Abstract
dc:description.abstractWet Thermal Oxidation of Silicon in VLSI is an extremely important step in the formation of field oxides. Understanding oxidation kinetics is critical for process reproducibility. The present study aims at gaining an insight into the oxidation kinetics through large experimental data at process temperatures of 800 C, 900 C, 1000 C and 1100 C with a bubbler temperature of 98 C. Oxides with thicknesses ranging from 100A to 7000A have been grown. Rate constants are obtained for the growth kinetics. Extensive characterization studies have been performed on MOS structures produced after wet oxidation. In addition, porous silicon which assumes a growing significance in the field of SOI technology has been produced using chemical method. SOI technology with porous silicon as an insulator marks a new concept with growing interest in porous silicon as a replacement to GaAs technology in optoelectronic devices. Characterization studies have also been performed for porous silicon structures.
Degree
thesis:*- Name thesis:degree_name
- Master of Science in Electrical Engineering - (M.S.)
- Discipline thesis:degree_discipline
- Electrical and Computer Engineering
Author and committee
dc:creator, dc:contributor.*- Author dc:creator
-
- Gharia, Nilesh A.
- Contributors dc:contributor
-
- N. M. Ravindra
- Kenneth Sohn
- Durgamadhab Misra
Subjects
dc:subject × 4Identifiers
dc:identifier.*- Repository record dc:identifier
- https://digitalcommons.njit.edu/theses/1758