University of Akron
Morphology Control in Mesoporous Carbon Films Using Solvent Engineering
Abstract
dc:descriptionMesoporous carbon materials (2-50 nm) have received much attention in many applications such as catalysis, water purification and energy storage. In the synthesis of mesoporous carbon, the nanostructures of the polymer precursors are usually stabilized by crosslinking in order for the structure to remain during carbonization. However, crosslinking limits the mobility of the polymer chains including the carbon precursors and templates for ordering. Segmental mobility is required for nanostructure formation by ordering of the template. In this study, mesoporous carbon films were fabricated using cooperative self-assembly of a phenolic resin oligomer (resol) with a novel block copolymer template (poly(styrene-block-polystyrenesulfonate N,N-dimethyl-n-octadecylamine), (PS-b-PSS-DMODA)), which is synthesized by reversible addition-fragmentation chain transfer (RAFT) polymerization. Due to the high Tg of the PS segment and the strong interactions between the phenolic resin and the PSS-DMODA, segmental re-arrangement is kinetically hindered relative to the crosslinking rate of the phenolic resin, which inhibits long range ordering and yields a poorly ordered mesoporous carbon with a broad pore size distribution. Two processing methods are introduced to overcome these limitations: (1) solvent vapor annealing and (2) the use of solvent additives. Controlled vapor pressures of methyl ethyl ketone (MEK) yields significant improvements in the long range ordering and narrows the pore size distribution of mesoporous polymer films. The average pore size increases as the solvent vapor pressure increases, but an upper limit of p/p0 = 0.85 exists above which the films dewet rapidly during solvent vapor annealing. Alternatively, addition of both dioctyl phthalate (DOP, PS selective) and dimethyl sulfoxide (DMSO, resol and PSS- DMODA selective) at modest concentrations to the casting solution provides sufficient mobility to produce highly ordered films with cylindrical mesopores. The DOP acts to swell the hydrophobic domain and can more than double the mesopore size, while the DMSO acts to swell the resol phase. Variation in the concentration of DOP and DMSO during casting enables facile tuning of the structure of mesoporous carbon films. These results illustrate the ability to fine tune the morphology of mesoporous carbon films through simple changes in the processing method without any compositional changes in the initial cast film. Also, the method of using mixed solvent additives should be easily extendable to other self-assembled systems including mesoporous metal oxide films from sol-gel or nanoparticle assembly.
Degree
thesis:*- Name thesis:degree_name
- Master of Science in Polymer Engineering
- Level thesis:degree_level
- masters
- Discipline thesis:degree_discipline
- Polymer Engineering
- Grantor dc:publisher
- University of Akron
- Year dc:date
- 2013
Author and committee
dc:creator, dc:contributor.*- Author dc:creator
-
- Qiang, Zhe
- Contributors dc:contributor
-
- Vogt, Bryan
- Cavicchi, Kevin
Subjects
dc:subject × 5Rights
dc:rights- Statement dc:rights
-
- unrestricted
- This thesis or dissertation is protected by copyright: all rights reserved. It may not be copied or redistributed beyond the terms of applicable copyright laws.
- Language dc:language
- English
Identifiers
dc:identifier.*- Repository record dc:identifier
- http://rave.ohiolink.edu/etdc/view?acc_num=akron1367336863