Massachusetts Institute of Technology
Repair of partially penetrated weld joints in cooper-nickel seawater piping on Naval Ships
Abstract
dc:description.abstractThe U.S. Navy has experienced several leaks in Cu-Ni seawater piping as a result of partially penetrated welds in the ships' original construction. If it were possible to repair the welds without cutting open the pipe, the Navy could realize significant cost savings on ship repair. This investigation evaluated whether it would be possible to achieve satisfactory weld repairs by remelting the weld zone, fusing the joint through its full thickness without cleaning the interior of the pipe. Elemental analysis of the internal deposits on pipes removed from service and manufacture of repair welds on these pipes show that it is possible to repair partially penetrated welded joints in Cu-Ni seawater pipe by remelting the weld zone. The repair weld is not likely to absorb contamination from the interior of the pipe, as shown by X-rays of the welds and elemental analysis of the weld bead, compared to the unwelded base metal.
Degree
thesis:*- Name thesis:degree_name
- Master of Science in Naval Architecture and Marine Engineering
- Level thesis:degree_level
- Masters
- Discipline thesis:degree_discipline
- Naval Architecture and Marine Engineering
- Grantor dc:publisher
- Massachusetts Institute of Technology
- Year dc:date.issued
- 2000
Author and committee
dc:creator, dc:contributor.*- Author dc:creator
-
- Rechel, Alan A.
- Advisor dc:contributor.advisor
-
- Burke, David V.
Rights
dc:rights- Statement dc:rights
-
- This publication is a work of the U.S. Government as defined in Title 17, United States Code, Section 101. Copyright protection is not available for this work in the United States.
Identifiers
dc:identifier.*- OCLC
- o640952677