University of Manitoba
Evaluation Of zirconia-infused nano hybrid resin, composite resin, milled and autopolymerizing PMMA materials for fixed restorations: an in vitro study
Abstract
dc:description.abstractPurpose: This in vitro study evaluated and compared the mechanical properties of six provisional restorative materials fabricated using conventional, subtractive, and additive manufacturing techniques. The materials included autopolymerized acrylic resin, bis-acryl composite resin, CAD/CAM-milled polymethyl methacrylate (PMMA), and three 3D-printed resin-based materials (Rodin, Detax, and Vitality). The objective was to determine whether digitally fabricated provisional materials provide mechanical advantages over conventional materials. Materials and Methods: Square specimens were fabricated for nanoindentation and surface roughness testing, bar-shaped specimens for flexural strength testing, and standardized mandibular molar provisional crowns for fracture resistance testing. Hardness and elastic modulus were measured by nanoindentation, surface roughness by contact profilometry, flexural strength by a three-point bending test, and fracture resistance using 2-mm and 4-mm loading configurations. Data were analyzed using one-way and two-way ANOVA with appropriate post hoc tests. Results: Significant differences were found among the materials for all tested properties (p < 0.05). Rodin demonstrated the highest hardness and elastic modulus. Acrylic exhibited the greatest surface roughness, whereas Detax had the smoothest surface, followed by PMMA and Vitality. Acrylic also showed the lowest flexural strength, while PMMA, Rodin, Detax, and Vitality demonstrated similarly high flexural strength. Fracture resistance was significantly influenced by material, loading configuration, and their interaction. Bis-Acryl and PMMA demonstrated the highest fracture resistance under both loading conditions. PMMA, Rodin, and Acrylic exhibited significantly greater fracture resistance under 4-mm loading than under 2-mm loading. The overall fracture-resistance ranking was Bis-Acryl > PMMA > Acrylic ≈ Detax > Rodin > Vitality. Higher fracture resistance was generally associated with greater displacement before failure. Conclusion: Within the limitations of this in vitro study, provisional restorative materials demonstrated significant differences in nanomechanical properties, surface roughness, flexural strength, and fracture resistance. CAD/CAM-milled PMMA and selected 3D-printed materials showed mechanical advantages over conventional acrylic resin, although the performance of 3D-printed materials was material specific. Material selection should be based on clinical requirements, service duration, occlusal loading, restoration design, fabrication workflow, and finishing protocol rather than manufacturing technique alone.
Degree
thesis:*- Level thesis:degree_level
- Master of Dentistry (M.Dent.)
- Discipline thesis:degree_discipline
- Restorative Dentistry (Prosthodontics)
- Year dc:date.issued
- 2026
Author and committee
dc:creator, dc:contributor.*- Author dc:creator
-
- REESU, GOWRI VIJAY
- Advisor dc:contributor.supervisor
-
- Pesun, Igor
- Committee members dc:contributor.committeemember
-
- França, Rodrigo (Restorative Dentistry)
- Nowakowski, Anthony (Restorative Dentistry)
- ORCID person:identifier.orcid
Subjects
dc:subject × 6Rights
- Language dc:language.iso
- eng
Identifiers
dc:identifier.*- Handle dc:identifier.uri
- https://hdl.handle.net/1993/39854