Effect of Intermetallic Growth on Durability of High Temperature Solders (SnAg, SAC305, SAC+Mn, SnAg+Cu Nano) in Thermal and Vibration Environments
Abstract
dc:description.abstractThe RoHS ban of lead from electronics has pushed the industry to find lead free alternatives. In high temperature environments, high lead solders have typically been used. A suitable lead free replacement alloy is required. In this study quad flat packages (QFP) and 2512 chip resistors soldered with commercially available Sn3.5Ag and SAC305, and experimental SAC+Mn and SnAg+Cu Nano alloys on ENIG finished copper were subjected to three tests. Isothermal aging at 185°C for up to 1000 hours and at 200°C for up to 500 hours were performed to measure the interfacial intermetallic thickness, assess intermetallic compounds, and view the microstructure. A durability assessment was performed featuring thermal cycling ranges of -40 to 185°C and -40 to 200°C intermixed with 50G vibration cycling to determine the most durable solder alloy. Failure analysis was performed to understand the durability results. Finally, shear testing was performed to determine a correlation between shear strength and durability. The results show SAC305 is the most reliable solder under these conditions.
Degree
thesis:*- Department dc:contributor.department
- Mechanical Engineering
- Grantor dc:publisher
- Digital Repository at the University of Maryland
- Year dc:date.issued
- 2011
Author and committee
dc:creator, dc:contributor.*- Author dc:creator
-
- Crandall, Michael Adam
- Advisor dc:contributor.advisor
-
- McCluskey, Patrick
Identifiers
dc:identifier.*- Handle dc:identifier.uri
- http://hdl.handle.net/1903/12208