Abstract

dc:description.abstract

<p>Materials for high-temperature turbine environments face rigorous operating conditions. Not only are components exposed to high-temperature oxidation, but corrosive gasses that evolve during combustion can also lead to degradation. Ni-based superalloys are used in turbines for their strength and creep resistance at high temperature. The compositions of these superalloys are such that they do not provide adequate environmental protection alone; therefore coatings are used to protect the underlying materials from degradation. Currently, there is no coating that provides adequate protection to both oxidation and hot corrosion. In high temperature areas where the main degradation mode is oxidation, β-NiAl-type diffusion coatings are often used. These coatings have a significant Al content to insure Al<sub>2</sub>O<sub>3</sub>-scale formation, which provides excellent oxidation protection but variable corrosion resistance that is highly dependent on composition. Conversely, MCrAlY overlay coatings (M=Ni, Co, or NiCo) provide superior corrosion resistance due to their relatively high Cr content (up to about 30at%), but cannot be used in applications exceeding 1000°C due to the limited oxidation protection. A new generation of Al<sub>2</sub>O<sub>3</sub>-scale-forming coating, based on Hf+Pt-modified γ-Ni + γ'-Ni<sub>3</sub>Al, can show excellent oxidation protection and increased corrosion protection compared to β-type coatings. This research modifies the Hf+Pt-modified γ-Ni + γ'-Ni<sub>3</sub>Al coating composition with Cr and Si to increase the hot corrosion protection provided, while maintaining superior oxidation resistance, with the best-performing γ-Ni + γ'-Ni<sub>3</sub>Al composition being, Ni-18Al-10Cr-3Pt-2Si-0.1Hf alloy (at%). Tests were conducted on both bulk-alloys and coatings. Thermal spraying was used to generate the coatings for testing. A Pt-modification procedure was devised for the thermal spray coatings. Oxidation testing and accelerated hot corrosion testing were used to assess performance. Metallography, SEM and EDS techniques were used to characterize samples and rank performance. As will be shown, the Ni-18Al-10Cr-3Pt-2Si-0.1Hf composition provided the best combined oxidation and hot corrosion protection when compared to Ni-50Al-15Pt (Pt-modified β), Ni-20Al-20Pt-1wt%Hf (γ-Ni + γ'-Ni3Al), Ni-21.7Cr-19.5Al-0.5Y (β+γ MCrAlY), and Ni-17.6Cr-12Al-0.3Y (γ+γ' MCrAlY), with all compositions listed in at%.</p>

Degree

thesis:*
Name thesis:degree_name
Master of Science
Level thesis:degree_level
thesis
Department dc:contributor.department
Department of Materials Science and Engineering
Year dc:date.issued
2010

Author and committee

dc:creator, dc:contributor.*
Author dc:creator
  • Guyer Ii, Douglas
Advisor dc:contributor.advisor
  • Brian M. Gleeson

Rights

Language dc:language.iso
en

Identifiers

dc:identifier.*
Identifier
archive/lib.dr.iastate.edu/etd/11165/
Dc Identifier Other
2194
2807392
Mods Identifier Filename
archive/lib.dr.iastate.edu/etd/11165/GuyerII_iastate_0097M_10963.pdf|||Fri Jan 14 18:43:53 UTC 2022

Chain of custody

source
Harvested from
Iowa State University
Base URL
dr.lib.iastate.edu/server/oai/request
Last updated
2026-11-18
Source record
OAI-PMH GetRecord
related terms
citation

Guyer Ii, Douglas. Oxidation and hot corrosion of Pt- and Si-modified Ni-18Al-10Cr-0.1Hf and comparison compositions. thesis thesis, 2010. https://doi.org/10.31274/etd-180810-300