Back to search

Iowa State University

Study of O/Ni(100) with LEED and AES: from chemisorption to oxidation

Abstract

dc:description.abstract

<p>The structures formed on the Ni(100) surface during oxygen adsorption, leading to oxidation, are studied with Video-LEED (low-energy electron diffraction) and AES (Auger electron spectroscopy). The temperature- and exposure-dependence in the development of LEED patterns observed during oxidation on Ni(100), at oxidation temperatures of 80 to 400 K, are investigated extensively. Integrated diffraction spot intensities and fractional spot profiles are measured quantitatively and continuously, allowing unambiguous correlation of various surface processes. A LEED pattern with 7th order spots around the substrate integral spots, (7 x 7), is observed. Possible models to explain this observation are discussed. AES is used to measure the oxidation onset during adsorption and the final relative thickness of the oxide. It also helps to characterize the structural differences between NiO(111), (7 x 7) and NiO(100). We find a strong temperature-dependence in the development of LEED patterns associated with NiO. The formation of NiO(111) is favored by adsorption temperatures below 300 K, whereas a (7 x 7)-like structure is favored by adsorption temperatures of 300 to 400 K. Room temperature is a "crossover" point between these two forms of the oxide. The final depth of the oxide is independent of adsorption temperature and, therefore, of epitaxial orientation, between 80 and 400 K. Also, the exposure at which oxidation begins as measured by AES, correlates well with the onset of the NiO(111) pattern or the (7 x 7)-like pattern, whichever is favored at a given adsorption temperature. NiO(100) is formed when the oxygen-covered surface, showing either a NiO(111) or (7 x 7) pattern, is heated above 550-600 K. A possible mechanism to explain the formation sequence of different oxide structures is proposed throughout this dissertation. In addition, the Debye-Waller factor and, therefore, Debye temperatures of surface and bulk NiO are estimated experimentally. The linearity of the Debye-Waller effect is found to hold at temperatures as low as 1/2 the surface Debye temperature. The pressure effect, postulated by others, on the epitaxy of oxide growth and the depth of oxide layer is also checked in this work. As oxygen pressure varies from 10[superscript]-7 to 10[superscript]-9 Torr, only the intensity of the grown oxide superstructure is affected, not the nature of the superstructure itself nor the exposure-dependent progression of superstructures.</p>

Degree

thesis:*
Name thesis:degree_name
Doctor of Philosophy
Level thesis:degree_level
dissertation
Department dc:contributor.department
Department of Chemistry
Year dc:date.issued
1990

Author and committee

dc:creator, dc:contributor.*
Author dc:creator
  • Wang, Wen-Di
Advisor dc:contributor.advisor
  • Patricia A. Thiel

Rights

Language dc:language.iso
en

Identifiers

dc:identifier.*
Identifier
archive/lib.dr.iastate.edu/rtd/9908/
Dc Identifier Other
10907
6371613
Mods Identifier Filename
archive/lib.dr.iastate.edu/rtd/9908/r_9110581.pdf|||Sat Jan 15 02:39:28 UTC 2022

Chain of custody

source
Harvested from
Iowa State University
Base URL
dr.lib.iastate.edu/server/oai/request
Last updated
2026-11-18
Source record
OAI-PMH GetRecord
related terms
citation

Wang, Wen-Di. Study of O/Ni(100) with LEED and AES: from chemisorption to oxidation. dissertation thesis, 1990. https://dr.lib.iastate.edu/handle/20.500.12876/83058