Back to search

University of Manitoba

Strength of early-age concrete masonry prism short-term exposed to freezing temperatures

Abstract

dc:description.abstract

Concrete masonry is extensively utilized in Canada due to its superior compressive strength, aesthetic versatility, cost-effectiveness, ease of construction, and proven durability. However, akin to other construction materials, concrete masonry exhibits high sensitivity to temperature variations during construction, curing, and mature stages. The majority of extant research has concentrated on the influence of temperature on mature masonry structures (beyond 28-day curing), investigating the mechanical behavior of fully cured assemblies under freezing conditions. This focus has resulted in a notable knowledge gap concerning the effects of freezing temperatures on early-age masonry. Prevailing masonry construction guidelines advocate maintaining temperatures above 4.44°C to mitigate mortar freezing and grout expansion, often necessitating thermal insulation or protective measures during low-temperature construction. Nonetheless, these guidelines overlook two pivotal uncontrollable factors during the construction phase: unpredictable weather exposure and potential failures in structural protection against freezing temperatures. The mechanical performance of early-age masonry subjected to unintentional or accidental short-term exposure to freezing temperatures remains inadequately explored, leaving uncertainty regarding its impact on structural capacity. To address these deficiencies, 324 specimens were tested under diverse temperature regimes and exposure durations to assess their compressive and tensile strengths. The experimental outcomes delineate a multifaceted pattern: freezing temperatures can augment strength development in ungrouted and grouted compression specimens, as well as grouted tension specimens. Specifically, ungrouted compression specimens exposed to -6°C surpassed the CSA compressive strength design requirement by an average of 46.98\% and exceeded the control group strength by 28.66\%. Grouted compression specimens at -6°C exhibited 9.88\% higher strength than the CSA standard and 12.64\% higher than the control group. Ungrouted compression specimens at -12°C exceeded the CSA standard by 39.38\% and were 23.49\% stronger than the control group, while grouted counterparts were 1.94\% above the standard and 4.19\% above the control. At -24°C, ungrouted compression specimens were 17.99\% higher than the CSA requirement and 3.32\% higher than the control, whereas grouted specimens at this temperature demonstrated adverse effects, yielding compressive strengths 4.91\% and 3.16\% lower than the CSA standard and control group, respectively. Furthermore, freezing temperatures exerted pronounced detrimental effects on ungrouted tension specimens across all temperature levels, resulting in an average tensile strength reduction of 86\% relative to the CSA design requirement. In comparison to the control group, however, -6°C ungrouted tension specimens exhibited 1.82\% higher tensile strength, -12°C specimens were 5.32\% higher, and -24°C specimens were 5.67\% higher. For grouted tension specimens, those at -6°C were 41.03\% above the CSA tensile strength requirement but 25.59\% below the control group. The -12°C grouted tension group demonstrated 95.95\% higher strength than the CSA standard yet remained 7.18\% below the control. Notably, -24°C grouted tension specimens performed optimally, achieving 141.48\% higher tensile strength than the CSA requirement and 19.42\% higher than the control. These findings quantitatively elucidate the ramifications of freezing temperatures on nascent masonry assemblies, offering valuable insights for enhancing quality control in masonry construction under adverse conditions. Moreover, solely mitigating cold temperatures should not constitute the exclusive strategy, as the beneficial effects of freezing have been substantiated in this and prior investigations. Instead, greater integration of cold-weather considerations during design and construction processes should be pursued to optimize masonry quality and reliability.

Degree

thesis:*
Level thesis:degree_level
Master of Science (M.Sc.)
Discipline thesis:degree_discipline
Civil Engineering
Year dc:date.issued
2025

Author and committee

dc:creator, dc:contributor.*
Author dc:creator
  • Zhong, Rui
Advisor dc:contributor.supervisor
  • Fiorillo, Graziano
Committee members dc:contributor.committeemember
  • Svecova, Dagmar (Civil Engineering)
  • EI-Salakawy, Ehab (Civil Engineering)
ORCID person:identifier.orcid

Subjects

dc:subject × 4

Rights

Language dc:language.iso
eng

Identifiers

dc:identifier.*
Handle dc:identifier.uri
http://hdl.handle.net/1993/39237

Chain of custody

source
Harvested from
University of Manitoba
Base URL
mspace.lib.umanitoba.ca/oai/request
Last updated
2026-11-19
Source record
OAI-PMH GetRecord
citation

Zhong, Rui. Strength of early-age concrete masonry prism short-term exposed to freezing temperatures. Master of Science (M.Sc.) thesis, 2025. http://hdl.handle.net/1993/39237