Abstract
dc:description<p>Tung oil was used as a diene for modification with acrylate dienophiles via a Diels-Alder reaction. In this thesis, the research was divided into two related parts. In the first part, UV-curable resins were prepared from tung oil and tung oil alkyd for a high solids coating application. In the second part, tung oil alkyd was modified with three different acrylate monomers, possessing either alkoxysilane, triallyl ether, or fluorinated groups. The structures of the modified tung oil and alkyds were characterized by <sup>1</sup>H NMR, <sup>13</sup>C NMR, MALDI-TOF mass spectroscopy, and gel permeation chromatography(GPC).</p><p>Two UV-curable tung oil-based resins in the first part were synthesized via theDiels-Alder cycloaddition. A UV-curable Tung Oil (UVTO) was prepared from bodiedtung oil and trimethylolpropane trimethacrylate (TMPTMA) by a two-step reaction.Bodied tung oil was primarily prepared by treatment at high temperature, and thenreacted with TMPTMA on the α-eleosterate of tung oil triglyceride via the Diels-Alderreaction. An inhibitor, phenothiazine, was added to avoid homopolymerziaton ofTMPTMA. UV-curable Tung Oil Alkyd (UVTA) was prepared by the monoglycerideprocess, and then reacted with TMPTMA via the Diels-Alder reaction. The UVTO andUVTA were formulated with a free radical reactive diluent, tripropylene glycol diacrylate(TPGDA) and photoinitiator Irgacure 2100. Photo Differential Scanning Calorimeter (Photo-DSC) was used to investigate the curing kinetics of the UVTO and the UVTA.The data showed that the UVTA formula was cured faster than to the UVTO formula.</p><p>In the second part, the α-eleosterate pendent fatty acid of tung oil alkyd wasfunctionalized via a Diels-Alder reaction with three different acrylate groups, 2,2,2-trifluoroethyl methacrylate, 3-methacryloxypropyl trimethoxysilane, and triallyl etheracrylate. Drying time and viscoelastic properties of the alkyd-modified film wereinvestigated. Dynamic Mechanical Thermal Analysis (DMTA) was employed to evaluatethe viscoelastic properties of the alkyd-modified films. The viscoelastic and drying timeresult shows that the alkyd modified with siloxane and triallyl group shows a fasterdrying time, higher crosslink density, and higher glass transition temperature compared tothe unmodified alkyd, whereas the fluorinated alkyd showed surface active properties,but lacks in drying and crosslink density.</p>
Degree
thesis:*- Name thesis:degree_name
- Master of Science
- Level thesis:degree_level
- masters
- Discipline thesis:degree_discipline
- Chemistry
- Grantor dc:publisher
- University of Akron
- Year dc:date
- 2008
Author and committee
dc:creator, dc:contributor.*- Author dc:creator
-
- Thanamongkollit, Narin
- Advisor dc:contributor.advisor
-
- Soucek, Mark D.
Subjects
dc:subject × 5Rights
dc:rights- Statement dc:rights
-
- unrestricted
- This thesis or dissertation is protected by copyright: all rights reserved. It may not be copied or redistributed beyond the terms of applicable copyright laws.
- Language dc:language
- English
Identifiers
dc:identifier.*- Repository record dc:identifier
- http://rave.ohiolink.edu/etdc/view?acc_num=akron1218080747