<p>Tissue engineering scaffolds (or matrices) with a controllable degradation profile were fabricated from multiple blends of two L-tyrosine polyurethanes (denoted as PCL<sub>1250</sub>-HDI-DTH and PEG<sub>1000</sub>-HDI-DTH ) by means of the electrospinning process. By adjusting the ratios (2:1, 1:1, 1:2, and pure solutions) of the two polymers in the blends, relative control over the scaffolds' degradation properties was achieved without detriment to other scaffold properties. The ability to control the degradation rate allows for scaffold residence time to be design variable when fabricating a medical device intended on mimicking the body. The matrices produced were characterized chemically, morphologically, and mechanically and then subjected to hydrolytic degradation. </p><p>As theorized, the scaffolds degraded in a predictable and controllable manner. The scaffolds containing the higher proportion of the more resilient PCL<sub>1250</sub>-HDI-DTH polymer degraded more slowly and to a lesser extent (by mass) than those principally composed of the more hydrophilic PEG<sub>1000</sub>-HDI-DTH polymer. Specifically, after 60 days of exposure, mass losses (from highest to lowest concentration of PEG<sub>1000</sub>-HDI-DTH) were approximately 35%, 26%, 21%, 16%, and 9%. Note that decreasing concentration of PEG<sub>1000</sub>-HDI-DTH correlates to increased resistance to hydrolytic degradation. The mass lost per electrospun scaffold was between 76% and 108% greater than the identical blend in thin film configuration, demonstrating the enhanced degradation characteristics of the structure. Specifically, after 35 days of exposure, mass losses from the electrospun membranes were (from highest to lowest concentration of PEG<sub>1000</sub>-HDI-DTH) approximately 76%, 85%, 108%, 103%, and 98% greater than those of each blend’s thin film counterpart.</p><p>Morphologically, despite differing polymeric compositions, the scaffolds were fabricated under almost identical conditions and produced similar, acceptable fiber diameters, distributions, and pore sizes with minor variation across the blends. Specifically, the average fiber diameters in order of highest to lowest concentration of PEG<sub>1000</sub>-HDI-DTH were approximately 4.9 µm, 10.4 µm, 8.2 µm, 9.7 µm, and 9.8µm. The morphological and mechanical properties, pore sizes between 5 and 10 µm and Young’s moduli localized around ~12 MPa, combined with a controllable degradation profile, would suggest that the scaffolds produced would serve as a suitable mimic for soft tissue engineering.</p>

Degree

thesis:*
Name thesis:degree_name
Master of Science
Level thesis:degree_level
masters
Discipline thesis:degree_discipline
Chemical Engineering
Grantor dc:publisher
University of Akron
Year dc:date
2011

Author and committee

dc:creator, dc:contributor.*
Author dc:creator
  • Spagnuolo, Michael
Advisor dc:contributor.advisor
  • Liu, Lingyun

Subjects

dc:subject × 15

Rights

dc:rights
Statement dc:rights
  • unrestricted
  • This thesis or dissertation is protected by copyright: all rights reserved. It may not be copied or redistributed beyond the terms of applicable copyright laws.
Language dc:language
English

Identifiers

dc:identifier.*

Chain of custody

source
Harvested from
OhioLINK
Base URL
etd.ohiolink.edu/acprod/odb_etd/ws/oai/oai
Last updated
2026-11-27
Source record
OAI-PMH GetRecord
citation

Spagnuolo, Michael. Fabrication and Degradation of Electrospun Scaffolds from L-Tyrosine Based Polyurethane Blends for Tissue Engineering Applications. masters thesis, University of Akron, 2011. http://rave.ohiolink.edu/etdc/view?acc_num=akron1304538022