National Technical University of Athens (NTUA)
Ενίσχυση ελαστομερών με προηγμένα νανοϋλικά άνθρακα
Abstract
dc:descriptionThe purpose of the present doctoral thesis was the design and development of a method for preparing elastomeric nanocomposites of advanced carbon-based nanomaterials with satisfactory dispersion, as well as the study of the effect of carbon nanoparticles on the vulcanization reaction, structure and critical functional properties of selected elastomers. The elastomers studied were polydimethylsiloxane (PDMS) with terminal hydroxyl groups (two molecular weights: LMW-26000 and HMW-49000 g/mol) and the terpolymer of ethylene-propylene-diene (EPDM, 55.5-40-4.5 % w/w), while the reinforcing agents used were graphene (GN), graphene oxide (GO; modified Hummer’s method), multiwalled carbon nanotubes (MWCNTs) as well as hybrid GN/MWCNTs systems. From the study of the PDMS vulcanization using Brookfield viscometry and modulated differential scanning calorimetry (ADSC), it was determined that MWCNTs and GN do not favorably affect the reaction. Conversely, GO, significantly accelerates the reaction, due to the reactive oxygen-containing groups on its surface which react with the elastomer. Regarding the preparation of PDMS nanocomposites, the following methods were used: i) the direct mixing technique and ii) the solution mixing technique (tetrahydrofuran, THF) with ultrasound application, which, particularly at low reinforcing agent concentrations, yields nanocomposites with satisfactory dispersion (determined by Scanning Electron Microscopy-SEM).From the application of RAMAN spectroscopy to GN/PDMS and GO/PDMS composites, an increase was observed in the defects in the graphitic structure of GN and GO (to a lesser extent), following their incorporation into the elastomer. This increase was reflected as an increase in the intensity ratio ID/IG (D: 1350 cm⁻¹, G: 1580 cm⁻¹) and was attributed to ultrasound processing during solution mixing. In MWCNTs/PDMS composites, the carbon nanotubes showed no noticeable change in their morphology, attributed to the pre-existing structural defects from their synthesis process.DSC analysis showed increased Tc values, indicating that at low concentrations, GN and GO act as heterogeneous nucleation agents and facilitate the crystallization of PDMS. The addition of MWCNTs did not significantly affect the thermal transitions of PDMS. However, it noticeably reduced the crystallinity of the elastomer in composites of lower concentrations, as therein the dispersion of the nanoparticles was more uniform.TGA characterization of the PDMS composites revealed that GO and GN significantly enhanced the thermal stability of their composites. Specifically, in composites of higher GN (2-5 phr) and GO (1 phr) concentrations, the thermal decomposition completion range shifted by more than 100°C and 110°C, respectively. The addition of MWCNTs did not bring significant improvement in the thermal stability of PDMS. For all examined concentrations (0.02-4 phr MWCNTs), Tonset decreased while Tendset increased. At higher concentrations (2 and 4 phr MWCNTs), Td5% and Tpeak also showed improvement. Tensile testing revealed that all composites exhibit increased tensile strength compared to pristine PDMS. MWCNTs/PDMS composites presented the greatest tensile strength enhancement (100% for 1 phr MWCNTs), a phenomenon linked to the morphology of the reinforcing agent. Among the sheet-like fillers, GO had the strongest effect on PDMS tensile strength (94% for 1 phr GO) compared to GN (36% for 1 phr GN), due to improved interfacial interaction with the matrix. GN/PDMS composites showed noticeable tensile strength improvement at higher filler concentrations (73% for 2 and 4 phr GN). High-concentration hybrid GN/MWCNTs composites showed the greatest tensile strength (0.70 MPa for 2 phr of GN/MWCNTs at 50-50 wt.% analogy), a result indicating strong synergistic action between the two agents. The composites’ modulus of elasticity was significantly increased in MWCNTs/PDMS (99% for 4 phr MWCNTs) and GN-MWCNTs/PDMS composites. The study of oxygen (O₂) permeability in membranes from PDMS nanocomposites is of particular interest for various applications and constitutes an element of originality of this thesis. The membranes of the examined nanocomposites presented reduced permeability compared to the pristine matrix. Composites reinforced with sheet-like nanofillers (GN and GO) presented the greatest permeability reduction (61% for 0.5 phr GN and 44% for 0.5 phr GO). In composite membranes of higher filler content, the addition of MWCNTs was more effective in reducing the permeability (52% at 2 phr MWCNTs). The greatest reduction was recorded by the hybrid PDMS membranes (86% for 1 phr of GN-MWCNTs in 30-70 wt.% analogy), a result possibly linked to the improvement of nanofiller dispersion in the matrix and the combination of their geometry, which causes an increase in the tortuosity of the gas diffusion path. Dielectric relaxation spectroscopy (DRS) revealed that the addition of sheet-like reinforcements (GN and GO) does not allow the formation of conductive networks and thus their composites behave as insulators. MWCNTs/PDMS composites presented conductive behavior with a significantly low percolation threshold (0.036 phr MWCNTs), compared to corresponding literature data. Further increase in their concentration led to an exponential increase in conductivity, up to the saturation point. The hybrid GN-MWCNTs/PDMS composites (1 phr) exhibited particularly enhanced conductivity compared to the corresponding composite reinforced exclusively with MWCNTs. This behavior can be attributed to their uniform dispersion, which allows the formation of a conductive carbon network, enhancing electron transport within the elastomer. The rapid development and use of electronic and telecommunications equipment have made electromagnetic interference (EMI) a significant challenge, making the design and development of suitable protective materials critical. In this thesis, EMI shielding was studied in the X-band frequency range (X-band: 8.2-12.4 GHz). It was determined that the addition of GN didn’t affect the shielding ability of PDMS positively. On the other hand, the addition of MWCNTs at higher concentrations resulted in the significant reduction of the transmission coefficient, leading to shielding values of 17-18 dB (composites with 4 phr MWCNTs), close to the values required for commercial applications. The study of PDMS composites was completed with the characterization of the surface wettability of the composites using deionized water droplets. The addition of GN and MWCNTs did not alter the hydrophobic character of the elastomer. On the contrary, GO/PDMS composites presented enhanced water repellency, possibly due to the morphology imparted to the surface by the GO nanoplatelets. The study continued with EPDM, an elastomer with advanced technological applications and industrial interest. For the preparation of EPDM nanocomposites, two techniques were followed: i) direct mixing in a Banbury-type internal mixer (one-stage method) and ii) preparation of a high-concentration masterbatch mixture and subsequently dilution thereof to the desired concentration in a Banbury-type internal mixer (masterbatch technique, two-stage method). The optimization of the system for bulk vulcanization of EPDM using peroxide was carried out through: i) isothermal DSC experiments and using the autocatalytic model (Šesták-Berggren equation) for kinetic analysis and ii) dynamic DSC experiments and using the Kissinger and Ozawa models. The optimal ratios determined were: 5 phr dicumyl peroxide (DCP) and 4 phr co-agent (TAC). Subsequently, the effect of carbon nanoparticles on the vulcanization reaction was examined. Incorporation of MWCNTs increased the activation energy (Ea) of the reaction, particularly in composites of higher concentration, while the addition of sheet-like nanofillers (GN and GO) resulted in reduced values.XRD spectra of GO/EPDM and MWCNTs/EPDM did not present peaks associated with carbon nanoparticles, suggesting their successful dispersion. Conversely, the detection of these peaks in GN/EPDM composites indicates the presence of nanoparticle aggregates.EPDM composites reinforced with GN and MWCNTs showed improved thermal stability (TGA). This phenomenon was attributed to their inherent thermal stability and the hindrance of decomposition product removal due to the formation of surface char layers. Conversely, GO/EPDM composites exhibited reduced thermal resistance, a behavior attributed to the sensitivity of GO due to strain during its synthesis, as well as during the composite preparation stage. Tensile testing of GN/EPDM composites showed improvement in their tensile strength with increasing reinforcing agent content (198% for 10 phr GN). Additionally, an increase was recorded in the modulus of elasticity in all composites (71% for 10 phr GN), particularly those prepared using the masterbatch technique. The addition of GO did not demonstrate a clear positive trend in EPDM composite behavior under this test. MWCNTs/EPDM composites showed strength enhancement at higher concentrations (88% for 10 phr MWCNTs) and modulus of elasticity increase proportional to MWCNTs concentration (218% for 10 phr MWCNTs). DRS testing revealed that GN/EPDM composites did not demonstrate conductive behavior. On the contrary, the addition of MWCNTs allowed the formation of a conductive graphitic network within EPDM, with a conductivity threshold at 2-3 phr. Further increase in MWCNTs concentration led to an even denser electron transport network, dramatically increasing the conductivity of the composites. The EMI shielding effectiveness of GN/EPDM improved marginally compared to pristine EPDM. In contrast, higher-concentration MWCNTs/EPDM composites exhibited significant EM shielding improvement, reaching 17-19 dB (10 phr MWCNTs). The high electrical conductivity of MWCNTs/EPDM composites favors the reflection mechanism, which prevents EM radiation penetration and acts antagonistically to the absorption mechanism. Thermal conductivity measurements (Light Flash Analysis, LFA) showed a marginal increase in EPDM composites reinforced with GN and MWCNTs, a fact linked to the nature of the matrix and the examined reinforcing agent concentrations. In summary, the reduced O₂ permeability and improved shielding capability against EM radiation render MWCNTs/PDMS nanocomposites ideal for protective coatings and particularly for equipment exposed to EM radiation. Additionally, the controlled and high electrical conductivity, as well as the significantly enhanced mechanical properties, enable their exploitation in the manufacturing of flexible sensors, which, considering the good biocompatibility of PDMS, can be applied in biomedical applications. GN/PDMS composites exhibited the most significant improvement in thermal stability and, combined with improved mechanical properties and reduced O₂ permeability, render these materials also suitable for flexible protective coatings.Regarding EPDM composites, among the examined carbon nanoparticles, MWCNTs presented the optimal combination of property enhancement (thermal, mechanical, dielectric, shielding against EM radiation), rendering MWCNTs/EPDM composites suitable for high-demand industrial applications such as EMI shielding coatings on cables, electronic systems, energy storage systems, and thermal insulation materials for engines in aeronautics. The originality of the present thesis lies in the following:Comparative study of the effect of carbon nanoparticles (GN, GO, MWCNTs, hybrid GN/MWCNTs) on PDMS vulcanization via condensation mechanism, using combined rheological and calorimetric measurementsComparative evaluation of PDMS nanocomposites with advanced carbon nanomaterials with respect to critical functional properties (O₂ permeability, electrical conductivity, shielding against EM radiation) and correlation with their structure and characteristicsIdentification of the percolation threshold (via DRS) at very low MWCNTs concentration (0.036 phr) and proposal of conductive network formation mechanism for PDMS compositesDevelopment of a flexible laboratory method for preparing EPDM nanocomposites (masterbatch technique) with effective nanoparticles’ dispersion, offering marked scalability potentialStudy of the effect of carbon nanoparticles (GN, GO, MWCNTs) on bulk peroxide vulcanization reaction of EPDM, via isothermal/dynamic DSC experiments, and its exploitation in optimizing the preparation method of these elastomer nanocompositesComparative evaluation of EPDM nanocomposites with respect to critical functional properties (electrical conductivity, EM radiation shielding, thermal conductivity) and correlation with their structure and characteristics.
Degree
thesis:*- Grantor dc:publisher
- National Technical University of Athens (NTUA)
- Year dc:date
- 2026
Author and committee
dc:creator, dc:contributor.*- Authors dc:creator
-
- Ketikis, Panagiotis
- Κετίκης, Παναγιώτης
Subjects
dc:subject × 15Rights
- Language dc:language
- gre
Identifiers
dc:identifier.*- Identifier
- 10.12681/eadd/62785