University of Akron
Aging of Thin Glassy Polymers Probed by Ellipsometry and Mechanics
Abstract
dc:descriptionThe nature of interfacial interactions can significantly alter the physical and mechanical properties of thin polymer films. Glassy films are particularly prone to changes in physical aging in thin films, which can significantly alter the properties in applications. A glassy polymer film is initially inherently in a non-equilibrium state, but the chains will slowly relax towards equilibrium below the glass transition temperature (Tg). This aging can be assessed with a variety of properties from thermodynamic to volumetric to dynamic.In this work, the physical aging of a promising copolymer for membrane separations, butylnorbornene-ran-hydroxyhexafluoroisopropyl norbornene (BuNB-ran-HFANB), in thin films was systematically investigated. The BuNB-ran-HFANB film thickness and aging temperature both impacted the aging rate of the films. We observed rapid densification of the BuNB-ran-HFANB polymer even when aged >200°C below Tg via ellipsometric measurements during isothermal aging process. However, for the thinnest polymer films, the film thickness increases instead of decreases during aging, which we attribute to an initial highly non-equilibrium state for the BuNB-ran-HFANB chains as a result of the rapid evaporation during the spin coating process. The substrate selection for these films impacted the observed physical aging of the BuNB-ran-HFANB films with bare silicon, 2nm polystyrene sulfonate (PSS), and 2nm poly(acrylic acid) (PAA) coatings investigated as substrates for the BuNB-ran-HFANB films. The unusual aging behavior of increasing film thickness was seen for the thinnest polymer films for all three substrates, but the onset for the increasing thickness during aging was substrate dependent (<250nm for PSS, <115nm PAA, <150nm silicon). To understand this behavior, the stress state after different aging times were determined via wrinkling experiments on the aged films. The residual stress in the thin films initially increased during aging, but the stress then decreased approximately when the increase in film thickness occurred. These results suggest that the unusual aging behavior is associated with the stress state in the films.
Degree
thesis:*- Name thesis:degree_name
- Doctor of Philosophy
- Level thesis:degree_level
- doctoral
- Discipline thesis:degree_discipline
- Polymer Engineering
- Grantor dc:publisher
- University of Akron
- Year dc:date
- 2020
Author and committee
dc:creator, dc:contributor.*- Author dc:creator
-
- Lewis, Elizabeth A.
- Advisors dc:contributor.advisor
-
- Vogt, Bryan
- Cavicchi, Kevin
- Chair dc:contributor.committeechair
-
- Kyu, Thein
Subjects
dc:subject × 7Rights
dc:rights- Statement dc:rights
-
- unrestricted
- This thesis or dissertation is protected by copyright: all rights reserved. It may not be copied or redistributed beyond the terms of applicable copyright laws.
- Language dc:language
- English
Identifiers
dc:identifier.*- Repository record dc:identifier
- http://rave.ohiolink.edu/etdc/view?acc_num=akron158465039485355