite and the activation of their pozzolanic reactivity than the required calcination time (t ≥ 30 min), b) unlike calcination, mechanical treatment resulted in the mechanochemical dehydroxylation of smectite, which showed a high temperature dehydroxylation mass loss (T = 726 - 884°C), c) no greenhouse gases were emitted during mechanical treatment of palygorskite clays. Dry grinding resulted in the reduction in particle size and the degradation of clay mineral crystal structure, whereas, following wet grinding, the crystallinity of clay minerals was retained and the population of finer particles with a diameter of 0,1 - 1 μm, increased. The Chapelle test was performed and pastes were prepared, consisted of 20 wt% replacement of the cement with the SCM, in order to investigate the influence of the addition of treated GPC on the pozzolanic reactivity, hydration and mineral composition of the pastes. At this stage, the consumption of calcium hydroxide (CH) by the treated GPC was determined by means of titration with HCl (Chapelle test), the quantities of the hydrate phases (H) and CH in the blended cement pastes at 7, 28 and 90 days, by means of TG - DTG analysis and the mineralogical and crystal chemistry composition of the hydrate phases in blended paste, using semi-quantitative XRD and SEM-EDX analyses. The results demonstrated that the calcined and dry ground clays showed higher pozzolanic reactivity than metakaolin at 7 days and lower at 28 and 90 days, the pozzolanic reactivity of the thermally treated GPC was comparable to metakaolin but displayed significantly lower amount of hydrate phases. Following wet grinding, the clay minerals retained crystallinity, resulting in negligible pozzolanic reactivity and clay mineral consumption in paste, thus hampering hydration reactions relative to calcined and dry ground clays. The filler effect, observed in pastes containing 20 wt% dry ground GPC substitute, enhanced the hydration in paste and resulted in similar hydrates content to metakaolin at 7 and 28 days, respectively. The pozzolanic reactivity of treated clays was influenced by treatment methodology and octahedral structure of palygorskite. The treatment methodologies for optimum CH consumption were calcination at 700 - 750ºC for 3 h and dry grinding for 30 - 45 min at 800 rpm. Calcination of GPC at 700 - 750ºC for 3 h, displayed higher pozzolanic reactivity than dry grinding at 800 rpm for 45 min, despite palygorskite exhibiting similar degree of dehydroxylation after both treatments. Following calcination at 700 - 750ºC, clays containing trioctahedral palygorskite, displayed a higher pozzolanic reactivity than dioctahedral, whereas dry grinding of GPC, for 30 - 45 min, showed higher pozzolanic reactivity when dioctahedral palygorskite was present, at 28 and 90 days. The optimum calcination temperature for maximum CH consumption differed between the GPC with dioctahedral and trioctahedral palygorskite: 700ºC and 750ºC, respectively. Both the treatment methods and the octahedral structure of the palygorskite influenced the type of cement paste hydration reactions. The addition of calcined GPC, resulted in pozzolanic and hydraulic reactivity, whereas dry ground clays additionally displayed the filler effect, following 20 wt% replacement of cement with treated GPC. Unlike calcined trioctahedral palygorskite, dioctahedral site occupancy produced hydraulic reactivity, following calcination at 700 - 750ºC. Furthermore, as a result of the mechanochemical dehydroxylation of smectite, resulting in the availability of Al, the dry ground GPC showed hydraulic reactivity, regardless of the octahedral structure of the palygorskite. Two distinct C – S – H types were identified: I) Mg – rich and II) Mg – poor. The main difference between the two types of C – S – H, was that the former ones demonstrated extensive isomorphous substitution of Mg for Ca and Al, Fe for Si cations derived from the dehydroxylated palygorskite, in contrast to the relatively negligible substitution observed the latter. A positive relationship between the octahedral structure of palygorskite and the crystal chemistry of C – S – H type I, was observed. Following both treatments, palygorskite trioctahedral site occupancy produced C – S – H with higher Mg/Ca ratio than the dioctahedral one. In contrast, palygorskite trioctahedral site occupancy produced C – S – H with higher Al/Ca ratio than the trioctahedral one. Furthermore, the addition of calcined GPC with trioctahedral palygorskite, resulted in lower Mg / Ca, Al / Ca, Si / Ca, Fe / Ca, Al+Fe/Ca, (Si+Al+Fe) / Ca and (Si+Al+Fe) / (Ca+Mg) and higher Ca / Si and (Ca+Mg) / (Si+Al+Fe) ratios, than the dry ground one.Mortars with 20 wt% calcined clay were prepared in order to study the effect of the addition of GPC on mortar properties. This stage included the determination of workability by means of ASTM C 1437-07, 2009 standard test method for flow of hydraulic cement mortar, compressive strength (MPa) by using ASTM C109M-02, 2007 standard test method for compressive strength of hydraulic cement mortars at 7, 28 and 90 days of hydration. The results illustrated that the mortars with calcined clays showed similar strengths relative to neat cement ones, at all ages, due to the pozzolanic and/or hydraulic reactivity of palygorskite clays. Mortars with calcined clay displayed lower 7 and 28 – day compressive strength than metakaolin mortars, despite presenting similar CH consumption in SCM – pastes, mainly due to poor workability of the former related to the high water demand. The octahedral structure of palygorskite influenced the compressive strength of the mortars. Calcination of clays with trioctahedral palygorskite between 600 and 750ºC, presented higher strengths compared to the dioctahedral ones, at 28 and 90 days. The reduced workability of mortars with calcined palygorskite clays, hampered the compressive strength development at all ages.

Degree

thesis:*
Grantor dc:publisher
National Technical University of Athens (NTUA)
Year dc:date
2025

Author and committee

dc:creator, dc:contributor.*
Authors dc:creator
  • Georgopoulos, Georgios
  • Γεωργόπουλος, Γεώργιος

Subjects

dc:subject × 22

Rights

Language dc:language
gre

Identifiers

dc:identifier.*
Identifier
10.12681/eadd/58540

Chain of custody

source
Harvested from
Greek National Archive of PhD Theses
Base URL
phdtheses.ekt.gr/eadd_oai/request
Last updated
2026-11-18
Source record
OAI-PMH GetRecord
citation

Georgopoulos, Georgios; Γεωργόπουλος, Γεώργιος. Διερεύνηση θερμικής και μηχανικής ενεργοποίησης παλυγκορσκιτικής αργίλου με εφαρμογές σε δομικά υλικά. National Technical University of Athens (NTUA), 2025. http://hdl.handle.net/10442/hedi/58540