Crystallization kinetics and polyblends of poly(ethylene terephthalate) recycled from post-consumer beverage bottles

Abstract

dc:description.abstract

In order to reduce waste generation, and comply with state and federal laws, plastic beverage bottles are usually undergoing recycling. Poly(ethylene terephthalate) [PET], which is the main component the bottles are made of, cannot be used for manufacturing new food containers, and has to be used for manufacturing other end consumer products. The recycled PET is a cheap material, but its use is problematic due to the low crystallization rates of PET. The present study investigates ways of accelerating PET crystallization by using inorganic carbonate salts as nucleating agents. This study also explores the possibility of forming polymer blends based on recycled PET. Crystallization kinetics of recycled PET were studied in the presence of Na_2CO_3, NaHCO_3, K_2CO_3, Li_2CO_3, MgCO_3, CaCO_3, SrCO_3, BaCO_3, ZnCO_3, CdCO_3, and PbCO_3 as nucleating agents. Based on results from Differential Scanning Calorimetry, Optical Microscopy, and thermal stability studies, it has been concluded that among the additives tried, Na_2CO_3 and NaHCO_3 are the most effective nucleating agents for recycled PET crystallization. From the results obtained during this study, and from published data on virgin PET crystallization, it has been concluded that the effectiveness of an additive as a nucleating agent for PET can be predicted based on the following general criteria: the additive must have a good solubility in both water and alcohol and the resulting solution must be basic; the additive should be easily dispersed in the molten PET. Processability of recycled PET in injection molding has been also investigated in the present study. It has been found that temperatures below 100 C can be effectively used with low cycle times. More specifically, it has been found that a mold temperature of 40 C can be used to produce amorphous specimens while at 90 C, and in the presence of either Na_2CO_3 or NaHCO_3, crystalline products with good properties can be formed. Recycled PET has been also used for producing blends with polyester elastomers and low density polyethylene (LDPE). With polyester elastomers the blends resulted in products having a high degree of crystallinity, a good appearance, but relatively poor mechanical properties. With LDPE, blends of very good properties were produced but only in the presence of various ionomers which acted as compatibilizers.

Degree

thesis:*
Name thesis:degree_name
Doctor of Philosophy in Chemical Engineering - (Ph.D.)
Discipline thesis:degree_discipline
Chemical Engineering, Chemistry and Environmental Science

Author and committee

dc:creator, dc:contributor.*
Author dc:creator
  • Hsu, Peming Peter
Contributors dc:contributor
  • Basil Baltzis
  • David S. Kristol
  • George Y. Lei

Subjects

dc:subject × 7

Identifiers

dc:identifier.*
Repository record dc:identifier
https://digitalcommons.njit.edu/dissertations/1140

Chain of custody

source
Harvested from
NJIT
Base URL
digitalcommons.njit.edu/do/oai/
Last updated
2026-11-19
Source record
OAI-PMH GetRecord
citation

Hsu, Peming Peter. Crystallization kinetics and polyblends of poly(ethylene terephthalate) recycled from post-consumer beverage bottles. https://digitalcommons.njit.edu/dissertations/1140